Catalytic Methane Decomposition over Fe‐Al 2 O 3
The presence of a Fe–FeAl 2 O 4 structure over an Fe–Al 2 O 3 catalysts is demonstrated to be vital for the catalytic methane decomposition (CMD) activity. After H 2 reduction at 750 °C, Fe–Al 2 O 3 prepared by means of a fusion method, containing 86.5 wt % FeAl 2 O 4 and 13.5 wt % Fe 0 , showed a s...
Saved in:
Published in: | ChemSusChem 2016-06, Vol.9 (11), p.1243-1248 |
---|---|
Main Authors: | , , , , , , |
Format: | Article |
Language: | English |
Citations: | Items that this one cites Items that cite this one |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | The presence of a Fe–FeAl
2
O
4
structure over an Fe–Al
2
O
3
catalysts is demonstrated to be vital for the catalytic methane decomposition (CMD) activity. After H
2
reduction at 750 °C, Fe–Al
2
O
3
prepared by means of a fusion method, containing 86.5 wt % FeAl
2
O
4
and 13.5 wt % Fe
0
, showed a stable CMD activity at 750 °C for as long as 10 h. |
---|---|