Optical transmission and photoconductivity of chemical bath-deposited CdS thin films for optoelectronic applications

•Chemical bath-deposited CdS films show an optical energy band gap of 2.42 eV.•The CdS films show optical transmission of 75 % in the 500–900 nm wavelength range.•We have studied the wavelength dependence of photoconductivity of these CdS films.•Photoconductivity peaks at 492 nm showing an electrica...

Full description

Saved in:
Bibliographic Details
Published in:Thin solid films 2024-02, Vol.791, p.140225, Article 140225
Main Authors: Dissanayake, M.A.K.L., Paramanathan, K., Senadeera, G.K.R., Thotawattage, C.A., Balashangar, K., Ravirajan, P., Dassanayake, B.S.
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
cited_by cdi_FETCH-LOGICAL-c297t-792d57169baebe0c7cd0a28c89372eb178e04ecb97decbf82b581a80557e1b3b3
cites cdi_FETCH-LOGICAL-c297t-792d57169baebe0c7cd0a28c89372eb178e04ecb97decbf82b581a80557e1b3b3
container_end_page
container_issue
container_start_page 140225
container_title Thin solid films
container_volume 791
creator Dissanayake, M.A.K.L.
Paramanathan, K.
Senadeera, G.K.R.
Thotawattage, C.A.
Balashangar, K.
Ravirajan, P.
Dassanayake, B.S.
description •Chemical bath-deposited CdS films show an optical energy band gap of 2.42 eV.•The CdS films show optical transmission of 75 % in the 500–900 nm wavelength range.•We have studied the wavelength dependence of photoconductivity of these CdS films.•Photoconductivity peaks at 492 nm showing an electrical energy band gap of 2.52 eV.•Annealed CdS films show improved conductivity, carrier concentration, and mobility. This paper presents a comprehensive study of the optical transmission, photoconductivity, and morphology of CdS thin films deposited via the chemical bath deposition (CBD) method. The films deposited for 60 min exhibit an optical energy band gap value of 2.42 eV and the highest optical transmission of 75 % in the wavelength range of 500–900 nm. For these films, the transmission electron microscopy imaging shows a distribution of particle sizes around 10 nm. The wavelength dependence of the photoconductivity, extracted from photo resistivity data, shows that the maximum photoconductivity occurs at 492 nm wavelength. This corresponds to an electrical energy band gap of 2.52 eV, which is greater than the optically measured energy gap of 2.42 eV. Based on these results, the electron-hole pair binding energy for CdS films is estimated as 100 meV. According to the electrical resistivity vs. temperature measurements, the activation energy is 1.26 eV which agrees with the electrical energy band gap of 2.52 eV. CdS films annealed under nitrogen gas at 200 °C for one hour exhibited an energy gap of 2.32 eV. These films displayed a conductivity of 60 × 10−4 Scm−1, a carrier concentration of 6.38 × 1014 cm−3, and a mobility of 7.46 cm2 V−1 s−1. These impressive characteristics suggest the suitability of CBD-grown CdS films annealed at 200 °C in nitrogen gas, to be used as the window material in CdS/CdTe thin film solar cells and other optoelectronic applications.
doi_str_mv 10.1016/j.tsf.2024.140225
format article
fullrecord <record><control><sourceid>elsevier_cross</sourceid><recordid>TN_cdi_crossref_primary_10_1016_j_tsf_2024_140225</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S0040609024000270</els_id><sourcerecordid>S0040609024000270</sourcerecordid><originalsourceid>FETCH-LOGICAL-c297t-792d57169baebe0c7cd0a28c89372eb178e04ecb97decbf82b581a80557e1b3b3</originalsourceid><addsrcrecordid>eNp9kMtOwzAQRS0EEqXwAez8AwljJ6kTsUIRL6lSF8Da8mOiuEriyDaV-veklDWbuZs5VzOHkHsGOQO2edjnKXY5B17mrATOqwuyYrVoMi4KdklWACVkG2jgmtzEuAcAxnmxImk3J2fUQFNQUxxdjM5PVE2Wzr1P3vjJfpvkDi4dqe-o6XH8Xdcq9ZnF2UeX0NLWftDUu4l2bhgj7Xygfk4eBzQp-MkZquZ5WMi01MdbctWpIeLdX67J18vzZ_uWbXev7-3TNjO8ESkTDbeVYJtGK9QIRhgLitembgrBUTNRI5RodCPsMrua66pmqoaqEsh0oYs1YedeE3yMATs5BzeqcJQM5Emb3MtFmzxpk2dtC_N4ZnA57OAwyGgcTgatC8sz0nr3D_0DyS95RA</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Optical transmission and photoconductivity of chemical bath-deposited CdS thin films for optoelectronic applications</title><source>ScienceDirect Freedom Collection</source><creator>Dissanayake, M.A.K.L. ; Paramanathan, K. ; Senadeera, G.K.R. ; Thotawattage, C.A. ; Balashangar, K. ; Ravirajan, P. ; Dassanayake, B.S.</creator><creatorcontrib>Dissanayake, M.A.K.L. ; Paramanathan, K. ; Senadeera, G.K.R. ; Thotawattage, C.A. ; Balashangar, K. ; Ravirajan, P. ; Dassanayake, B.S.</creatorcontrib><description>•Chemical bath-deposited CdS films show an optical energy band gap of 2.42 eV.•The CdS films show optical transmission of 75 % in the 500–900 nm wavelength range.•We have studied the wavelength dependence of photoconductivity of these CdS films.•Photoconductivity peaks at 492 nm showing an electrical energy band gap of 2.52 eV.•Annealed CdS films show improved conductivity, carrier concentration, and mobility. This paper presents a comprehensive study of the optical transmission, photoconductivity, and morphology of CdS thin films deposited via the chemical bath deposition (CBD) method. The films deposited for 60 min exhibit an optical energy band gap value of 2.42 eV and the highest optical transmission of 75 % in the wavelength range of 500–900 nm. For these films, the transmission electron microscopy imaging shows a distribution of particle sizes around 10 nm. The wavelength dependence of the photoconductivity, extracted from photo resistivity data, shows that the maximum photoconductivity occurs at 492 nm wavelength. This corresponds to an electrical energy band gap of 2.52 eV, which is greater than the optically measured energy gap of 2.42 eV. Based on these results, the electron-hole pair binding energy for CdS films is estimated as 100 meV. According to the electrical resistivity vs. temperature measurements, the activation energy is 1.26 eV which agrees with the electrical energy band gap of 2.52 eV. CdS films annealed under nitrogen gas at 200 °C for one hour exhibited an energy gap of 2.32 eV. These films displayed a conductivity of 60 × 10−4 Scm−1, a carrier concentration of 6.38 × 1014 cm−3, and a mobility of 7.46 cm2 V−1 s−1. These impressive characteristics suggest the suitability of CBD-grown CdS films annealed at 200 °C in nitrogen gas, to be used as the window material in CdS/CdTe thin film solar cells and other optoelectronic applications.</description><identifier>ISSN: 0040-6090</identifier><identifier>EISSN: 1879-2731</identifier><identifier>DOI: 10.1016/j.tsf.2024.140225</identifier><language>eng</language><publisher>Elsevier B.V</publisher><subject>Cadmium sulfide ; Chemical bath deposition ; Energy band gap ; Grain size ; Optical transmission ; Photoconductivity</subject><ispartof>Thin solid films, 2024-02, Vol.791, p.140225, Article 140225</ispartof><rights>2024 Elsevier B.V.</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c297t-792d57169baebe0c7cd0a28c89372eb178e04ecb97decbf82b581a80557e1b3b3</citedby><cites>FETCH-LOGICAL-c297t-792d57169baebe0c7cd0a28c89372eb178e04ecb97decbf82b581a80557e1b3b3</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,780,784,27923,27924</link.rule.ids></links><search><creatorcontrib>Dissanayake, M.A.K.L.</creatorcontrib><creatorcontrib>Paramanathan, K.</creatorcontrib><creatorcontrib>Senadeera, G.K.R.</creatorcontrib><creatorcontrib>Thotawattage, C.A.</creatorcontrib><creatorcontrib>Balashangar, K.</creatorcontrib><creatorcontrib>Ravirajan, P.</creatorcontrib><creatorcontrib>Dassanayake, B.S.</creatorcontrib><title>Optical transmission and photoconductivity of chemical bath-deposited CdS thin films for optoelectronic applications</title><title>Thin solid films</title><description>•Chemical bath-deposited CdS films show an optical energy band gap of 2.42 eV.•The CdS films show optical transmission of 75 % in the 500–900 nm wavelength range.•We have studied the wavelength dependence of photoconductivity of these CdS films.•Photoconductivity peaks at 492 nm showing an electrical energy band gap of 2.52 eV.•Annealed CdS films show improved conductivity, carrier concentration, and mobility. This paper presents a comprehensive study of the optical transmission, photoconductivity, and morphology of CdS thin films deposited via the chemical bath deposition (CBD) method. The films deposited for 60 min exhibit an optical energy band gap value of 2.42 eV and the highest optical transmission of 75 % in the wavelength range of 500–900 nm. For these films, the transmission electron microscopy imaging shows a distribution of particle sizes around 10 nm. The wavelength dependence of the photoconductivity, extracted from photo resistivity data, shows that the maximum photoconductivity occurs at 492 nm wavelength. This corresponds to an electrical energy band gap of 2.52 eV, which is greater than the optically measured energy gap of 2.42 eV. Based on these results, the electron-hole pair binding energy for CdS films is estimated as 100 meV. According to the electrical resistivity vs. temperature measurements, the activation energy is 1.26 eV which agrees with the electrical energy band gap of 2.52 eV. CdS films annealed under nitrogen gas at 200 °C for one hour exhibited an energy gap of 2.32 eV. These films displayed a conductivity of 60 × 10−4 Scm−1, a carrier concentration of 6.38 × 1014 cm−3, and a mobility of 7.46 cm2 V−1 s−1. These impressive characteristics suggest the suitability of CBD-grown CdS films annealed at 200 °C in nitrogen gas, to be used as the window material in CdS/CdTe thin film solar cells and other optoelectronic applications.</description><subject>Cadmium sulfide</subject><subject>Chemical bath deposition</subject><subject>Energy band gap</subject><subject>Grain size</subject><subject>Optical transmission</subject><subject>Photoconductivity</subject><issn>0040-6090</issn><issn>1879-2731</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2024</creationdate><recordtype>article</recordtype><recordid>eNp9kMtOwzAQRS0EEqXwAez8AwljJ6kTsUIRL6lSF8Da8mOiuEriyDaV-veklDWbuZs5VzOHkHsGOQO2edjnKXY5B17mrATOqwuyYrVoMi4KdklWACVkG2jgmtzEuAcAxnmxImk3J2fUQFNQUxxdjM5PVE2Wzr1P3vjJfpvkDi4dqe-o6XH8Xdcq9ZnF2UeX0NLWftDUu4l2bhgj7Xygfk4eBzQp-MkZquZ5WMi01MdbctWpIeLdX67J18vzZ_uWbXev7-3TNjO8ESkTDbeVYJtGK9QIRhgLitembgrBUTNRI5RodCPsMrua66pmqoaqEsh0oYs1YedeE3yMATs5BzeqcJQM5Emb3MtFmzxpk2dtC_N4ZnA57OAwyGgcTgatC8sz0nr3D_0DyS95RA</recordid><startdate>20240229</startdate><enddate>20240229</enddate><creator>Dissanayake, M.A.K.L.</creator><creator>Paramanathan, K.</creator><creator>Senadeera, G.K.R.</creator><creator>Thotawattage, C.A.</creator><creator>Balashangar, K.</creator><creator>Ravirajan, P.</creator><creator>Dassanayake, B.S.</creator><general>Elsevier B.V</general><scope>AAYXX</scope><scope>CITATION</scope></search><sort><creationdate>20240229</creationdate><title>Optical transmission and photoconductivity of chemical bath-deposited CdS thin films for optoelectronic applications</title><author>Dissanayake, M.A.K.L. ; Paramanathan, K. ; Senadeera, G.K.R. ; Thotawattage, C.A. ; Balashangar, K. ; Ravirajan, P. ; Dassanayake, B.S.</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c297t-792d57169baebe0c7cd0a28c89372eb178e04ecb97decbf82b581a80557e1b3b3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2024</creationdate><topic>Cadmium sulfide</topic><topic>Chemical bath deposition</topic><topic>Energy band gap</topic><topic>Grain size</topic><topic>Optical transmission</topic><topic>Photoconductivity</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Dissanayake, M.A.K.L.</creatorcontrib><creatorcontrib>Paramanathan, K.</creatorcontrib><creatorcontrib>Senadeera, G.K.R.</creatorcontrib><creatorcontrib>Thotawattage, C.A.</creatorcontrib><creatorcontrib>Balashangar, K.</creatorcontrib><creatorcontrib>Ravirajan, P.</creatorcontrib><creatorcontrib>Dassanayake, B.S.</creatorcontrib><collection>CrossRef</collection><jtitle>Thin solid films</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Dissanayake, M.A.K.L.</au><au>Paramanathan, K.</au><au>Senadeera, G.K.R.</au><au>Thotawattage, C.A.</au><au>Balashangar, K.</au><au>Ravirajan, P.</au><au>Dassanayake, B.S.</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Optical transmission and photoconductivity of chemical bath-deposited CdS thin films for optoelectronic applications</atitle><jtitle>Thin solid films</jtitle><date>2024-02-29</date><risdate>2024</risdate><volume>791</volume><spage>140225</spage><pages>140225-</pages><artnum>140225</artnum><issn>0040-6090</issn><eissn>1879-2731</eissn><abstract>•Chemical bath-deposited CdS films show an optical energy band gap of 2.42 eV.•The CdS films show optical transmission of 75 % in the 500–900 nm wavelength range.•We have studied the wavelength dependence of photoconductivity of these CdS films.•Photoconductivity peaks at 492 nm showing an electrical energy band gap of 2.52 eV.•Annealed CdS films show improved conductivity, carrier concentration, and mobility. This paper presents a comprehensive study of the optical transmission, photoconductivity, and morphology of CdS thin films deposited via the chemical bath deposition (CBD) method. The films deposited for 60 min exhibit an optical energy band gap value of 2.42 eV and the highest optical transmission of 75 % in the wavelength range of 500–900 nm. For these films, the transmission electron microscopy imaging shows a distribution of particle sizes around 10 nm. The wavelength dependence of the photoconductivity, extracted from photo resistivity data, shows that the maximum photoconductivity occurs at 492 nm wavelength. This corresponds to an electrical energy band gap of 2.52 eV, which is greater than the optically measured energy gap of 2.42 eV. Based on these results, the electron-hole pair binding energy for CdS films is estimated as 100 meV. According to the electrical resistivity vs. temperature measurements, the activation energy is 1.26 eV which agrees with the electrical energy band gap of 2.52 eV. CdS films annealed under nitrogen gas at 200 °C for one hour exhibited an energy gap of 2.32 eV. These films displayed a conductivity of 60 × 10−4 Scm−1, a carrier concentration of 6.38 × 1014 cm−3, and a mobility of 7.46 cm2 V−1 s−1. These impressive characteristics suggest the suitability of CBD-grown CdS films annealed at 200 °C in nitrogen gas, to be used as the window material in CdS/CdTe thin film solar cells and other optoelectronic applications.</abstract><pub>Elsevier B.V</pub><doi>10.1016/j.tsf.2024.140225</doi></addata></record>
fulltext fulltext
identifier ISSN: 0040-6090
ispartof Thin solid films, 2024-02, Vol.791, p.140225, Article 140225
issn 0040-6090
1879-2731
language eng
recordid cdi_crossref_primary_10_1016_j_tsf_2024_140225
source ScienceDirect Freedom Collection
subjects Cadmium sulfide
Chemical bath deposition
Energy band gap
Grain size
Optical transmission
Photoconductivity
title Optical transmission and photoconductivity of chemical bath-deposited CdS thin films for optoelectronic applications
url http://sfxeu10.hosted.exlibrisgroup.com/loughborough?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-11T05%3A17%3A40IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-elsevier_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Optical%20transmission%20and%20photoconductivity%20of%20chemical%20bath-deposited%20CdS%20thin%20films%20for%20optoelectronic%20applications&rft.jtitle=Thin%20solid%20films&rft.au=Dissanayake,%20M.A.K.L.&rft.date=2024-02-29&rft.volume=791&rft.spage=140225&rft.pages=140225-&rft.artnum=140225&rft.issn=0040-6090&rft.eissn=1879-2731&rft_id=info:doi/10.1016/j.tsf.2024.140225&rft_dat=%3Celsevier_cross%3ES0040609024000270%3C/elsevier_cross%3E%3Cgrp_id%3Ecdi_FETCH-LOGICAL-c297t-792d57169baebe0c7cd0a28c89372eb178e04ecb97decbf82b581a80557e1b3b3%3C/grp_id%3E%3Coa%3E%3C/oa%3E%3Curl%3E%3C/url%3E&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true