Fabrication of Al/BN composite strips and evaluation of fracture toughness and forming limit diagram

In this study, mechanical properties, fracture toughness (FT) and forming limit diagram (FLD) of Al base composites manufactured by accumulative roll bonding (ARB) have been studies experimentally. AA1100/BN composite strips have been manufactured with thickness of 1 mm up to 10 ARB cycles at 300°C....

Full description

Saved in:
Bibliographic Details
Published in:Materials today communications 2023-12, Vol.37, p.107457, Article 107457
Main Authors: Daneshmand, Saeed, Vini, Mohammad Heydari, Bravo-Apaza, Jinmer, Carbajal, Nestor Cuba, Kumar, Abhinav, Abdulameer, Sajjad Firas
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
cited_by
cites cdi_FETCH-LOGICAL-c255t-b3f7a25379f242faaee4fb1659c175d63974d4033cc5f916d70aa82261422863
container_end_page
container_issue
container_start_page 107457
container_title Materials today communications
container_volume 37
creator Daneshmand, Saeed
Vini, Mohammad Heydari
Bravo-Apaza, Jinmer
Carbajal, Nestor Cuba
Kumar, Abhinav
Abdulameer, Sajjad Firas
description In this study, mechanical properties, fracture toughness (FT) and forming limit diagram (FLD) of Al base composites manufactured by accumulative roll bonding (ARB) have been studies experimentally. AA1100/BN composite strips have been manufactured with thickness of 1 mm up to 10 ARB cycles at 300°C. Their strength enhanced to 168 MPa which was 248 % enhancement than the primary aluminum alloy 1100. Also, the bonding between layers enhanced by fabrication of thin layers through the thickness of composites with more plastic strains. SEM fracture morphology of composites showed that a shear ductile fracture was achieved at higher passes. So, relative to the annealed sample, deep dimples are shrinking slowly. UTS, elongation and hardness of samples improved to 169 MPa, 11.4 % and 55.6 HV after the 10 cycle, respectively. After the first pass as the criterion of formability, the area under the FLDs dropped sharply and then enhanced at higher passes. Based on the results obtained FT enhanced to 30 MPam12 at the 10th pass. [Display omitted]
doi_str_mv 10.1016/j.mtcomm.2023.107457
format article
fullrecord <record><control><sourceid>elsevier_cross</sourceid><recordid>TN_cdi_crossref_primary_10_1016_j_mtcomm_2023_107457</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S2352492823021487</els_id><sourcerecordid>S2352492823021487</sourcerecordid><originalsourceid>FETCH-LOGICAL-c255t-b3f7a25379f242faaee4fb1659c175d63974d4033cc5f916d70aa82261422863</originalsourceid><addsrcrecordid>eNp9kM1KAzEURoMoWGrfwEVeYNr8TmY2Qi1WhaKb7kMmk9SUyaQkacG38Vl8MqeOiCtX93L5vsPlAHCL0RwjXC72c5918H5OEKHDSTAuLsCEUE4KVpPq8s9-DWYp7RFCuOKI1WwCzFo10WmVXehhsHDZLe5f4MA7hOSygSlHd0hQ9e3nhzmp7vibtFHpfIwG5nDcvfUmfaegDdG7fgc7512GrVO7qPwNuLKqS2b2M6dgu37Yrp6Kzevj82q5KTThPBcNtUIRTkVtCSNWKWOYbXDJa40Fb0taC9YyRKnW3Na4bAVSqiKkxIyQqqRTwEasjiGlaKw8ROdVfJcYybMsuZejLHmWJUdZQ-1urJnhtZMzUSbtTK9N66LRWbbB_Q_4AhgVdkM</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Fabrication of Al/BN composite strips and evaluation of fracture toughness and forming limit diagram</title><source>Elsevier</source><creator>Daneshmand, Saeed ; Vini, Mohammad Heydari ; Bravo-Apaza, Jinmer ; Carbajal, Nestor Cuba ; Kumar, Abhinav ; Abdulameer, Sajjad Firas</creator><creatorcontrib>Daneshmand, Saeed ; Vini, Mohammad Heydari ; Bravo-Apaza, Jinmer ; Carbajal, Nestor Cuba ; Kumar, Abhinav ; Abdulameer, Sajjad Firas</creatorcontrib><description>In this study, mechanical properties, fracture toughness (FT) and forming limit diagram (FLD) of Al base composites manufactured by accumulative roll bonding (ARB) have been studies experimentally. AA1100/BN composite strips have been manufactured with thickness of 1 mm up to 10 ARB cycles at 300°C. Their strength enhanced to 168 MPa which was 248 % enhancement than the primary aluminum alloy 1100. Also, the bonding between layers enhanced by fabrication of thin layers through the thickness of composites with more plastic strains. SEM fracture morphology of composites showed that a shear ductile fracture was achieved at higher passes. So, relative to the annealed sample, deep dimples are shrinking slowly. UTS, elongation and hardness of samples improved to 169 MPa, 11.4 % and 55.6 HV after the 10 cycle, respectively. After the first pass as the criterion of formability, the area under the FLDs dropped sharply and then enhanced at higher passes. Based on the results obtained FT enhanced to 30 MPam12 at the 10th pass. [Display omitted]</description><identifier>ISSN: 2352-4928</identifier><identifier>EISSN: 2352-4928</identifier><identifier>DOI: 10.1016/j.mtcomm.2023.107457</identifier><language>eng</language><publisher>Elsevier Ltd</publisher><subject>Accumulative roll bonding (ARB) ; Forming limit diagram (FLD) ; Fracture toughness (FT) ; Hardness ; Mechanical properties</subject><ispartof>Materials today communications, 2023-12, Vol.37, p.107457, Article 107457</ispartof><rights>2023 Elsevier Ltd</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><cites>FETCH-LOGICAL-c255t-b3f7a25379f242faaee4fb1659c175d63974d4033cc5f916d70aa82261422863</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,780,784,27923,27924</link.rule.ids></links><search><creatorcontrib>Daneshmand, Saeed</creatorcontrib><creatorcontrib>Vini, Mohammad Heydari</creatorcontrib><creatorcontrib>Bravo-Apaza, Jinmer</creatorcontrib><creatorcontrib>Carbajal, Nestor Cuba</creatorcontrib><creatorcontrib>Kumar, Abhinav</creatorcontrib><creatorcontrib>Abdulameer, Sajjad Firas</creatorcontrib><title>Fabrication of Al/BN composite strips and evaluation of fracture toughness and forming limit diagram</title><title>Materials today communications</title><description>In this study, mechanical properties, fracture toughness (FT) and forming limit diagram (FLD) of Al base composites manufactured by accumulative roll bonding (ARB) have been studies experimentally. AA1100/BN composite strips have been manufactured with thickness of 1 mm up to 10 ARB cycles at 300°C. Their strength enhanced to 168 MPa which was 248 % enhancement than the primary aluminum alloy 1100. Also, the bonding between layers enhanced by fabrication of thin layers through the thickness of composites with more plastic strains. SEM fracture morphology of composites showed that a shear ductile fracture was achieved at higher passes. So, relative to the annealed sample, deep dimples are shrinking slowly. UTS, elongation and hardness of samples improved to 169 MPa, 11.4 % and 55.6 HV after the 10 cycle, respectively. After the first pass as the criterion of formability, the area under the FLDs dropped sharply and then enhanced at higher passes. Based on the results obtained FT enhanced to 30 MPam12 at the 10th pass. [Display omitted]</description><subject>Accumulative roll bonding (ARB)</subject><subject>Forming limit diagram (FLD)</subject><subject>Fracture toughness (FT)</subject><subject>Hardness</subject><subject>Mechanical properties</subject><issn>2352-4928</issn><issn>2352-4928</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2023</creationdate><recordtype>article</recordtype><recordid>eNp9kM1KAzEURoMoWGrfwEVeYNr8TmY2Qi1WhaKb7kMmk9SUyaQkacG38Vl8MqeOiCtX93L5vsPlAHCL0RwjXC72c5918H5OEKHDSTAuLsCEUE4KVpPq8s9-DWYp7RFCuOKI1WwCzFo10WmVXehhsHDZLe5f4MA7hOSygSlHd0hQ9e3nhzmp7vibtFHpfIwG5nDcvfUmfaegDdG7fgc7512GrVO7qPwNuLKqS2b2M6dgu37Yrp6Kzevj82q5KTThPBcNtUIRTkVtCSNWKWOYbXDJa40Fb0taC9YyRKnW3Na4bAVSqiKkxIyQqqRTwEasjiGlaKw8ROdVfJcYybMsuZejLHmWJUdZQ-1urJnhtZMzUSbtTK9N66LRWbbB_Q_4AhgVdkM</recordid><startdate>202312</startdate><enddate>202312</enddate><creator>Daneshmand, Saeed</creator><creator>Vini, Mohammad Heydari</creator><creator>Bravo-Apaza, Jinmer</creator><creator>Carbajal, Nestor Cuba</creator><creator>Kumar, Abhinav</creator><creator>Abdulameer, Sajjad Firas</creator><general>Elsevier Ltd</general><scope>AAYXX</scope><scope>CITATION</scope></search><sort><creationdate>202312</creationdate><title>Fabrication of Al/BN composite strips and evaluation of fracture toughness and forming limit diagram</title><author>Daneshmand, Saeed ; Vini, Mohammad Heydari ; Bravo-Apaza, Jinmer ; Carbajal, Nestor Cuba ; Kumar, Abhinav ; Abdulameer, Sajjad Firas</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c255t-b3f7a25379f242faaee4fb1659c175d63974d4033cc5f916d70aa82261422863</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2023</creationdate><topic>Accumulative roll bonding (ARB)</topic><topic>Forming limit diagram (FLD)</topic><topic>Fracture toughness (FT)</topic><topic>Hardness</topic><topic>Mechanical properties</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Daneshmand, Saeed</creatorcontrib><creatorcontrib>Vini, Mohammad Heydari</creatorcontrib><creatorcontrib>Bravo-Apaza, Jinmer</creatorcontrib><creatorcontrib>Carbajal, Nestor Cuba</creatorcontrib><creatorcontrib>Kumar, Abhinav</creatorcontrib><creatorcontrib>Abdulameer, Sajjad Firas</creatorcontrib><collection>CrossRef</collection><jtitle>Materials today communications</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Daneshmand, Saeed</au><au>Vini, Mohammad Heydari</au><au>Bravo-Apaza, Jinmer</au><au>Carbajal, Nestor Cuba</au><au>Kumar, Abhinav</au><au>Abdulameer, Sajjad Firas</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Fabrication of Al/BN composite strips and evaluation of fracture toughness and forming limit diagram</atitle><jtitle>Materials today communications</jtitle><date>2023-12</date><risdate>2023</risdate><volume>37</volume><spage>107457</spage><pages>107457-</pages><artnum>107457</artnum><issn>2352-4928</issn><eissn>2352-4928</eissn><abstract>In this study, mechanical properties, fracture toughness (FT) and forming limit diagram (FLD) of Al base composites manufactured by accumulative roll bonding (ARB) have been studies experimentally. AA1100/BN composite strips have been manufactured with thickness of 1 mm up to 10 ARB cycles at 300°C. Their strength enhanced to 168 MPa which was 248 % enhancement than the primary aluminum alloy 1100. Also, the bonding between layers enhanced by fabrication of thin layers through the thickness of composites with more plastic strains. SEM fracture morphology of composites showed that a shear ductile fracture was achieved at higher passes. So, relative to the annealed sample, deep dimples are shrinking slowly. UTS, elongation and hardness of samples improved to 169 MPa, 11.4 % and 55.6 HV after the 10 cycle, respectively. After the first pass as the criterion of formability, the area under the FLDs dropped sharply and then enhanced at higher passes. Based on the results obtained FT enhanced to 30 MPam12 at the 10th pass. [Display omitted]</abstract><pub>Elsevier Ltd</pub><doi>10.1016/j.mtcomm.2023.107457</doi></addata></record>
fulltext fulltext
identifier ISSN: 2352-4928
ispartof Materials today communications, 2023-12, Vol.37, p.107457, Article 107457
issn 2352-4928
2352-4928
language eng
recordid cdi_crossref_primary_10_1016_j_mtcomm_2023_107457
source Elsevier
subjects Accumulative roll bonding (ARB)
Forming limit diagram (FLD)
Fracture toughness (FT)
Hardness
Mechanical properties
title Fabrication of Al/BN composite strips and evaluation of fracture toughness and forming limit diagram
url http://sfxeu10.hosted.exlibrisgroup.com/loughborough?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-11T12%3A31%3A57IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-elsevier_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Fabrication%20of%20Al/BN%20composite%20strips%20and%C2%A0evaluation%20of%20fracture%20toughness%20and%20forming%20limit%20diagram&rft.jtitle=Materials%20today%20communications&rft.au=Daneshmand,%20Saeed&rft.date=2023-12&rft.volume=37&rft.spage=107457&rft.pages=107457-&rft.artnum=107457&rft.issn=2352-4928&rft.eissn=2352-4928&rft_id=info:doi/10.1016/j.mtcomm.2023.107457&rft_dat=%3Celsevier_cross%3ES2352492823021487%3C/elsevier_cross%3E%3Cgrp_id%3Ecdi_FETCH-LOGICAL-c255t-b3f7a25379f242faaee4fb1659c175d63974d4033cc5f916d70aa82261422863%3C/grp_id%3E%3Coa%3E%3C/oa%3E%3Curl%3E%3C/url%3E&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true