Electromechanical properties and domain evolution of a tetragonal Er3+-doped Pb(Mg1/3Nb2/3)O3–PbTiO3 ferroelectric single crystal
Herein, a tetragonal Er3+-doped Pb(Mg1/3Nb2/3)O3–PbTiO3 single crystal is comprehensively investigated. The actual composition of the studied crystal is Pb(Mg1/3Nb2/3)O3–36PbTiO3 doped with 0.17-mol% Er3+ (PMN–36PT: 0.17-mol% Er3+). The crystal exhibits a high shear piezoelectric constant of ∼936 pC...
Saved in:
Published in: | Journal of alloys and compounds 2024-07, Vol.992, p.174565, Article 174565 |
---|---|
Main Authors: | , , , , , |
Format: | Article |
Language: | English |
Subjects: | |
Citations: | Items that this one cites |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
cited_by | |
---|---|
cites | cdi_FETCH-LOGICAL-c187t-f472da7d11ef6076356182c965a41309c861bdd88a9b45962414594079844fb73 |
container_end_page | |
container_issue | |
container_start_page | 174565 |
container_title | Journal of alloys and compounds |
container_volume | 992 |
creator | He, Aiguo Long, Wei Xi, Zengzhe Li, Xiaojuan Fang, Pinyang Liu, Weiguo |
description | Herein, a tetragonal Er3+-doped Pb(Mg1/3Nb2/3)O3–PbTiO3 single crystal is comprehensively investigated. The actual composition of the studied crystal is Pb(Mg1/3Nb2/3)O3–36PbTiO3 doped with 0.17-mol% Er3+ (PMN–36PT: 0.17-mol% Er3+). The crystal exhibits a high shear piezoelectric constant of ∼936 pC/N, approximately three times the longitudinal piezoelectric constant when poled along [001]c, as well as a higher Curie temperature of ∼170 °C and large coercive field of ∼4.58 kV/cm. At room temperature, the crystal presents a mass of domain walls along the c direction and extinction is observed four times within a 360° rotation, showing typical domain features of the tetragonal phase. Under a direct current–electric field along the [010]c direction, the extinction rule remains unchanged; however, changes in the domain configuration can be observed. In addition, the orientation dependence of the piezoelectric constant, dielectric coefficient, elastic compliance constant, and electromechanical coupling factor is calculated using the coordinate transformation method. The findings of this study are of considerable importance for the fundamental studies and device design of tetragonal ferroelectric crystals.
•The studied crystal presents a higher Tc of 164–170 ℃ and a larger Ec of 4.58 kV/cm.•The phase structure is clearly affirmed using domain configuration and extinction feature.•Full tensor parameters were characterized for [001]c-poled tetragonal Er3+-doped PMN-PT single crystal. |
doi_str_mv | 10.1016/j.jallcom.2024.174565 |
format | article |
fullrecord | <record><control><sourceid>elsevier_cross</sourceid><recordid>TN_cdi_crossref_primary_10_1016_j_jallcom_2024_174565</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S0925838824011526</els_id><sourcerecordid>S0925838824011526</sourcerecordid><originalsourceid>FETCH-LOGICAL-c187t-f472da7d11ef6076356182c965a41309c861bdd88a9b45962414594079844fb73</originalsourceid><addsrcrecordid>eNqFkE1OwzAUhC0EEqVwBCQvQSipHTuOs0KoKj9SoV2UteXYTnHkxJUdKnWHxBG4ISch0O5ZzebNzJsPgEuMUowwmzRpI51Tvk0zlNEUFzRn-REYYV6QhDJWHoMRKrM84YTzU3AWY4MQwiXBI_A5c0b1wbdGvcnOKungJviNCb01EcpOQ-1baTtott6999Z30NdQwt70Qa59N9zPArlJ9ODRcFldPa_xhLxU2YRcL8j3x9eyWtkFgbUJwZu_LqtgtN3aGajCLvbSnYOTWrpoLg46Bq_3s9X0MZkvHp6md_NEDUv6pKZFpmWhMTY1QwUjOcM8UyXLJcUElYozXGnNuSwrmpcso3gQioqSU1pXBRmDfJ-rgo8xmFpsgm1l2AmMxC9J0YgDSfFLUuxJDr7bvc8Mz22tCSIqazpltA3DIKG9_SfhB32Ff6c</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Electromechanical properties and domain evolution of a tetragonal Er3+-doped Pb(Mg1/3Nb2/3)O3–PbTiO3 ferroelectric single crystal</title><source>ScienceDirect Journals</source><creator>He, Aiguo ; Long, Wei ; Xi, Zengzhe ; Li, Xiaojuan ; Fang, Pinyang ; Liu, Weiguo</creator><creatorcontrib>He, Aiguo ; Long, Wei ; Xi, Zengzhe ; Li, Xiaojuan ; Fang, Pinyang ; Liu, Weiguo</creatorcontrib><description>Herein, a tetragonal Er3+-doped Pb(Mg1/3Nb2/3)O3–PbTiO3 single crystal is comprehensively investigated. The actual composition of the studied crystal is Pb(Mg1/3Nb2/3)O3–36PbTiO3 doped with 0.17-mol% Er3+ (PMN–36PT: 0.17-mol% Er3+). The crystal exhibits a high shear piezoelectric constant of ∼936 pC/N, approximately three times the longitudinal piezoelectric constant when poled along [001]c, as well as a higher Curie temperature of ∼170 °C and large coercive field of ∼4.58 kV/cm. At room temperature, the crystal presents a mass of domain walls along the c direction and extinction is observed four times within a 360° rotation, showing typical domain features of the tetragonal phase. Under a direct current–electric field along the [010]c direction, the extinction rule remains unchanged; however, changes in the domain configuration can be observed. In addition, the orientation dependence of the piezoelectric constant, dielectric coefficient, elastic compliance constant, and electromechanical coupling factor is calculated using the coordinate transformation method. The findings of this study are of considerable importance for the fundamental studies and device design of tetragonal ferroelectric crystals.
•The studied crystal presents a higher Tc of 164–170 ℃ and a larger Ec of 4.58 kV/cm.•The phase structure is clearly affirmed using domain configuration and extinction feature.•Full tensor parameters were characterized for [001]c-poled tetragonal Er3+-doped PMN-PT single crystal.</description><identifier>ISSN: 0925-8388</identifier><identifier>EISSN: 1873-4669</identifier><identifier>DOI: 10.1016/j.jallcom.2024.174565</identifier><language>eng</language><publisher>Elsevier B.V</publisher><subject>Domain evolution ; Electric properties ; Er3+-doped Pb(Mg1/3Nb2/3)O3–PbTiO3 ; Tetragonal phase</subject><ispartof>Journal of alloys and compounds, 2024-07, Vol.992, p.174565, Article 174565</ispartof><rights>2024 Elsevier B.V.</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><cites>FETCH-LOGICAL-c187t-f472da7d11ef6076356182c965a41309c861bdd88a9b45962414594079844fb73</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,780,784,27924,27925</link.rule.ids></links><search><creatorcontrib>He, Aiguo</creatorcontrib><creatorcontrib>Long, Wei</creatorcontrib><creatorcontrib>Xi, Zengzhe</creatorcontrib><creatorcontrib>Li, Xiaojuan</creatorcontrib><creatorcontrib>Fang, Pinyang</creatorcontrib><creatorcontrib>Liu, Weiguo</creatorcontrib><title>Electromechanical properties and domain evolution of a tetragonal Er3+-doped Pb(Mg1/3Nb2/3)O3–PbTiO3 ferroelectric single crystal</title><title>Journal of alloys and compounds</title><description>Herein, a tetragonal Er3+-doped Pb(Mg1/3Nb2/3)O3–PbTiO3 single crystal is comprehensively investigated. The actual composition of the studied crystal is Pb(Mg1/3Nb2/3)O3–36PbTiO3 doped with 0.17-mol% Er3+ (PMN–36PT: 0.17-mol% Er3+). The crystal exhibits a high shear piezoelectric constant of ∼936 pC/N, approximately three times the longitudinal piezoelectric constant when poled along [001]c, as well as a higher Curie temperature of ∼170 °C and large coercive field of ∼4.58 kV/cm. At room temperature, the crystal presents a mass of domain walls along the c direction and extinction is observed four times within a 360° rotation, showing typical domain features of the tetragonal phase. Under a direct current–electric field along the [010]c direction, the extinction rule remains unchanged; however, changes in the domain configuration can be observed. In addition, the orientation dependence of the piezoelectric constant, dielectric coefficient, elastic compliance constant, and electromechanical coupling factor is calculated using the coordinate transformation method. The findings of this study are of considerable importance for the fundamental studies and device design of tetragonal ferroelectric crystals.
•The studied crystal presents a higher Tc of 164–170 ℃ and a larger Ec of 4.58 kV/cm.•The phase structure is clearly affirmed using domain configuration and extinction feature.•Full tensor parameters were characterized for [001]c-poled tetragonal Er3+-doped PMN-PT single crystal.</description><subject>Domain evolution</subject><subject>Electric properties</subject><subject>Er3+-doped Pb(Mg1/3Nb2/3)O3–PbTiO3</subject><subject>Tetragonal phase</subject><issn>0925-8388</issn><issn>1873-4669</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2024</creationdate><recordtype>article</recordtype><recordid>eNqFkE1OwzAUhC0EEqVwBCQvQSipHTuOs0KoKj9SoV2UteXYTnHkxJUdKnWHxBG4ISch0O5ZzebNzJsPgEuMUowwmzRpI51Tvk0zlNEUFzRn-REYYV6QhDJWHoMRKrM84YTzU3AWY4MQwiXBI_A5c0b1wbdGvcnOKungJviNCb01EcpOQ-1baTtott6999Z30NdQwt70Qa59N9zPArlJ9ODRcFldPa_xhLxU2YRcL8j3x9eyWtkFgbUJwZu_LqtgtN3aGajCLvbSnYOTWrpoLg46Bq_3s9X0MZkvHp6md_NEDUv6pKZFpmWhMTY1QwUjOcM8UyXLJcUElYozXGnNuSwrmpcso3gQioqSU1pXBRmDfJ-rgo8xmFpsgm1l2AmMxC9J0YgDSfFLUuxJDr7bvc8Mz22tCSIqazpltA3DIKG9_SfhB32Ff6c</recordid><startdate>20240715</startdate><enddate>20240715</enddate><creator>He, Aiguo</creator><creator>Long, Wei</creator><creator>Xi, Zengzhe</creator><creator>Li, Xiaojuan</creator><creator>Fang, Pinyang</creator><creator>Liu, Weiguo</creator><general>Elsevier B.V</general><scope>AAYXX</scope><scope>CITATION</scope></search><sort><creationdate>20240715</creationdate><title>Electromechanical properties and domain evolution of a tetragonal Er3+-doped Pb(Mg1/3Nb2/3)O3–PbTiO3 ferroelectric single crystal</title><author>He, Aiguo ; Long, Wei ; Xi, Zengzhe ; Li, Xiaojuan ; Fang, Pinyang ; Liu, Weiguo</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c187t-f472da7d11ef6076356182c965a41309c861bdd88a9b45962414594079844fb73</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2024</creationdate><topic>Domain evolution</topic><topic>Electric properties</topic><topic>Er3+-doped Pb(Mg1/3Nb2/3)O3–PbTiO3</topic><topic>Tetragonal phase</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>He, Aiguo</creatorcontrib><creatorcontrib>Long, Wei</creatorcontrib><creatorcontrib>Xi, Zengzhe</creatorcontrib><creatorcontrib>Li, Xiaojuan</creatorcontrib><creatorcontrib>Fang, Pinyang</creatorcontrib><creatorcontrib>Liu, Weiguo</creatorcontrib><collection>CrossRef</collection><jtitle>Journal of alloys and compounds</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>He, Aiguo</au><au>Long, Wei</au><au>Xi, Zengzhe</au><au>Li, Xiaojuan</au><au>Fang, Pinyang</au><au>Liu, Weiguo</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Electromechanical properties and domain evolution of a tetragonal Er3+-doped Pb(Mg1/3Nb2/3)O3–PbTiO3 ferroelectric single crystal</atitle><jtitle>Journal of alloys and compounds</jtitle><date>2024-07-15</date><risdate>2024</risdate><volume>992</volume><spage>174565</spage><pages>174565-</pages><artnum>174565</artnum><issn>0925-8388</issn><eissn>1873-4669</eissn><abstract>Herein, a tetragonal Er3+-doped Pb(Mg1/3Nb2/3)O3–PbTiO3 single crystal is comprehensively investigated. The actual composition of the studied crystal is Pb(Mg1/3Nb2/3)O3–36PbTiO3 doped with 0.17-mol% Er3+ (PMN–36PT: 0.17-mol% Er3+). The crystal exhibits a high shear piezoelectric constant of ∼936 pC/N, approximately three times the longitudinal piezoelectric constant when poled along [001]c, as well as a higher Curie temperature of ∼170 °C and large coercive field of ∼4.58 kV/cm. At room temperature, the crystal presents a mass of domain walls along the c direction and extinction is observed four times within a 360° rotation, showing typical domain features of the tetragonal phase. Under a direct current–electric field along the [010]c direction, the extinction rule remains unchanged; however, changes in the domain configuration can be observed. In addition, the orientation dependence of the piezoelectric constant, dielectric coefficient, elastic compliance constant, and electromechanical coupling factor is calculated using the coordinate transformation method. The findings of this study are of considerable importance for the fundamental studies and device design of tetragonal ferroelectric crystals.
•The studied crystal presents a higher Tc of 164–170 ℃ and a larger Ec of 4.58 kV/cm.•The phase structure is clearly affirmed using domain configuration and extinction feature.•Full tensor parameters were characterized for [001]c-poled tetragonal Er3+-doped PMN-PT single crystal.</abstract><pub>Elsevier B.V</pub><doi>10.1016/j.jallcom.2024.174565</doi></addata></record> |
fulltext | fulltext |
identifier | ISSN: 0925-8388 |
ispartof | Journal of alloys and compounds, 2024-07, Vol.992, p.174565, Article 174565 |
issn | 0925-8388 1873-4669 |
language | eng |
recordid | cdi_crossref_primary_10_1016_j_jallcom_2024_174565 |
source | ScienceDirect Journals |
subjects | Domain evolution Electric properties Er3+-doped Pb(Mg1/3Nb2/3)O3–PbTiO3 Tetragonal phase |
title | Electromechanical properties and domain evolution of a tetragonal Er3+-doped Pb(Mg1/3Nb2/3)O3–PbTiO3 ferroelectric single crystal |
url | http://sfxeu10.hosted.exlibrisgroup.com/loughborough?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-02T21%3A47%3A22IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-elsevier_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Electromechanical%20properties%20and%20domain%20evolution%20of%20a%20tetragonal%20Er3+-doped%20Pb(Mg1/3Nb2/3)O3%E2%80%93PbTiO3%20ferroelectric%20single%20crystal&rft.jtitle=Journal%20of%20alloys%20and%20compounds&rft.au=He,%20Aiguo&rft.date=2024-07-15&rft.volume=992&rft.spage=174565&rft.pages=174565-&rft.artnum=174565&rft.issn=0925-8388&rft.eissn=1873-4669&rft_id=info:doi/10.1016/j.jallcom.2024.174565&rft_dat=%3Celsevier_cross%3ES0925838824011526%3C/elsevier_cross%3E%3Cgrp_id%3Ecdi_FETCH-LOGICAL-c187t-f472da7d11ef6076356182c965a41309c861bdd88a9b45962414594079844fb73%3C/grp_id%3E%3Coa%3E%3C/oa%3E%3Curl%3E%3C/url%3E&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |