Effect of soaking times on ferroelectric properties and strain behavior of PLZT ceramics

In this work, PLZT x/65/35 powders where x=4, 6, 8 and 10 mol% were prepared by mixed-oxide method and sintered at 1200 °C for 4, 8 and 12h. The electric field induced strain (S-E) and electric field induced polarization (P-E) were measured by using strain and polarization measurement system. It was...

Full description

Saved in:
Bibliographic Details
Published in:Journal of physics. Conference series 2021-01, Vol.1719 (1), p.12073
Main Authors: Funsueb, N, Limpichaipanit, A, Ngamjarurojana, A
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:In this work, PLZT x/65/35 powders where x=4, 6, 8 and 10 mol% were prepared by mixed-oxide method and sintered at 1200 °C for 4, 8 and 12h. The electric field induced strain (S-E) and electric field induced polarization (P-E) were measured by using strain and polarization measurement system. It was found that PLZT 6/65/35 had the optimized condition with the soaking time of 12h. The highest remnant polarization (18.24 μC/cm2), saturated polarization (24.73 μC/cm2), strain (0.4090%) and d*33 (204.50 pm/V) It can be concluded that the soaking times affected to ferroelectric properties and strain behavior.
ISSN:1742-6588
1742-6596
DOI:10.1088/1742-6596/1719/1/012073