Cr2O3 Thin Films on Ag(111) by XPS

Cr2O3 (0001) films are grown on Ag(111) by repeated cycles of 0.5 ML deposition of Cr followed by annealing in O2 at 240 °C for 5 min at 10-5 Torr. The spectra shown are for a 15 Å thick Cr2O3 film.

Saved in:
Bibliographic Details
Published in:Surface science spectra 2006-12, Vol.13 (1), p.94-99
Main Authors: Priyantha, W.A.A., Waddill, George D.
Format: Article
Language:English
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Cr2O3 (0001) films are grown on Ag(111) by repeated cycles of 0.5 ML deposition of Cr followed by annealing in O2 at 240 °C for 5 min at 10-5 Torr. The spectra shown are for a 15 Å thick Cr2O3 film.
ISSN:1055-5269
1520-8575
DOI:10.1116/11.20050901