Effect of scandia on tungsten oxide powder reduction process

Scandia doped tungsten powders were prepared by spray drying combined with two-step hydrogen reduction. The particle size of doped tungsten powder, powder morphology and doped tungsten matrix were characterized by scanning electron microscope, X-ray diffraction and laser diffraction particle size an...

Full description

Saved in:
Bibliographic Details
Published in:Journal of rare earths 2010-12, Vol.28, p.202-205
Main Authors: CUI, Yuntao, WANG, Jinshu, LIU, Wei, WANG, Xi
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Scandia doped tungsten powders were prepared by spray drying combined with two-step hydrogen reduction. The particle size of doped tungsten powder, powder morphology and doped tungsten matrix were characterized by scanning electron microscope, X-ray diffraction and laser diffraction particle size analyzer, respectively. The reduction behavior of Sc 2O 3 doped tungsten oxide and the effect of Sc 2O 3 on the property of tungsten powder were studied by the temperature programmed reduction. The experimental results showed that the precursor powders prepared by spray drying had spherical shape. The addition of Sc 2O 3 could decrease the reduction temperature of tungsten oxide. The scandia doped tungsten powder had sub-micrometer size in the range of 0.1 to1 μm and scandium distributed evenly in the powder. By using this kind powder, sub-microstructure cathode matrices with semispherical grains and homogenous distribution of scandium were obtained.