Tracer diffusion of 110Ag in YBa2Cu3O7-δ
Tracer diffusion of 110Ag in YBa2Cu3O7−δ has been measured in the temperature range 800–950 °C using serial sectioning. The polycrystalline samples were made either from a powder containing about 0.2% Zr prepared by a conventional technique, or from a purer powder that had been calcined in low-press...
Saved in:
Published in: | Journal of applied physics 1990-09, Vol.68 (5), p.2523-2525 |
---|---|
Main Authors: | , , |
Format: | Article |
Language: | English |
Subjects: | |
Citations: | Items that this one cites Items that cite this one |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | Tracer diffusion of 110Ag in YBa2Cu3O7−δ has been measured in the temperature range 800–950 °C using serial sectioning. The polycrystalline samples were made either from a powder containing about 0.2% Zr prepared by a conventional technique, or from a purer powder that had been calcined in low-pressure oxygen. Concentration profiles indicate both a volume and a fast diffusivity path contribution to diffusion. The activation energies were 227±3 and 249±17 kJ/mole for samples made from powder calcined in low-pressure oxygen and conventional powder, respectively. Diffusion was slower in the samples made from the purer powder. |
---|---|
ISSN: | 0021-8979 1089-7550 |
DOI: | 10.1063/1.346472 |