Effects of pre-existing interfacial defects on the structural evolution of alumina coated Si electrode during delithiation

[Display omitted] •Effective coverage ratio (ECR) were introduced to mimic the different degrees of pre-existing interface defects.•Battery capacity would have a rapider loss when the ECR reduced below a threshold (about 55%).•Pre-existing defects would “boost” interfacial delamination during subseq...

Full description

Saved in:
Bibliographic Details
Published in:Applied surface science 2020-08, Vol.520, p.146366, Article 146366
Main Authors: Feng, Chen, Shi, Tielin, Li, Junjie, Cheng, Siyi, Liao, Guanglan, Tang, Zirong
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
cited_by cdi_FETCH-LOGICAL-c306t-2d2dd5503adf22755e26cf0d74c013de2a802d6a5c53a98eead104536fd1664c3
cites cdi_FETCH-LOGICAL-c306t-2d2dd5503adf22755e26cf0d74c013de2a802d6a5c53a98eead104536fd1664c3
container_end_page
container_issue
container_start_page 146366
container_title Applied surface science
container_volume 520
creator Feng, Chen
Shi, Tielin
Li, Junjie
Cheng, Siyi
Liao, Guanglan
Tang, Zirong
description [Display omitted] •Effective coverage ratio (ECR) were introduced to mimic the different degrees of pre-existing interface defects.•Battery capacity would have a rapider loss when the ECR reduced below a threshold (about 55%).•Pre-existing defects would “boost” interfacial delamination during subsequent cycles in full discharge condition. Interfacial degradation is one of the root causes of the poor performance of Si-based lithium-ion batteries. Only figure out the role of interfacial degradation in cycling can we optimize electrodes to improve the battery robustness and durability. Here, we performed reactive force field (ReaxFF) atomistic simulations to investigate the “natural” delithiation responses of a-Si-core/a-Al2O3-coating electrode with different degrees of pre-existing interfacial defects. Effective coverage ratio (ECR) was introduced to mimic different degrees of the pre-existing defects on the a-LixSi/a-LixAl2O3 interface. The simulation quantitatively showed that, in any ECR samples, the delithiation could be characterized as two stages: a steady stage with a higher discharge rate and a lower nanoporosity, and an unsteady stage with a lower discharge rate and a larger aggregates of nanopores. The deterioration of ECR caused the steady stage shortened and unsteady stage prolonged. Consequently, further interfacial delamination was easier to form in lower ECR samples in full discharge condition, and the pre-existing defects would “boost” interfacial delamination during subsequent cycles. Besides, the battery capacity would have a rapid loss when the ECR reduced below a threshold (about 55%). This work provides a fundamental understanding of delithiation-induced interfacial degradation mechanism of Si electrodes at atomic-level.
doi_str_mv 10.1016/j.apsusc.2020.146366
format article
fullrecord <record><control><sourceid>elsevier_cross</sourceid><recordid>TN_cdi_crossref_primary_10_1016_j_apsusc_2020_146366</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S0169433220311235</els_id><sourcerecordid>S0169433220311235</sourcerecordid><originalsourceid>FETCH-LOGICAL-c306t-2d2dd5503adf22755e26cf0d74c013de2a802d6a5c53a98eead104536fd1664c3</originalsourceid><addsrcrecordid>eNp9kN1KAzEQhYMoWKtv4EVeYGt-Nun2RpBSf6DghXodQmZiU7a7JckW9enNsl57NTDnfIeZQ8gtZwvOuL7bL-wxDcktBBNlVWup9RmZ8WYpK6Wa-pzMim1V1VKKS3KV0p4xLoo6Iz8b79HlRHtPjxEr_Aoph-6Thi5j9NYF21LAP09H8w5pynFweYhFwVPfDjkUofC2HQ6hs9T1NiPQt0CxLVzsASkMcUwFbEPeBTsi1-TC2zbhzd-ck4_Hzfv6udq-Pr2sH7aVk0znSoAAUIpJC16IpVIotPMMlrVjXAIK2zAB2iqnpF01iBY4q5XUHrjWtZNzUk-5LvYpRfTmGMPBxm_DmRn7M3sz9WfG_szUX8HuJwzLbaeA0SQXsHMIIZavDPTh_4BfVL1-Zw</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Effects of pre-existing interfacial defects on the structural evolution of alumina coated Si electrode during delithiation</title><source>ScienceDirect Freedom Collection 2022-2024</source><creator>Feng, Chen ; Shi, Tielin ; Li, Junjie ; Cheng, Siyi ; Liao, Guanglan ; Tang, Zirong</creator><creatorcontrib>Feng, Chen ; Shi, Tielin ; Li, Junjie ; Cheng, Siyi ; Liao, Guanglan ; Tang, Zirong</creatorcontrib><description>[Display omitted] •Effective coverage ratio (ECR) were introduced to mimic the different degrees of pre-existing interface defects.•Battery capacity would have a rapider loss when the ECR reduced below a threshold (about 55%).•Pre-existing defects would “boost” interfacial delamination during subsequent cycles in full discharge condition. Interfacial degradation is one of the root causes of the poor performance of Si-based lithium-ion batteries. Only figure out the role of interfacial degradation in cycling can we optimize electrodes to improve the battery robustness and durability. Here, we performed reactive force field (ReaxFF) atomistic simulations to investigate the “natural” delithiation responses of a-Si-core/a-Al2O3-coating electrode with different degrees of pre-existing interfacial defects. Effective coverage ratio (ECR) was introduced to mimic different degrees of the pre-existing defects on the a-LixSi/a-LixAl2O3 interface. The simulation quantitatively showed that, in any ECR samples, the delithiation could be characterized as two stages: a steady stage with a higher discharge rate and a lower nanoporosity, and an unsteady stage with a lower discharge rate and a larger aggregates of nanopores. The deterioration of ECR caused the steady stage shortened and unsteady stage prolonged. Consequently, further interfacial delamination was easier to form in lower ECR samples in full discharge condition, and the pre-existing defects would “boost” interfacial delamination during subsequent cycles. Besides, the battery capacity would have a rapid loss when the ECR reduced below a threshold (about 55%). This work provides a fundamental understanding of delithiation-induced interfacial degradation mechanism of Si electrodes at atomic-level.</description><identifier>ISSN: 0169-4332</identifier><identifier>EISSN: 1873-5584</identifier><identifier>DOI: 10.1016/j.apsusc.2020.146366</identifier><language>eng</language><publisher>Elsevier B.V</publisher><subject>Capacity loss ; Interfacial delamination ; Molecular dynamics ; Nanoporosity ; Silicon electrode</subject><ispartof>Applied surface science, 2020-08, Vol.520, p.146366, Article 146366</ispartof><rights>2020 Elsevier B.V.</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c306t-2d2dd5503adf22755e26cf0d74c013de2a802d6a5c53a98eead104536fd1664c3</citedby><cites>FETCH-LOGICAL-c306t-2d2dd5503adf22755e26cf0d74c013de2a802d6a5c53a98eead104536fd1664c3</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,780,784,27924,27925</link.rule.ids></links><search><creatorcontrib>Feng, Chen</creatorcontrib><creatorcontrib>Shi, Tielin</creatorcontrib><creatorcontrib>Li, Junjie</creatorcontrib><creatorcontrib>Cheng, Siyi</creatorcontrib><creatorcontrib>Liao, Guanglan</creatorcontrib><creatorcontrib>Tang, Zirong</creatorcontrib><title>Effects of pre-existing interfacial defects on the structural evolution of alumina coated Si electrode during delithiation</title><title>Applied surface science</title><description>[Display omitted] •Effective coverage ratio (ECR) were introduced to mimic the different degrees of pre-existing interface defects.•Battery capacity would have a rapider loss when the ECR reduced below a threshold (about 55%).•Pre-existing defects would “boost” interfacial delamination during subsequent cycles in full discharge condition. Interfacial degradation is one of the root causes of the poor performance of Si-based lithium-ion batteries. Only figure out the role of interfacial degradation in cycling can we optimize electrodes to improve the battery robustness and durability. Here, we performed reactive force field (ReaxFF) atomistic simulations to investigate the “natural” delithiation responses of a-Si-core/a-Al2O3-coating electrode with different degrees of pre-existing interfacial defects. Effective coverage ratio (ECR) was introduced to mimic different degrees of the pre-existing defects on the a-LixSi/a-LixAl2O3 interface. The simulation quantitatively showed that, in any ECR samples, the delithiation could be characterized as two stages: a steady stage with a higher discharge rate and a lower nanoporosity, and an unsteady stage with a lower discharge rate and a larger aggregates of nanopores. The deterioration of ECR caused the steady stage shortened and unsteady stage prolonged. Consequently, further interfacial delamination was easier to form in lower ECR samples in full discharge condition, and the pre-existing defects would “boost” interfacial delamination during subsequent cycles. Besides, the battery capacity would have a rapid loss when the ECR reduced below a threshold (about 55%). This work provides a fundamental understanding of delithiation-induced interfacial degradation mechanism of Si electrodes at atomic-level.</description><subject>Capacity loss</subject><subject>Interfacial delamination</subject><subject>Molecular dynamics</subject><subject>Nanoporosity</subject><subject>Silicon electrode</subject><issn>0169-4332</issn><issn>1873-5584</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2020</creationdate><recordtype>article</recordtype><recordid>eNp9kN1KAzEQhYMoWKtv4EVeYGt-Nun2RpBSf6DghXodQmZiU7a7JckW9enNsl57NTDnfIeZQ8gtZwvOuL7bL-wxDcktBBNlVWup9RmZ8WYpK6Wa-pzMim1V1VKKS3KV0p4xLoo6Iz8b79HlRHtPjxEr_Aoph-6Thi5j9NYF21LAP09H8w5pynFweYhFwVPfDjkUofC2HQ6hs9T1NiPQt0CxLVzsASkMcUwFbEPeBTsi1-TC2zbhzd-ck4_Hzfv6udq-Pr2sH7aVk0znSoAAUIpJC16IpVIotPMMlrVjXAIK2zAB2iqnpF01iBY4q5XUHrjWtZNzUk-5LvYpRfTmGMPBxm_DmRn7M3sz9WfG_szUX8HuJwzLbaeA0SQXsHMIIZavDPTh_4BfVL1-Zw</recordid><startdate>20200801</startdate><enddate>20200801</enddate><creator>Feng, Chen</creator><creator>Shi, Tielin</creator><creator>Li, Junjie</creator><creator>Cheng, Siyi</creator><creator>Liao, Guanglan</creator><creator>Tang, Zirong</creator><general>Elsevier B.V</general><scope>AAYXX</scope><scope>CITATION</scope></search><sort><creationdate>20200801</creationdate><title>Effects of pre-existing interfacial defects on the structural evolution of alumina coated Si electrode during delithiation</title><author>Feng, Chen ; Shi, Tielin ; Li, Junjie ; Cheng, Siyi ; Liao, Guanglan ; Tang, Zirong</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c306t-2d2dd5503adf22755e26cf0d74c013de2a802d6a5c53a98eead104536fd1664c3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2020</creationdate><topic>Capacity loss</topic><topic>Interfacial delamination</topic><topic>Molecular dynamics</topic><topic>Nanoporosity</topic><topic>Silicon electrode</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Feng, Chen</creatorcontrib><creatorcontrib>Shi, Tielin</creatorcontrib><creatorcontrib>Li, Junjie</creatorcontrib><creatorcontrib>Cheng, Siyi</creatorcontrib><creatorcontrib>Liao, Guanglan</creatorcontrib><creatorcontrib>Tang, Zirong</creatorcontrib><collection>CrossRef</collection><jtitle>Applied surface science</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Feng, Chen</au><au>Shi, Tielin</au><au>Li, Junjie</au><au>Cheng, Siyi</au><au>Liao, Guanglan</au><au>Tang, Zirong</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Effects of pre-existing interfacial defects on the structural evolution of alumina coated Si electrode during delithiation</atitle><jtitle>Applied surface science</jtitle><date>2020-08-01</date><risdate>2020</risdate><volume>520</volume><spage>146366</spage><pages>146366-</pages><artnum>146366</artnum><issn>0169-4332</issn><eissn>1873-5584</eissn><abstract>[Display omitted] •Effective coverage ratio (ECR) were introduced to mimic the different degrees of pre-existing interface defects.•Battery capacity would have a rapider loss when the ECR reduced below a threshold (about 55%).•Pre-existing defects would “boost” interfacial delamination during subsequent cycles in full discharge condition. Interfacial degradation is one of the root causes of the poor performance of Si-based lithium-ion batteries. Only figure out the role of interfacial degradation in cycling can we optimize electrodes to improve the battery robustness and durability. Here, we performed reactive force field (ReaxFF) atomistic simulations to investigate the “natural” delithiation responses of a-Si-core/a-Al2O3-coating electrode with different degrees of pre-existing interfacial defects. Effective coverage ratio (ECR) was introduced to mimic different degrees of the pre-existing defects on the a-LixSi/a-LixAl2O3 interface. The simulation quantitatively showed that, in any ECR samples, the delithiation could be characterized as two stages: a steady stage with a higher discharge rate and a lower nanoporosity, and an unsteady stage with a lower discharge rate and a larger aggregates of nanopores. The deterioration of ECR caused the steady stage shortened and unsteady stage prolonged. Consequently, further interfacial delamination was easier to form in lower ECR samples in full discharge condition, and the pre-existing defects would “boost” interfacial delamination during subsequent cycles. Besides, the battery capacity would have a rapid loss when the ECR reduced below a threshold (about 55%). This work provides a fundamental understanding of delithiation-induced interfacial degradation mechanism of Si electrodes at atomic-level.</abstract><pub>Elsevier B.V</pub><doi>10.1016/j.apsusc.2020.146366</doi></addata></record>
fulltext fulltext
identifier ISSN: 0169-4332
ispartof Applied surface science, 2020-08, Vol.520, p.146366, Article 146366
issn 0169-4332
1873-5584
language eng
recordid cdi_crossref_primary_10_1016_j_apsusc_2020_146366
source ScienceDirect Freedom Collection 2022-2024
subjects Capacity loss
Interfacial delamination
Molecular dynamics
Nanoporosity
Silicon electrode
title Effects of pre-existing interfacial defects on the structural evolution of alumina coated Si electrode during delithiation
url http://sfxeu10.hosted.exlibrisgroup.com/loughborough?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-06T03%3A10%3A18IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-elsevier_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Effects%20of%20pre-existing%20interfacial%20defects%20on%20the%20structural%20evolution%20of%20alumina%20coated%20Si%20electrode%20during%20delithiation&rft.jtitle=Applied%20surface%20science&rft.au=Feng,%20Chen&rft.date=2020-08-01&rft.volume=520&rft.spage=146366&rft.pages=146366-&rft.artnum=146366&rft.issn=0169-4332&rft.eissn=1873-5584&rft_id=info:doi/10.1016/j.apsusc.2020.146366&rft_dat=%3Celsevier_cross%3ES0169433220311235%3C/elsevier_cross%3E%3Cgrp_id%3Ecdi_FETCH-LOGICAL-c306t-2d2dd5503adf22755e26cf0d74c013de2a802d6a5c53a98eead104536fd1664c3%3C/grp_id%3E%3Coa%3E%3C/oa%3E%3Curl%3E%3C/url%3E&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true