Doubling the coating-substrate pull-off strength by growth of CaCO3 nano-crystals
•The coating-substrate pull-off strength increased by up to 112.2% with carbonation curing.•Interfacial debonding was altered to substrate failure after ACC treatment.•Pure physical adhesion had limited contribution to the strength rises.•Pillar-like CaCO3 nano-crystals provided the crystals anchori...
Saved in:
Published in: | Chemical engineering journal (Lausanne, Switzerland : 1996) Switzerland : 1996), 2023-10, Vol.474, p.145763, Article 145763 |
---|---|
Main Authors: | , , , , , , , , |
Format: | Article |
Language: | English |
Subjects: | |
Citations: | Items that this one cites Items that cite this one |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | •The coating-substrate pull-off strength increased by up to 112.2% with carbonation curing.•Interfacial debonding was altered to substrate failure after ACC treatment.•Pure physical adhesion had limited contribution to the strength rises.•Pillar-like CaCO3 nano-crystals provided the crystals anchoring adhesion.
Strong coating-substrate adhesion is crucial for ensuring long-term durability and performance of protective coatings in various applications. The growth of nano crystals on the substrate may be a preferable way to enhance the coating-substrate interactions. Here, an accelerated carbonation curing (ACC) scheme (0.5 MPa CO2 gas pressure) was designed to grow calcium carbonate (CaCO3) nano-crystals on a mortar substrate at early age before coated with a waterborne epoxy resin (WER). Microstructures of the ACC-treated mortar specimens and the coating-substrate interfaces were characterized by multiple microscopic tests, and the compressive strength of the carbonated substrate and the pull-off coating-substrate strength were measured. Results showed that the ACC treatment not only increased the mortar strength (by up to 17%), but also greatly improved the pull-off strength (by up to 112.2%). Substrate failure took place in the mortars after the ACC treatment. The mechanisms of physical adhesion, surface roughness, and crystals anchoring caused by the growth of pillar-like CaCO3 nano-crystals may account for the largely raised pull-off strength. The findings would deepen the understandings of interfacial adhesion mechanisms between polymer coatings and cement-based substrates and provide new insights into developing stronger coating-substrate adhesions. |
---|---|