Effects of spark plasma sintering temperature on densification, hardness and thermal conductivity of titanium carbide

The effects of spark plasma sintering (SPS) temperature on densification, microstructure, hardness and thermal conductivity of monolithic TiC ceramics were studied. Three samples were spark plasma sintered at temperatures of 1800, 1900 and 2000 °C for holding time of 7 min under pressure of 40 MPa....

Full description

Saved in:
Bibliographic Details
Published in:Ceramics international 2018-08, Vol.44 (12), p.14541-14546
Main Authors: Babapoor, Aziz, Asl, Mehdi Shahedi, Ahmadi, Zohre, Namini, Abbas Sabahi
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:The effects of spark plasma sintering (SPS) temperature on densification, microstructure, hardness and thermal conductivity of monolithic TiC ceramics were studied. Three samples were spark plasma sintered at temperatures of 1800, 1900 and 2000 °C for holding time of 7 min under pressure of 40 MPa. The relative density, hardness and thermal conductivity increased with sintering temperature from 1800° to 1900°C, but the mentioned properties decreased by spark plasma sintering at 2000 °C. The microstructural analyses showed that a fully-sintered TiC ceramic can be achieved at the SPS temperature of 1900 °C, with no significant growth of grains. The relative density, Vickers hardness and thermal conductivity of the TiC ceramic, sintered at the optimal temperature of 1900 °C, reached 99.4%, 25.7 GPa and 17.9 W/mK, respectively.