Synthesis, photoluminescence, and up-conversion luminescence properties of YTiTaO6:Er3+/Yb3
The relationship between the factors (i.e. the concentrations of Yb3+ and Er3+ and heating temperature in air) and the properties of photoluminescence (PL) and up-conversion luminescence of YTiTaO6:Er3+/Yb3+ whose crystalline phase depended on heating temperature in air was examined using samples sy...
Saved in:
Published in: | Journal of solid state chemistry 2022-09, Vol.313, p.123316, Article 123316 |
---|---|
Main Authors: | , |
Format: | Article |
Language: | English |
Subjects: | |
Citations: | Items that this one cites Items that cite this one |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | The relationship between the factors (i.e. the concentrations of Yb3+ and Er3+ and heating temperature in air) and the properties of photoluminescence (PL) and up-conversion luminescence of YTiTaO6:Er3+/Yb3+ whose crystalline phase depended on heating temperature in air was examined using samples synthesized hydrothermally. The intense green emission (: 2H11/2,4S3/2→4I15/2 transitions of Er3+) was obtained by the excitation at 288 nm using the indirect energy transfer from the YTiTaO6 host crystal, which was about 1.8 times stronger than that obtained by the direct excitation at 380 nm via the f-f transition (: 4I15/2→4G11/2) of Er3+. Aeschynite phase exhibited intermediate luminescence property. The up-conversion emission intensity increased with increasing heating temperature and became the maximum at x = 0.10 and y = 0.20 with euxenite phase, although the co-presence of Yb3+ gave negative effect on the PL intensity of ErxYbyY1-x-yTiTaO6. As heating temperature rose to 1300–1400 °C the intensity of the red up-conversion emission (: 4F9/2→4I15/2 transition) became greater than that of the green emission (: 4S3/2→4I15/2 transition), accordingly the position of the color chromaticity coordinates shifted slightly from green to yellow.
The up conversion emission intensity of YTiTaO6: Er3+/Yb3+ increases with increasing heat-treating temperature and becomes the maximum at x = 0.10 and y = 0.20 with euxenite phase, although the presence of Yb3+ gives negative effect on the PL intensity of ErxYbyY1-x-yTiTaO6. [Display omitted]
•The PL property of YTiTaO6:Er3+/Yb3+ was investigated using samples formed hydrothermally.•Aeschynite phase exhibits intermediate luminescence property.•The PL intensity of ErxYbyY1-x-yTiTaO6 increases with increasing heat-treating temperature.•The up conversion emission intensity became the maximum at x = 0.10 and y = 0.20 with euxenite phase. |
---|---|