Synthesis, characterization of Mo and Mn doped ZnO and their photocatalytic activity for the decolorization of two different chromophoric dyes

•Photocatalytic performance of doped-ZnO using different chromophoric dyes.•SEM images show fused supramolecular structure with rough surfaces.•The red shift occurred after metal ion doping.•ZnO with dopant 0.60% (Mo), 0.80% (Mn) showed best photocatalytic efficiency.•Azo dye degrades faster than an...

Full description

Saved in:
Bibliographic Details
Published in:Applied catalysis. A, General General, 2015-09, Vol.505, p.507-514
Main Authors: Umar, Khalid, Aris, Azmi, Parveen, Tabassum, Jaafar, Jafariah, Abdul Majid, Zaiton, Vijaya Bhaskar Reddy, A., Talib, Juhaizah
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:•Photocatalytic performance of doped-ZnO using different chromophoric dyes.•SEM images show fused supramolecular structure with rough surfaces.•The red shift occurred after metal ion doping.•ZnO with dopant 0.60% (Mo), 0.80% (Mn) showed best photocatalytic efficiency.•Azo dye degrades faster than anthraquinone dye in the presence of Mo-doped (0.60%) ZnO. Using sol–gel method, nano crystalline ZnO particles doped with different concentrations of molybdenum (Mo) and manganese (Mn) (0.2–1.0%) were synthesized. The structural and optical properties were studied with standard analytical techniques such as scanning electron microscopy (SEM), X-ray diffraction (XRD) and UV–vis spectroscopy. The crystalline nature of undoped and doped ZnO is indicated by XRD analysis. The SEM images of undoped ZnO showed irregular shape while doped ZnO showed fused supramolecular structure with rough surfaces. The photocatalytic activity of the synthesized particles (ZnO doped with Mo and Mn) was tested by studying the decolorization of two different chromophoric dyes namely Direct Yellow 27 (azo dye) and Acid Blue 129 (anthraquinone dye) with a 500W halogen linear lamp in the presence of atmospheric oxygen as a function of irradiation time. The results indicate that ZnO with dopant concentration of 0.60% Mo and 0.80% Mn showed the highest photocatalytic activity as compared to the other dopant concentrations for the decolorization of both dyes. In the case of azo dye, 84% decolorization was found while in case of anthraquinone dye, 66% decolorization took place using 0.60% Mo in 390min.
ISSN:0926-860X
1873-3875
DOI:10.1016/j.apcata.2015.02.001