Loading…
Nanostructured Polyurethane/POSS Hybrid Aqueous Dispersions Prepared by Homogeneous Solution Polymerization
Aqueous polyurethane dispersions were prepared with 4−10 wt % of functionalized polyhedral oligomeric silsesquioxanes (POSS) via homogeneous solution polymerization in acetone followed by solvent exchange with water. The use of acetone as the initial polymerization solvent allowed for the facile inc...
Saved in:
Published in: | Macromolecules 2006-10, Vol.39 (20), p.7037-7043 |
---|---|
Main Authors: | , , , |
Format: | Article |
Language: | English |
Subjects: | |
Citations: | Items that this one cites Items that cite this one |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
cited_by | cdi_FETCH-LOGICAL-a355t-fe47dc67b3d7a05e99d616151114f64d8de997ce45501d96799314e6081d29e43 |
---|---|
cites | cdi_FETCH-LOGICAL-a355t-fe47dc67b3d7a05e99d616151114f64d8de997ce45501d96799314e6081d29e43 |
container_end_page | 7043 |
container_issue | 20 |
container_start_page | 7037 |
container_title | Macromolecules |
container_volume | 39 |
creator | Nanda, Ajaya K Wicks, Douglas A Madbouly, Samy A Otaigbe, Joshua U |
description | Aqueous polyurethane dispersions were prepared with 4−10 wt % of functionalized polyhedral oligomeric silsesquioxanes (POSS) via homogeneous solution polymerization in acetone followed by solvent exchange with water. The use of acetone as the initial polymerization solvent allowed for the facile incorporation of both diamino and dihydroxy functional POSS monomers in a homogeneous reaction environment. After addition of water and removal of the acetone, stable dispersions with unimodal particle sizes were obtained. The incorporation of the POSS monomers did not have a significant effect on the dispersion's properties; however, the physical properties of the isolated polymers did display significant changes, with notable increases in storage modulus, T g, complex viscosity, and surface hydrophobicity. These changes were attributed to the incorporation of the POSS residues into the polyurethane hard segment domains found. Though no sign of any gross phase heterogeneity due to the inclusion of POSS moieties was detected by either thermal characterization or wide-angle X-ray diffraction (WAXD), a significant change was observed by atomic force microscopy (AFM) when the samples were recast from organic solvent. |
doi_str_mv | 10.1021/ma060809h |
format | article |
fullrecord | <record><control><sourceid>acs_cross</sourceid><recordid>TN_cdi_crossref_primary_10_1021_ma060809h</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>c533626234</sourcerecordid><originalsourceid>FETCH-LOGICAL-a355t-fe47dc67b3d7a05e99d616151114f64d8de997ce45501d96799314e6081d29e43</originalsourceid><addsrcrecordid>eNptkDtPwzAUhS0EEqUw8A-yMDCE-ia2E49VeRSpopUKc-TaNzQliYOdDOHXkxZEF6b70HeOdA4h10DvgEYwqRQVNKVye0JGwCMa8jTmp2REacRCGcnknFx4v6MUgLN4RD5eVG196zrddg5NsLJlPyztVtU4WS3X62Deb1xhgulnh7bzwX3hG3S-sLUPVg4btVdt-mBuK_uO9YFZ27JrB-LgVqErvtT-vCRnuSo9Xv3OMXl7fHidzcPF8ul5Nl2EKua8DXNkidEi2cQmUZSjlEaAAA4ALBfMpGZ4JRoZ5xSMFImUMTAcYoOJJLJ4TG5_fLWz3jvMs8YVlXJ9BjTbt5T9tTSwNz9so7xWZe5UrQt_FKTAU56KI6e0z3a2c_WQ4B-_b7ZEdNQ</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Nanostructured Polyurethane/POSS Hybrid Aqueous Dispersions Prepared by Homogeneous Solution Polymerization</title><source>American Chemical Society:Jisc Collections:American Chemical Society Read & Publish Agreement 2022-2024 (Reading list)</source><creator>Nanda, Ajaya K ; Wicks, Douglas A ; Madbouly, Samy A ; Otaigbe, Joshua U</creator><creatorcontrib>Nanda, Ajaya K ; Wicks, Douglas A ; Madbouly, Samy A ; Otaigbe, Joshua U</creatorcontrib><description>Aqueous polyurethane dispersions were prepared with 4−10 wt % of functionalized polyhedral oligomeric silsesquioxanes (POSS) via homogeneous solution polymerization in acetone followed by solvent exchange with water. The use of acetone as the initial polymerization solvent allowed for the facile incorporation of both diamino and dihydroxy functional POSS monomers in a homogeneous reaction environment. After addition of water and removal of the acetone, stable dispersions with unimodal particle sizes were obtained. The incorporation of the POSS monomers did not have a significant effect on the dispersion's properties; however, the physical properties of the isolated polymers did display significant changes, with notable increases in storage modulus, T g, complex viscosity, and surface hydrophobicity. These changes were attributed to the incorporation of the POSS residues into the polyurethane hard segment domains found. Though no sign of any gross phase heterogeneity due to the inclusion of POSS moieties was detected by either thermal characterization or wide-angle X-ray diffraction (WAXD), a significant change was observed by atomic force microscopy (AFM) when the samples were recast from organic solvent.</description><identifier>ISSN: 0024-9297</identifier><identifier>EISSN: 1520-5835</identifier><identifier>DOI: 10.1021/ma060809h</identifier><identifier>CODEN: MAMOBX</identifier><language>eng</language><publisher>Washington, DC: American Chemical Society</publisher><subject>Applied sciences ; Exact sciences and technology ; Inorganic and organomineral polymers ; Physicochemistry of polymers ; Preparation</subject><ispartof>Macromolecules, 2006-10, Vol.39 (20), p.7037-7043</ispartof><rights>Copyright © 2006 American Chemical Society</rights><rights>2006 INIST-CNRS</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-a355t-fe47dc67b3d7a05e99d616151114f64d8de997ce45501d96799314e6081d29e43</citedby><cites>FETCH-LOGICAL-a355t-fe47dc67b3d7a05e99d616151114f64d8de997ce45501d96799314e6081d29e43</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,776,780,27901,27902</link.rule.ids><backlink>$$Uhttp://pascal-francis.inist.fr/vibad/index.php?action=getRecordDetail&idt=18158586$$DView record in Pascal Francis$$Hfree_for_read</backlink></links><search><creatorcontrib>Nanda, Ajaya K</creatorcontrib><creatorcontrib>Wicks, Douglas A</creatorcontrib><creatorcontrib>Madbouly, Samy A</creatorcontrib><creatorcontrib>Otaigbe, Joshua U</creatorcontrib><title>Nanostructured Polyurethane/POSS Hybrid Aqueous Dispersions Prepared by Homogeneous Solution Polymerization</title><title>Macromolecules</title><addtitle>Macromolecules</addtitle><description>Aqueous polyurethane dispersions were prepared with 4−10 wt % of functionalized polyhedral oligomeric silsesquioxanes (POSS) via homogeneous solution polymerization in acetone followed by solvent exchange with water. The use of acetone as the initial polymerization solvent allowed for the facile incorporation of both diamino and dihydroxy functional POSS monomers in a homogeneous reaction environment. After addition of water and removal of the acetone, stable dispersions with unimodal particle sizes were obtained. The incorporation of the POSS monomers did not have a significant effect on the dispersion's properties; however, the physical properties of the isolated polymers did display significant changes, with notable increases in storage modulus, T g, complex viscosity, and surface hydrophobicity. These changes were attributed to the incorporation of the POSS residues into the polyurethane hard segment domains found. Though no sign of any gross phase heterogeneity due to the inclusion of POSS moieties was detected by either thermal characterization or wide-angle X-ray diffraction (WAXD), a significant change was observed by atomic force microscopy (AFM) when the samples were recast from organic solvent.</description><subject>Applied sciences</subject><subject>Exact sciences and technology</subject><subject>Inorganic and organomineral polymers</subject><subject>Physicochemistry of polymers</subject><subject>Preparation</subject><issn>0024-9297</issn><issn>1520-5835</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2006</creationdate><recordtype>article</recordtype><recordid>eNptkDtPwzAUhS0EEqUw8A-yMDCE-ia2E49VeRSpopUKc-TaNzQliYOdDOHXkxZEF6b70HeOdA4h10DvgEYwqRQVNKVye0JGwCMa8jTmp2REacRCGcnknFx4v6MUgLN4RD5eVG196zrddg5NsLJlPyztVtU4WS3X62Deb1xhgulnh7bzwX3hG3S-sLUPVg4btVdt-mBuK_uO9YFZ27JrB-LgVqErvtT-vCRnuSo9Xv3OMXl7fHidzcPF8ul5Nl2EKua8DXNkidEi2cQmUZSjlEaAAA4ALBfMpGZ4JRoZ5xSMFImUMTAcYoOJJLJ4TG5_fLWz3jvMs8YVlXJ9BjTbt5T9tTSwNz9so7xWZe5UrQt_FKTAU56KI6e0z3a2c_WQ4B-_b7ZEdNQ</recordid><startdate>20061003</startdate><enddate>20061003</enddate><creator>Nanda, Ajaya K</creator><creator>Wicks, Douglas A</creator><creator>Madbouly, Samy A</creator><creator>Otaigbe, Joshua U</creator><general>American Chemical Society</general><scope>IQODW</scope><scope>AAYXX</scope><scope>CITATION</scope></search><sort><creationdate>20061003</creationdate><title>Nanostructured Polyurethane/POSS Hybrid Aqueous Dispersions Prepared by Homogeneous Solution Polymerization</title><author>Nanda, Ajaya K ; Wicks, Douglas A ; Madbouly, Samy A ; Otaigbe, Joshua U</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-a355t-fe47dc67b3d7a05e99d616151114f64d8de997ce45501d96799314e6081d29e43</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2006</creationdate><topic>Applied sciences</topic><topic>Exact sciences and technology</topic><topic>Inorganic and organomineral polymers</topic><topic>Physicochemistry of polymers</topic><topic>Preparation</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Nanda, Ajaya K</creatorcontrib><creatorcontrib>Wicks, Douglas A</creatorcontrib><creatorcontrib>Madbouly, Samy A</creatorcontrib><creatorcontrib>Otaigbe, Joshua U</creatorcontrib><collection>Pascal-Francis</collection><collection>CrossRef</collection><jtitle>Macromolecules</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Nanda, Ajaya K</au><au>Wicks, Douglas A</au><au>Madbouly, Samy A</au><au>Otaigbe, Joshua U</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Nanostructured Polyurethane/POSS Hybrid Aqueous Dispersions Prepared by Homogeneous Solution Polymerization</atitle><jtitle>Macromolecules</jtitle><addtitle>Macromolecules</addtitle><date>2006-10-03</date><risdate>2006</risdate><volume>39</volume><issue>20</issue><spage>7037</spage><epage>7043</epage><pages>7037-7043</pages><issn>0024-9297</issn><eissn>1520-5835</eissn><coden>MAMOBX</coden><abstract>Aqueous polyurethane dispersions were prepared with 4−10 wt % of functionalized polyhedral oligomeric silsesquioxanes (POSS) via homogeneous solution polymerization in acetone followed by solvent exchange with water. The use of acetone as the initial polymerization solvent allowed for the facile incorporation of both diamino and dihydroxy functional POSS monomers in a homogeneous reaction environment. After addition of water and removal of the acetone, stable dispersions with unimodal particle sizes were obtained. The incorporation of the POSS monomers did not have a significant effect on the dispersion's properties; however, the physical properties of the isolated polymers did display significant changes, with notable increases in storage modulus, T g, complex viscosity, and surface hydrophobicity. These changes were attributed to the incorporation of the POSS residues into the polyurethane hard segment domains found. Though no sign of any gross phase heterogeneity due to the inclusion of POSS moieties was detected by either thermal characterization or wide-angle X-ray diffraction (WAXD), a significant change was observed by atomic force microscopy (AFM) when the samples were recast from organic solvent.</abstract><cop>Washington, DC</cop><pub>American Chemical Society</pub><doi>10.1021/ma060809h</doi><tpages>7</tpages></addata></record> |
fulltext | fulltext |
identifier | ISSN: 0024-9297 |
ispartof | Macromolecules, 2006-10, Vol.39 (20), p.7037-7043 |
issn | 0024-9297 1520-5835 |
language | eng |
recordid | cdi_crossref_primary_10_1021_ma060809h |
source | American Chemical Society:Jisc Collections:American Chemical Society Read & Publish Agreement 2022-2024 (Reading list) |
subjects | Applied sciences Exact sciences and technology Inorganic and organomineral polymers Physicochemistry of polymers Preparation |
title | Nanostructured Polyurethane/POSS Hybrid Aqueous Dispersions Prepared by Homogeneous Solution Polymerization |
url | http://sfxeu10.hosted.exlibrisgroup.com/loughborough?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-01T12%3A10%3A35IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-acs_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Nanostructured%20Polyurethane/POSS%20Hybrid%20Aqueous%20Dispersions%20Prepared%20by%20Homogeneous%20Solution%20Polymerization&rft.jtitle=Macromolecules&rft.au=Nanda,%20Ajaya%20K&rft.date=2006-10-03&rft.volume=39&rft.issue=20&rft.spage=7037&rft.epage=7043&rft.pages=7037-7043&rft.issn=0024-9297&rft.eissn=1520-5835&rft.coden=MAMOBX&rft_id=info:doi/10.1021/ma060809h&rft_dat=%3Cacs_cross%3Ec533626234%3C/acs_cross%3E%3Cgrp_id%3Ecdi_FETCH-LOGICAL-a355t-fe47dc67b3d7a05e99d616151114f64d8de997ce45501d96799314e6081d29e43%3C/grp_id%3E%3Coa%3E%3C/oa%3E%3Curl%3E%3C/url%3E&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |