Ultra-low thermal conductivity and improved thermoelectric performance in La2O3-dispersed Bi2Sr2Co2Oy ceramics

•Grain refinement effect of La2O3 dispersant.•Ultra-low thermal conductivity (κ) caused by enhanced phonon scattering.•The optimized ZT value is improved by 21 % compared with the pristine Bi2Sr2Co2Oy. Thermoelectric materials are functional materials that directly convert heat energy and electric e...

Full description

Saved in:
Bibliographic Details
Published in:Materials science & engineering. B, Solid-state materials for advanced technology Solid-state materials for advanced technology, 2024-01, Vol.299, p.116976, Article 116976
Main Authors: He, Qinglin, Yang, Delin, Xia, Siyi, Song, Hongzhang
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:•Grain refinement effect of La2O3 dispersant.•Ultra-low thermal conductivity (κ) caused by enhanced phonon scattering.•The optimized ZT value is improved by 21 % compared with the pristine Bi2Sr2Co2Oy. Thermoelectric materials are functional materials that directly convert heat energy and electric energy into each other. Nano-second-phase dispersion is an effective strategy to improve the energy conversion efficiency of thermoelectric materials through the energy filtering effect and the phonon scattering effect. In this study, the solid-state reaction method was used to prepare Bi2Sr2Co2Oy + l wt% La2O3 (l = 0.0, 0.1, 0.25, 0.5, 1.75) thermoelectric composites. An ultra-low thermal conductivity of 0.58 W/Km at 923 K was obtained by dispersing a small quantity of La2O3 as the nano-second-phase additive in the Bi2Sr2Co2Oy matrix. This was attributed to the increased hetero-interfaces and improved phonon scattering through the grain refinement effect. The dimensionless thermoelectric figure of merit (ZT) values of Bi2Sr2Co2Oy + 0.25 wt% La2O3 reached 0.28 at 923 K when their power factors were combined with littlechange, which was 21 % higher than that of the un-optimised pristine Bi2Sr2Co2Oy.
ISSN:0921-5107
1873-4944
DOI:10.1016/j.mseb.2023.116976