Spinel-type structure of Co in conditions of HDS catalyst aging

The structural investigation of CoO–MoO 3/ γ-Al 2O 3 HDS catalystassumed to accelerate aging in laboratory conditions followed by the DRS method pointed out the surface spinel formation The amount of spinel structure formed increased with increasing temperature and decreased with the treatment atmos...

Full description

Saved in:
Bibliographic Details
Published in:Polyhedron 1999-01, Vol.18 (5), p.741-747
Main Authors: Kiurski, J, Obadovic, D.Z, Marinkovic-Nedučin, R, Kis, E
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:The structural investigation of CoO–MoO 3/ γ-Al 2O 3 HDS catalystassumed to accelerate aging in laboratory conditions followed by the DRS method pointed out the surface spinel formation The amount of spinel structure formed increased with increasing temperature and decreased with the treatment atmosphere in the order: nitrogen>air>steam On the basis of the experimental data of electronic d–d transitions of Co (II) ion in a catalyst treated in nitrogen atmosphere the parameter of the crystal-field splitting 10 D q and the energies of the electronic state of Co (II) in a spinel-type structure were calculated The most probable scheme of the molecular orbital has been proposed.