Correlation of Dielectric Confinement and Excitonic Binding Energy in 2D Layered Hybrid Perovskites Using Temperature Dependent Photoluminescence

In 2D layered hybrid perovskite like (PEA)2PbX4 (PEA = phenylethyl­ammonium, X = Cl, Br, I), the high frequency dielectric constants for inorganic well layer (εw) and organic barrier (εb) are distinctly different. The dielectric contrast significantly influences their excitonic binding energy (E ex...

Full description

Saved in:
Bibliographic Details
Published in:Journal of physical chemistry. C 2020-07, Vol.124 (29), p.16177-16185
Main Authors: Chakraborty, Rayan, Nag, Angshuman
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:In 2D layered hybrid perovskite like (PEA)2PbX4 (PEA = phenylethyl­ammonium, X = Cl, Br, I), the high frequency dielectric constants for inorganic well layer (εw) and organic barrier (εb) are distinctly different. The dielectric contrast significantly influences their excitonic binding energy (E ex 2D). Here we vary εw/εb by varying both the halide anion and the organic cation and then correlate the influence of the dielectric contrast on E ex 2D. We estimate E ex 2D by employing temperature (5.4–300 K) dependent photoluminescence (PL) and find that the change in E ex 2D can be qualitatively monitored simply by measuring the PL lifetime at room temperature. E ex 2D increases, and therefore, PL lifetime decreases by varying halide ions from Cl to Br to I for (PEA)2PbX4. Notably, this trend is opposite the case of 3D Pb-halide perovskites, where the excitonic binding energy decreases for X = Cl to Br to I. The opposite trend for 2D perovskites is explained by dielectric confinement, where we find E ex 2D ∝ (εw/εb) m , with m as an unknown positive number and εw > εb. The dielectric confinement drastically diminishes with increasing εb. (EA)2PbI4 (EA = ethanolammonium) with εb = 37.7 shows E ex 2D = 65 meV, as opposed to (PEA)2PbI4 with εb = 3.3 and E ex 2D = 453 meV. This correlation of εw/εb with E ex 2D is critical for optoelectronic applications of 2D layered perovskites.
ISSN:1932-7447
1932-7455
DOI:10.1021/acs.jpcc.0c04284