Loading…
Relations of slow relaxation of ferromagnets to saturating and recoiling fields
Systematic experiments on the Nd–Fe–B, Sm–Co, and Sr–Ferrite samples were performed to study the measuring-process dependent magnetic slow relaxation (magnetic viscosity). The relaxation coefficient (S) is proportional to the magnetic susceptibility (χ) for the Sr–Ferrite sample as the saturating fi...
Saved in:
Published in: | Journal of applied physics 1999-04, Vol.85 (8), p.4536-4538 |
---|---|
Main Author: | |
Format: | Article |
Language: | English |
Citations: | Items that this one cites |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
cited_by | |
---|---|
cites | cdi_FETCH-LOGICAL-c186t-1324dea50849f256325a717ac87c58608408fde5a7d54259bffbba65b527489e3 |
container_end_page | 4538 |
container_issue | 8 |
container_start_page | 4536 |
container_title | Journal of applied physics |
container_volume | 85 |
creator | Hsu, Shau-Wei |
description | Systematic experiments on the Nd–Fe–B, Sm–Co, and Sr–Ferrite samples were performed to study the measuring-process dependent magnetic slow relaxation (magnetic viscosity). The relaxation coefficient (S) is proportional to the magnetic susceptibility (χ) for the Sr–Ferrite sample as the saturating field (Hs) and demagnetization field (Hd) are relatively large. The S–χ data for the Sm–Co sample are confined between two lines, which are related to the magnitudes of Hs and Hd. S is proportional to a specific magnetization difference (ΔM1) for the measurements along recoil curves. The proportional constants of the Nd–Fe–B sample are 0.163 and 0.171 for the applied field parallel and perpendicular to the c axis, respectively. |
doi_str_mv | 10.1063/1.370400 |
format | article |
fullrecord | <record><control><sourceid>crossref</sourceid><recordid>TN_cdi_crossref_primary_10_1063_1_370400</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>10_1063_1_370400</sourcerecordid><originalsourceid>FETCH-LOGICAL-c186t-1324dea50849f256325a717ac87c58608408fde5a7d54259bffbba65b527489e3</originalsourceid><addsrcrecordid>eNot0E1LxDAQBuAgCtZV8Cfk6CXrTD6a5CiLX7CwIHouaZMslW4jSUX997aup2Ged5jDS8g1whqhFre4FhokwAmpEIxlWik4JRUAR2astufkopR3AEQjbEV2L2FwU5_GQlOkZUhfNM_y_WcLxZBzOrj9GKZCp0SLmz7znI576kY_H3epH5Yt9mHw5ZKcRTeUcPU_V-Tt4f5188S2u8fnzd2WdWjqiaHg0genwEgbuaoFV06jdp3RnTL1zGCiDzN6JbmybYxt62rVKq6lsUGsyM3xb5dTKTnE5iP3B5d_GoRmKaLB5liE-AUh-VAy</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Relations of slow relaxation of ferromagnets to saturating and recoiling fields</title><source>American Institute of Physics:Jisc Collections:Transitional Journals Agreement 2021-23 (Reading list)</source><creator>Hsu, Shau-Wei</creator><creatorcontrib>Hsu, Shau-Wei</creatorcontrib><description>Systematic experiments on the Nd–Fe–B, Sm–Co, and Sr–Ferrite samples were performed to study the measuring-process dependent magnetic slow relaxation (magnetic viscosity). The relaxation coefficient (S) is proportional to the magnetic susceptibility (χ) for the Sr–Ferrite sample as the saturating field (Hs) and demagnetization field (Hd) are relatively large. The S–χ data for the Sm–Co sample are confined between two lines, which are related to the magnitudes of Hs and Hd. S is proportional to a specific magnetization difference (ΔM1) for the measurements along recoil curves. The proportional constants of the Nd–Fe–B sample are 0.163 and 0.171 for the applied field parallel and perpendicular to the c axis, respectively.</description><identifier>ISSN: 0021-8979</identifier><identifier>EISSN: 1089-7550</identifier><identifier>DOI: 10.1063/1.370400</identifier><language>eng</language><ispartof>Journal of applied physics, 1999-04, Vol.85 (8), p.4536-4538</ispartof><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><cites>FETCH-LOGICAL-c186t-1324dea50849f256325a717ac87c58608408fde5a7d54259bffbba65b527489e3</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,780,784,27924,27925</link.rule.ids></links><search><creatorcontrib>Hsu, Shau-Wei</creatorcontrib><title>Relations of slow relaxation of ferromagnets to saturating and recoiling fields</title><title>Journal of applied physics</title><description>Systematic experiments on the Nd–Fe–B, Sm–Co, and Sr–Ferrite samples were performed to study the measuring-process dependent magnetic slow relaxation (magnetic viscosity). The relaxation coefficient (S) is proportional to the magnetic susceptibility (χ) for the Sr–Ferrite sample as the saturating field (Hs) and demagnetization field (Hd) are relatively large. The S–χ data for the Sm–Co sample are confined between two lines, which are related to the magnitudes of Hs and Hd. S is proportional to a specific magnetization difference (ΔM1) for the measurements along recoil curves. The proportional constants of the Nd–Fe–B sample are 0.163 and 0.171 for the applied field parallel and perpendicular to the c axis, respectively.</description><issn>0021-8979</issn><issn>1089-7550</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>1999</creationdate><recordtype>article</recordtype><recordid>eNot0E1LxDAQBuAgCtZV8Cfk6CXrTD6a5CiLX7CwIHouaZMslW4jSUX997aup2Ged5jDS8g1whqhFre4FhokwAmpEIxlWik4JRUAR2astufkopR3AEQjbEV2L2FwU5_GQlOkZUhfNM_y_WcLxZBzOrj9GKZCp0SLmz7znI576kY_H3epH5Yt9mHw5ZKcRTeUcPU_V-Tt4f5188S2u8fnzd2WdWjqiaHg0genwEgbuaoFV06jdp3RnTL1zGCiDzN6JbmybYxt62rVKq6lsUGsyM3xb5dTKTnE5iP3B5d_GoRmKaLB5liE-AUh-VAy</recordid><startdate>19990415</startdate><enddate>19990415</enddate><creator>Hsu, Shau-Wei</creator><scope>AAYXX</scope><scope>CITATION</scope></search><sort><creationdate>19990415</creationdate><title>Relations of slow relaxation of ferromagnets to saturating and recoiling fields</title><author>Hsu, Shau-Wei</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c186t-1324dea50849f256325a717ac87c58608408fde5a7d54259bffbba65b527489e3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>1999</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Hsu, Shau-Wei</creatorcontrib><collection>CrossRef</collection><jtitle>Journal of applied physics</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Hsu, Shau-Wei</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Relations of slow relaxation of ferromagnets to saturating and recoiling fields</atitle><jtitle>Journal of applied physics</jtitle><date>1999-04-15</date><risdate>1999</risdate><volume>85</volume><issue>8</issue><spage>4536</spage><epage>4538</epage><pages>4536-4538</pages><issn>0021-8979</issn><eissn>1089-7550</eissn><abstract>Systematic experiments on the Nd–Fe–B, Sm–Co, and Sr–Ferrite samples were performed to study the measuring-process dependent magnetic slow relaxation (magnetic viscosity). The relaxation coefficient (S) is proportional to the magnetic susceptibility (χ) for the Sr–Ferrite sample as the saturating field (Hs) and demagnetization field (Hd) are relatively large. The S–χ data for the Sm–Co sample are confined between two lines, which are related to the magnitudes of Hs and Hd. S is proportional to a specific magnetization difference (ΔM1) for the measurements along recoil curves. The proportional constants of the Nd–Fe–B sample are 0.163 and 0.171 for the applied field parallel and perpendicular to the c axis, respectively.</abstract><doi>10.1063/1.370400</doi><tpages>3</tpages></addata></record> |
fulltext | fulltext |
identifier | ISSN: 0021-8979 |
ispartof | Journal of applied physics, 1999-04, Vol.85 (8), p.4536-4538 |
issn | 0021-8979 1089-7550 |
language | eng |
recordid | cdi_crossref_primary_10_1063_1_370400 |
source | American Institute of Physics:Jisc Collections:Transitional Journals Agreement 2021-23 (Reading list) |
title | Relations of slow relaxation of ferromagnets to saturating and recoiling fields |
url | http://sfxeu10.hosted.exlibrisgroup.com/loughborough?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-07T13%3A51%3A19IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-crossref&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Relations%20of%20slow%20relaxation%20of%20ferromagnets%20to%20saturating%20and%20recoiling%20fields&rft.jtitle=Journal%20of%20applied%20physics&rft.au=Hsu,%20Shau-Wei&rft.date=1999-04-15&rft.volume=85&rft.issue=8&rft.spage=4536&rft.epage=4538&rft.pages=4536-4538&rft.issn=0021-8979&rft.eissn=1089-7550&rft_id=info:doi/10.1063/1.370400&rft_dat=%3Ccrossref%3E10_1063_1_370400%3C/crossref%3E%3Cgrp_id%3Ecdi_FETCH-LOGICAL-c186t-1324dea50849f256325a717ac87c58608408fde5a7d54259bffbba65b527489e3%3C/grp_id%3E%3Coa%3E%3C/oa%3E%3Curl%3E%3C/url%3E&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |