The analysis of surface extended energy loss fine structure of zinc oxide

The SEELFS (Surface Extended Energy Loss Fine Structure) of zinc oxide was observed. We obtained a nearest-neighbor atomic spacing of 0.202±0.001 nm (l=2) by correcting the phase shift which was dependent on the final angular momentum of l. This value is about 0.007 nm longer than the one of bulk.

Saved in:
Bibliographic Details
Published in:Japanese Journal of Applied Physics 1988-07, Vol.27 (7), p.1347-1348
Main Authors: KONISHI, R, ARIOKA, M, KOBAYASHI, Y, SASAKURA, H
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:The SEELFS (Surface Extended Energy Loss Fine Structure) of zinc oxide was observed. We obtained a nearest-neighbor atomic spacing of 0.202±0.001 nm (l=2) by correcting the phase shift which was dependent on the final angular momentum of l. This value is about 0.007 nm longer than the one of bulk.
ISSN:0021-4922