Loading…

Crazing and Toughness in Diblock Copolymer-Modified Semicrystalline Poly(l‑lactide)

Sustainable semicrystalline poly­(l-lactide) (PLLA) was melt mixed with 5 wt % poly­(ethylene oxide)-b-poly­(butylene oxide) (PEO-PBO) diblock copolymer, resulting in blends that display an exceptional combination of properties. The blends were annealed at various temperatures, leading to different...

Full description

Saved in:
Bibliographic Details
Published in:Macromolecules 2021-12, Vol.54 (23), p.11154-11169
Main Authors: McCutcheon, Charles J, Zhao, Boran, Ellison, Christopher J, Bates, Frank S
Format: Article
Language:English
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
cited_by cdi_FETCH-LOGICAL-a292t-e0be9dbbefead2bda1fb2962a79a27c04ae48684e5f60bf945a38387040c8ad93
cites cdi_FETCH-LOGICAL-a292t-e0be9dbbefead2bda1fb2962a79a27c04ae48684e5f60bf945a38387040c8ad93
container_end_page 11169
container_issue 23
container_start_page 11154
container_title Macromolecules
container_volume 54
creator McCutcheon, Charles J
Zhao, Boran
Ellison, Christopher J
Bates, Frank S
description Sustainable semicrystalline poly­(l-lactide) (PLLA) was melt mixed with 5 wt % poly­(ethylene oxide)-b-poly­(butylene oxide) (PEO-PBO) diblock copolymer, resulting in blends that display an exceptional combination of properties. The blends were annealed at various temperatures, leading to different degrees of crystallinity. The addition of 5 wt % PEO-PBO produced finely dispersed liquid particles that caused a significant reduction in the time for crystallization after quenching from the melt, where T m = 166 °C. At 95 °C, the halftime for crystallization was t 1/2(95 °C) = t 1/2 o/7, while at 135 °C, t 1/2(135 °C) = t 1/2 o/5, where t 1/2 o is the time required to obtain 50% of the final extent of crystallization with pure PLLA. The block copolymer particles also enhanced the ductility of the blends by facilitating stress-induced cavitation and uniform crazing without impacting the modulus. Tensile toughness increased by 7–15 fold, scaling inversely with the degree of crystallinity. The deformation mechanism was investigated by small- and wide-angle X-ray scattering as a function of applied strain, revealing that the craze volume is dependent on crystallinity, while the crystal structure displayed minimal changes. Regardless of the extent of crystallinity, crazing was found to be the primary deformation mechanism, countering the ductile-to-brittle transition associated with the aging of PLLA. Adding 5 wt % PEO-PBO extends the strain at break from 4% for pure PLLA after 2 days to more than approximately 50% after 85 or more days of aging. These findings, along with the industrially relevant blend preparation method, reveal that PEO-PBO is a unique and potent additive that could expand the applications served by PLLA, promoting a more sustainable future.
doi_str_mv 10.1021/acs.macromol.1c01702
format article
fullrecord <record><control><sourceid>acs_cross</sourceid><recordid>TN_cdi_crossref_primary_10_1021_acs_macromol_1c01702</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>b003507568</sourcerecordid><originalsourceid>FETCH-LOGICAL-a292t-e0be9dbbefead2bda1fb2962a79a27c04ae48684e5f60bf945a38387040c8ad93</originalsourceid><addsrcrecordid>eNp9kLFOwzAQhi0EEqXwBgweYUg5O04TjyhQQCoCiXaOLrZTXJy4stuhTLwCr8iTkKplZbrh7jv9_0fIJYMRA85uUMVRiyr41rsRU8By4EdkwDIOSVak2TEZAHCRSC7zU3IW4xKAsUykAzIvA37abkGx03TmN4v3zsRIbUfvbO28-qClX3m3bU1Inr22jTWavpnWqrCNa3TOdoa-9gdX7ufr26FaW22uz8lJgy6ai8MckvnkflY-JtOXh6fydpogl3ydGKiN1HVtGoOa1xpZU3M55phL5LkCgUYU40KYrBlD3UiRYVqkRQ4CVIFapkMi9n_77jEG01SrYFsM24pBtVNT9WqqPzXVQU2PwR7bbZd-E7o-5P_IL1Smbj4</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Crazing and Toughness in Diblock Copolymer-Modified Semicrystalline Poly(l‑lactide)</title><source>American Chemical Society:Jisc Collections:American Chemical Society Read &amp; Publish Agreement 2022-2024 (Reading list)</source><creator>McCutcheon, Charles J ; Zhao, Boran ; Ellison, Christopher J ; Bates, Frank S</creator><creatorcontrib>McCutcheon, Charles J ; Zhao, Boran ; Ellison, Christopher J ; Bates, Frank S</creatorcontrib><description>Sustainable semicrystalline poly­(l-lactide) (PLLA) was melt mixed with 5 wt % poly­(ethylene oxide)-b-poly­(butylene oxide) (PEO-PBO) diblock copolymer, resulting in blends that display an exceptional combination of properties. The blends were annealed at various temperatures, leading to different degrees of crystallinity. The addition of 5 wt % PEO-PBO produced finely dispersed liquid particles that caused a significant reduction in the time for crystallization after quenching from the melt, where T m = 166 °C. At 95 °C, the halftime for crystallization was t 1/2(95 °C) = t 1/2 o/7, while at 135 °C, t 1/2(135 °C) = t 1/2 o/5, where t 1/2 o is the time required to obtain 50% of the final extent of crystallization with pure PLLA. The block copolymer particles also enhanced the ductility of the blends by facilitating stress-induced cavitation and uniform crazing without impacting the modulus. Tensile toughness increased by 7–15 fold, scaling inversely with the degree of crystallinity. The deformation mechanism was investigated by small- and wide-angle X-ray scattering as a function of applied strain, revealing that the craze volume is dependent on crystallinity, while the crystal structure displayed minimal changes. Regardless of the extent of crystallinity, crazing was found to be the primary deformation mechanism, countering the ductile-to-brittle transition associated with the aging of PLLA. Adding 5 wt % PEO-PBO extends the strain at break from 4% for pure PLLA after 2 days to more than approximately 50% after 85 or more days of aging. These findings, along with the industrially relevant blend preparation method, reveal that PEO-PBO is a unique and potent additive that could expand the applications served by PLLA, promoting a more sustainable future.</description><identifier>ISSN: 0024-9297</identifier><identifier>EISSN: 1520-5835</identifier><identifier>DOI: 10.1021/acs.macromol.1c01702</identifier><language>eng</language><publisher>American Chemical Society</publisher><ispartof>Macromolecules, 2021-12, Vol.54 (23), p.11154-11169</ispartof><rights>2021 American Chemical Society</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-a292t-e0be9dbbefead2bda1fb2962a79a27c04ae48684e5f60bf945a38387040c8ad93</citedby><cites>FETCH-LOGICAL-a292t-e0be9dbbefead2bda1fb2962a79a27c04ae48684e5f60bf945a38387040c8ad93</cites><orcidid>0000-0003-3977-1278 ; 0000-0002-0393-2941</orcidid></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,780,784,27924,27925</link.rule.ids></links><search><creatorcontrib>McCutcheon, Charles J</creatorcontrib><creatorcontrib>Zhao, Boran</creatorcontrib><creatorcontrib>Ellison, Christopher J</creatorcontrib><creatorcontrib>Bates, Frank S</creatorcontrib><title>Crazing and Toughness in Diblock Copolymer-Modified Semicrystalline Poly(l‑lactide)</title><title>Macromolecules</title><addtitle>Macromolecules</addtitle><description>Sustainable semicrystalline poly­(l-lactide) (PLLA) was melt mixed with 5 wt % poly­(ethylene oxide)-b-poly­(butylene oxide) (PEO-PBO) diblock copolymer, resulting in blends that display an exceptional combination of properties. The blends were annealed at various temperatures, leading to different degrees of crystallinity. The addition of 5 wt % PEO-PBO produced finely dispersed liquid particles that caused a significant reduction in the time for crystallization after quenching from the melt, where T m = 166 °C. At 95 °C, the halftime for crystallization was t 1/2(95 °C) = t 1/2 o/7, while at 135 °C, t 1/2(135 °C) = t 1/2 o/5, where t 1/2 o is the time required to obtain 50% of the final extent of crystallization with pure PLLA. The block copolymer particles also enhanced the ductility of the blends by facilitating stress-induced cavitation and uniform crazing without impacting the modulus. Tensile toughness increased by 7–15 fold, scaling inversely with the degree of crystallinity. The deformation mechanism was investigated by small- and wide-angle X-ray scattering as a function of applied strain, revealing that the craze volume is dependent on crystallinity, while the crystal structure displayed minimal changes. Regardless of the extent of crystallinity, crazing was found to be the primary deformation mechanism, countering the ductile-to-brittle transition associated with the aging of PLLA. Adding 5 wt % PEO-PBO extends the strain at break from 4% for pure PLLA after 2 days to more than approximately 50% after 85 or more days of aging. These findings, along with the industrially relevant blend preparation method, reveal that PEO-PBO is a unique and potent additive that could expand the applications served by PLLA, promoting a more sustainable future.</description><issn>0024-9297</issn><issn>1520-5835</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2021</creationdate><recordtype>article</recordtype><recordid>eNp9kLFOwzAQhi0EEqXwBgweYUg5O04TjyhQQCoCiXaOLrZTXJy4stuhTLwCr8iTkKplZbrh7jv9_0fIJYMRA85uUMVRiyr41rsRU8By4EdkwDIOSVak2TEZAHCRSC7zU3IW4xKAsUykAzIvA37abkGx03TmN4v3zsRIbUfvbO28-qClX3m3bU1Inr22jTWavpnWqrCNa3TOdoa-9gdX7ufr26FaW22uz8lJgy6ai8MckvnkflY-JtOXh6fydpogl3ydGKiN1HVtGoOa1xpZU3M55phL5LkCgUYU40KYrBlD3UiRYVqkRQ4CVIFapkMi9n_77jEG01SrYFsM24pBtVNT9WqqPzXVQU2PwR7bbZd-E7o-5P_IL1Smbj4</recordid><startdate>20211214</startdate><enddate>20211214</enddate><creator>McCutcheon, Charles J</creator><creator>Zhao, Boran</creator><creator>Ellison, Christopher J</creator><creator>Bates, Frank S</creator><general>American Chemical Society</general><scope>AAYXX</scope><scope>CITATION</scope><orcidid>https://orcid.org/0000-0003-3977-1278</orcidid><orcidid>https://orcid.org/0000-0002-0393-2941</orcidid></search><sort><creationdate>20211214</creationdate><title>Crazing and Toughness in Diblock Copolymer-Modified Semicrystalline Poly(l‑lactide)</title><author>McCutcheon, Charles J ; Zhao, Boran ; Ellison, Christopher J ; Bates, Frank S</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-a292t-e0be9dbbefead2bda1fb2962a79a27c04ae48684e5f60bf945a38387040c8ad93</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2021</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>McCutcheon, Charles J</creatorcontrib><creatorcontrib>Zhao, Boran</creatorcontrib><creatorcontrib>Ellison, Christopher J</creatorcontrib><creatorcontrib>Bates, Frank S</creatorcontrib><collection>CrossRef</collection><jtitle>Macromolecules</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>McCutcheon, Charles J</au><au>Zhao, Boran</au><au>Ellison, Christopher J</au><au>Bates, Frank S</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Crazing and Toughness in Diblock Copolymer-Modified Semicrystalline Poly(l‑lactide)</atitle><jtitle>Macromolecules</jtitle><addtitle>Macromolecules</addtitle><date>2021-12-14</date><risdate>2021</risdate><volume>54</volume><issue>23</issue><spage>11154</spage><epage>11169</epage><pages>11154-11169</pages><issn>0024-9297</issn><eissn>1520-5835</eissn><abstract>Sustainable semicrystalline poly­(l-lactide) (PLLA) was melt mixed with 5 wt % poly­(ethylene oxide)-b-poly­(butylene oxide) (PEO-PBO) diblock copolymer, resulting in blends that display an exceptional combination of properties. The blends were annealed at various temperatures, leading to different degrees of crystallinity. The addition of 5 wt % PEO-PBO produced finely dispersed liquid particles that caused a significant reduction in the time for crystallization after quenching from the melt, where T m = 166 °C. At 95 °C, the halftime for crystallization was t 1/2(95 °C) = t 1/2 o/7, while at 135 °C, t 1/2(135 °C) = t 1/2 o/5, where t 1/2 o is the time required to obtain 50% of the final extent of crystallization with pure PLLA. The block copolymer particles also enhanced the ductility of the blends by facilitating stress-induced cavitation and uniform crazing without impacting the modulus. Tensile toughness increased by 7–15 fold, scaling inversely with the degree of crystallinity. The deformation mechanism was investigated by small- and wide-angle X-ray scattering as a function of applied strain, revealing that the craze volume is dependent on crystallinity, while the crystal structure displayed minimal changes. Regardless of the extent of crystallinity, crazing was found to be the primary deformation mechanism, countering the ductile-to-brittle transition associated with the aging of PLLA. Adding 5 wt % PEO-PBO extends the strain at break from 4% for pure PLLA after 2 days to more than approximately 50% after 85 or more days of aging. These findings, along with the industrially relevant blend preparation method, reveal that PEO-PBO is a unique and potent additive that could expand the applications served by PLLA, promoting a more sustainable future.</abstract><pub>American Chemical Society</pub><doi>10.1021/acs.macromol.1c01702</doi><tpages>16</tpages><orcidid>https://orcid.org/0000-0003-3977-1278</orcidid><orcidid>https://orcid.org/0000-0002-0393-2941</orcidid></addata></record>
fulltext fulltext
identifier ISSN: 0024-9297
ispartof Macromolecules, 2021-12, Vol.54 (23), p.11154-11169
issn 0024-9297
1520-5835
language eng
recordid cdi_crossref_primary_10_1021_acs_macromol_1c01702
source American Chemical Society:Jisc Collections:American Chemical Society Read & Publish Agreement 2022-2024 (Reading list)
title Crazing and Toughness in Diblock Copolymer-Modified Semicrystalline Poly(l‑lactide)
url http://sfxeu10.hosted.exlibrisgroup.com/loughborough?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-02T20%3A57%3A25IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-acs_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Crazing%20and%20Toughness%20in%20Diblock%20Copolymer-Modified%20Semicrystalline%20Poly(l%E2%80%91lactide)&rft.jtitle=Macromolecules&rft.au=McCutcheon,%20Charles%20J&rft.date=2021-12-14&rft.volume=54&rft.issue=23&rft.spage=11154&rft.epage=11169&rft.pages=11154-11169&rft.issn=0024-9297&rft.eissn=1520-5835&rft_id=info:doi/10.1021/acs.macromol.1c01702&rft_dat=%3Cacs_cross%3Eb003507568%3C/acs_cross%3E%3Cgrp_id%3Ecdi_FETCH-LOGICAL-a292t-e0be9dbbefead2bda1fb2962a79a27c04ae48684e5f60bf945a38387040c8ad93%3C/grp_id%3E%3Coa%3E%3C/oa%3E%3Curl%3E%3C/url%3E&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true