A study of nonstoichiometry and the electrical conductivity of erbium sesquioxide

The nonstoichiometric composition of Er 2 O 3 and the electrical conductivity of Er 2 O 3 were measured in the temperature range of 800–1050°C under oxygen partial pressure from 10 −5 to 2 × 10 −1 atm. The nonstoichiometric deviation, x in Er 2 O 3+ x was found to be

Saved in:
Bibliographic Details
Published in:The Journal of physics and chemistry of solids 1987, Vol.48 (8), p.733-737
Main Authors: Yo, Chul Hyun, Park, Sung Ho, Choi, Jae Shi, Moo Sil Pyon
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:The nonstoichiometric composition of Er 2 O 3 and the electrical conductivity of Er 2 O 3 were measured in the temperature range of 800–1050°C under oxygen partial pressure from 10 −5 to 2 × 10 −1 atm. The nonstoichiometric deviation, x in Er 2 O 3+ x was found to be