Microstructure evolution and deformation mechanism of AZ80 alloy during die forging

Die forging is a processing method that can produce a size and shape close to the finished product and improve the mechanical properties of the alloy. In this paper, Mg–8Al-0.5Zn magnesium alloy was used to prepare stepped shaft by isothermal die forging. The microstructure and stress-strain state o...

Full description

Saved in:
Bibliographic Details
Published in:Materials science & engineering. A, Structural materials : properties, microstructure and processing Structural materials : properties, microstructure and processing, 2023-03, Vol.869, p.144789, Article 144789
Main Authors: Li, Zhu-jin, Wang, Jin-guo, Ni, Tian-yi, Zhang, Wei, Tong, Guo-dong, Chen, Xue-gang, Li, Jun, Yan, Rui-fang
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
cited_by cdi_FETCH-LOGICAL-c300t-4169a8250b51ed03462d2acd1c19c2bbef142a4e23840f3751b8ff659072c65e3
cites cdi_FETCH-LOGICAL-c300t-4169a8250b51ed03462d2acd1c19c2bbef142a4e23840f3751b8ff659072c65e3
container_end_page
container_issue
container_start_page 144789
container_title Materials science & engineering. A, Structural materials : properties, microstructure and processing
container_volume 869
creator Li, Zhu-jin
Wang, Jin-guo
Ni, Tian-yi
Zhang, Wei
Tong, Guo-dong
Chen, Xue-gang
Li, Jun
Yan, Rui-fang
description Die forging is a processing method that can produce a size and shape close to the finished product and improve the mechanical properties of the alloy. In this paper, Mg–8Al-0.5Zn magnesium alloy was used to prepare stepped shaft by isothermal die forging. The microstructure and stress-strain state of different parts of stepped shaft forging were analyzed. The metal rheological law and microstructure evolution mechanism of AZ80 alloy during die forging were discussed. At the position of low stress and high strain state of the die forging, continuous dynamic recrystallization (CDRX) is the main deformation mechanism, and the microstructure is mainly composed of coarse un-dynamic recrystallized (unDRXed) grains and fine equiaxed dynamic recrystallized (DRXed) grains. The unDRXed grains have a strong basal texture, while the DRXed grains exhibit random orientations. At the position of high stress and low strain state of the die forging, {10–12} twinning is the main deformation mechanism, the parent grains show a strong basal texture, while {10–12} twins present [-12-10]-[01–10] double fiber texture parallel to forging direction (FD). The compressive strength and yield strength of the part in the low stress and high strain state are higher than those in the high stress and low strain state, but the fracture strain of the former is lower than that of the latter. The results of this study can provide a reference for the design of die forging die together with the blank shape and size, so as to meet the corresponding performance requirements of different parts of the die forging.
doi_str_mv 10.1016/j.msea.2023.144789
format article
fullrecord <record><control><sourceid>elsevier_cross</sourceid><recordid>TN_cdi_crossref_primary_10_1016_j_msea_2023_144789</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S0921509323002137</els_id><sourcerecordid>S0921509323002137</sourcerecordid><originalsourceid>FETCH-LOGICAL-c300t-4169a8250b51ed03462d2acd1c19c2bbef142a4e23840f3751b8ff659072c65e3</originalsourceid><addsrcrecordid>eNp9kE1LAzEQhoMoWKt_wFP-wK6Tj_0CL6WoFSoe1IuXkE0mNWU_JNkt9N-7az17mhl4n2HmIeSWQcqA5Xf7tI2oUw5cpEzKoqzOyIKVhUhkJfJzsoCKsySDSlySqxj3AMAkZAvy9uJN6OMQRjOMASke-mYcfN9R3Vlq0fWh1b9zi-ZLdz62tHd09VkC1U3TH6kdg-921HqkU3g39dfkwukm4s1fXZKPx4f39SbZvj49r1fbxAiAIZEsr3TJM6gzhhaEzLnl2lhmWGV4XaNjkmuJXJQSnCgyVpfO5VkFBTd5hmJJ-Gnv_EEM6NR38K0OR8VAzVrUXs1a1KxFnbRM0P0Jwumyg8egovHYGbQ-oBmU7f1_-A-QdGv9</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Microstructure evolution and deformation mechanism of AZ80 alloy during die forging</title><source>ScienceDirect Freedom Collection</source><creator>Li, Zhu-jin ; Wang, Jin-guo ; Ni, Tian-yi ; Zhang, Wei ; Tong, Guo-dong ; Chen, Xue-gang ; Li, Jun ; Yan, Rui-fang</creator><creatorcontrib>Li, Zhu-jin ; Wang, Jin-guo ; Ni, Tian-yi ; Zhang, Wei ; Tong, Guo-dong ; Chen, Xue-gang ; Li, Jun ; Yan, Rui-fang</creatorcontrib><description>Die forging is a processing method that can produce a size and shape close to the finished product and improve the mechanical properties of the alloy. In this paper, Mg–8Al-0.5Zn magnesium alloy was used to prepare stepped shaft by isothermal die forging. The microstructure and stress-strain state of different parts of stepped shaft forging were analyzed. The metal rheological law and microstructure evolution mechanism of AZ80 alloy during die forging were discussed. At the position of low stress and high strain state of the die forging, continuous dynamic recrystallization (CDRX) is the main deformation mechanism, and the microstructure is mainly composed of coarse un-dynamic recrystallized (unDRXed) grains and fine equiaxed dynamic recrystallized (DRXed) grains. The unDRXed grains have a strong basal texture, while the DRXed grains exhibit random orientations. At the position of high stress and low strain state of the die forging, {10–12} twinning is the main deformation mechanism, the parent grains show a strong basal texture, while {10–12} twins present [-12-10]-[01–10] double fiber texture parallel to forging direction (FD). The compressive strength and yield strength of the part in the low stress and high strain state are higher than those in the high stress and low strain state, but the fracture strain of the former is lower than that of the latter. The results of this study can provide a reference for the design of die forging die together with the blank shape and size, so as to meet the corresponding performance requirements of different parts of the die forging.</description><identifier>ISSN: 0921-5093</identifier><identifier>EISSN: 1873-4936</identifier><identifier>DOI: 10.1016/j.msea.2023.144789</identifier><language>eng</language><publisher>Elsevier B.V</publisher><subject>Deformation mechanism ; Die forging ; Microstructure evolution</subject><ispartof>Materials science &amp; engineering. A, Structural materials : properties, microstructure and processing, 2023-03, Vol.869, p.144789, Article 144789</ispartof><rights>2023 Elsevier B.V.</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c300t-4169a8250b51ed03462d2acd1c19c2bbef142a4e23840f3751b8ff659072c65e3</citedby><cites>FETCH-LOGICAL-c300t-4169a8250b51ed03462d2acd1c19c2bbef142a4e23840f3751b8ff659072c65e3</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,780,784,27924,27925</link.rule.ids></links><search><creatorcontrib>Li, Zhu-jin</creatorcontrib><creatorcontrib>Wang, Jin-guo</creatorcontrib><creatorcontrib>Ni, Tian-yi</creatorcontrib><creatorcontrib>Zhang, Wei</creatorcontrib><creatorcontrib>Tong, Guo-dong</creatorcontrib><creatorcontrib>Chen, Xue-gang</creatorcontrib><creatorcontrib>Li, Jun</creatorcontrib><creatorcontrib>Yan, Rui-fang</creatorcontrib><title>Microstructure evolution and deformation mechanism of AZ80 alloy during die forging</title><title>Materials science &amp; engineering. A, Structural materials : properties, microstructure and processing</title><description>Die forging is a processing method that can produce a size and shape close to the finished product and improve the mechanical properties of the alloy. In this paper, Mg–8Al-0.5Zn magnesium alloy was used to prepare stepped shaft by isothermal die forging. The microstructure and stress-strain state of different parts of stepped shaft forging were analyzed. The metal rheological law and microstructure evolution mechanism of AZ80 alloy during die forging were discussed. At the position of low stress and high strain state of the die forging, continuous dynamic recrystallization (CDRX) is the main deformation mechanism, and the microstructure is mainly composed of coarse un-dynamic recrystallized (unDRXed) grains and fine equiaxed dynamic recrystallized (DRXed) grains. The unDRXed grains have a strong basal texture, while the DRXed grains exhibit random orientations. At the position of high stress and low strain state of the die forging, {10–12} twinning is the main deformation mechanism, the parent grains show a strong basal texture, while {10–12} twins present [-12-10]-[01–10] double fiber texture parallel to forging direction (FD). The compressive strength and yield strength of the part in the low stress and high strain state are higher than those in the high stress and low strain state, but the fracture strain of the former is lower than that of the latter. The results of this study can provide a reference for the design of die forging die together with the blank shape and size, so as to meet the corresponding performance requirements of different parts of the die forging.</description><subject>Deformation mechanism</subject><subject>Die forging</subject><subject>Microstructure evolution</subject><issn>0921-5093</issn><issn>1873-4936</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2023</creationdate><recordtype>article</recordtype><recordid>eNp9kE1LAzEQhoMoWKt_wFP-wK6Tj_0CL6WoFSoe1IuXkE0mNWU_JNkt9N-7az17mhl4n2HmIeSWQcqA5Xf7tI2oUw5cpEzKoqzOyIKVhUhkJfJzsoCKsySDSlySqxj3AMAkZAvy9uJN6OMQRjOMASke-mYcfN9R3Vlq0fWh1b9zi-ZLdz62tHd09VkC1U3TH6kdg-921HqkU3g39dfkwukm4s1fXZKPx4f39SbZvj49r1fbxAiAIZEsr3TJM6gzhhaEzLnl2lhmWGV4XaNjkmuJXJQSnCgyVpfO5VkFBTd5hmJJ-Gnv_EEM6NR38K0OR8VAzVrUXs1a1KxFnbRM0P0Jwumyg8egovHYGbQ-oBmU7f1_-A-QdGv9</recordid><startdate>20230324</startdate><enddate>20230324</enddate><creator>Li, Zhu-jin</creator><creator>Wang, Jin-guo</creator><creator>Ni, Tian-yi</creator><creator>Zhang, Wei</creator><creator>Tong, Guo-dong</creator><creator>Chen, Xue-gang</creator><creator>Li, Jun</creator><creator>Yan, Rui-fang</creator><general>Elsevier B.V</general><scope>AAYXX</scope><scope>CITATION</scope></search><sort><creationdate>20230324</creationdate><title>Microstructure evolution and deformation mechanism of AZ80 alloy during die forging</title><author>Li, Zhu-jin ; Wang, Jin-guo ; Ni, Tian-yi ; Zhang, Wei ; Tong, Guo-dong ; Chen, Xue-gang ; Li, Jun ; Yan, Rui-fang</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c300t-4169a8250b51ed03462d2acd1c19c2bbef142a4e23840f3751b8ff659072c65e3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2023</creationdate><topic>Deformation mechanism</topic><topic>Die forging</topic><topic>Microstructure evolution</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Li, Zhu-jin</creatorcontrib><creatorcontrib>Wang, Jin-guo</creatorcontrib><creatorcontrib>Ni, Tian-yi</creatorcontrib><creatorcontrib>Zhang, Wei</creatorcontrib><creatorcontrib>Tong, Guo-dong</creatorcontrib><creatorcontrib>Chen, Xue-gang</creatorcontrib><creatorcontrib>Li, Jun</creatorcontrib><creatorcontrib>Yan, Rui-fang</creatorcontrib><collection>CrossRef</collection><jtitle>Materials science &amp; engineering. A, Structural materials : properties, microstructure and processing</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Li, Zhu-jin</au><au>Wang, Jin-guo</au><au>Ni, Tian-yi</au><au>Zhang, Wei</au><au>Tong, Guo-dong</au><au>Chen, Xue-gang</au><au>Li, Jun</au><au>Yan, Rui-fang</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Microstructure evolution and deformation mechanism of AZ80 alloy during die forging</atitle><jtitle>Materials science &amp; engineering. A, Structural materials : properties, microstructure and processing</jtitle><date>2023-03-24</date><risdate>2023</risdate><volume>869</volume><spage>144789</spage><pages>144789-</pages><artnum>144789</artnum><issn>0921-5093</issn><eissn>1873-4936</eissn><abstract>Die forging is a processing method that can produce a size and shape close to the finished product and improve the mechanical properties of the alloy. In this paper, Mg–8Al-0.5Zn magnesium alloy was used to prepare stepped shaft by isothermal die forging. The microstructure and stress-strain state of different parts of stepped shaft forging were analyzed. The metal rheological law and microstructure evolution mechanism of AZ80 alloy during die forging were discussed. At the position of low stress and high strain state of the die forging, continuous dynamic recrystallization (CDRX) is the main deformation mechanism, and the microstructure is mainly composed of coarse un-dynamic recrystallized (unDRXed) grains and fine equiaxed dynamic recrystallized (DRXed) grains. The unDRXed grains have a strong basal texture, while the DRXed grains exhibit random orientations. At the position of high stress and low strain state of the die forging, {10–12} twinning is the main deformation mechanism, the parent grains show a strong basal texture, while {10–12} twins present [-12-10]-[01–10] double fiber texture parallel to forging direction (FD). The compressive strength and yield strength of the part in the low stress and high strain state are higher than those in the high stress and low strain state, but the fracture strain of the former is lower than that of the latter. The results of this study can provide a reference for the design of die forging die together with the blank shape and size, so as to meet the corresponding performance requirements of different parts of the die forging.</abstract><pub>Elsevier B.V</pub><doi>10.1016/j.msea.2023.144789</doi></addata></record>
fulltext fulltext
identifier ISSN: 0921-5093
ispartof Materials science & engineering. A, Structural materials : properties, microstructure and processing, 2023-03, Vol.869, p.144789, Article 144789
issn 0921-5093
1873-4936
language eng
recordid cdi_crossref_primary_10_1016_j_msea_2023_144789
source ScienceDirect Freedom Collection
subjects Deformation mechanism
Die forging
Microstructure evolution
title Microstructure evolution and deformation mechanism of AZ80 alloy during die forging
url http://sfxeu10.hosted.exlibrisgroup.com/loughborough?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-20T18%3A20%3A04IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-elsevier_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Microstructure%20evolution%20and%20deformation%20mechanism%20of%20AZ80%20alloy%20during%20die%20forging&rft.jtitle=Materials%20science%20&%20engineering.%20A,%20Structural%20materials%20:%20properties,%20microstructure%20and%20processing&rft.au=Li,%20Zhu-jin&rft.date=2023-03-24&rft.volume=869&rft.spage=144789&rft.pages=144789-&rft.artnum=144789&rft.issn=0921-5093&rft.eissn=1873-4936&rft_id=info:doi/10.1016/j.msea.2023.144789&rft_dat=%3Celsevier_cross%3ES0921509323002137%3C/elsevier_cross%3E%3Cgrp_id%3Ecdi_FETCH-LOGICAL-c300t-4169a8250b51ed03462d2acd1c19c2bbef142a4e23840f3751b8ff659072c65e3%3C/grp_id%3E%3Coa%3E%3C/oa%3E%3Curl%3E%3C/url%3E&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true