Effect of Surface Biopolymeric Treatment on Sisal Fiber Properties and Fiber-Cement Bond

Sisal fiber, available in various semi-arid regions around the world, is the most studied natural fiber for the reinforcement of polymeric and cement-based composites. However, to improve the fiber–matrix interaction and to reduce the hydrophilicity of the fiber, it is necessary to establish surface...

Full description

Saved in:
Bibliographic Details
Published in:Journal of engineered fibers and fabrics 2017-06, Vol.12 (2)
Main Authors: Lima, Paulo R. L., Santos, Heni Mirna, Camilloto, Geany Peruch, Cruz, Renato Souza
Format: Article
Language:English
Citations: Items that this one cites
Items that cite this one
Online Access:Request full text
Tags: Add Tag
No Tags, Be the first to tag this record!
cited_by cdi_FETCH-LOGICAL-c331t-bc2fcbe95ab0cbc95794332c03e2d3b3aa1ac3d19985b8eb255ef8c7783b79cf3
cites cdi_FETCH-LOGICAL-c331t-bc2fcbe95ab0cbc95794332c03e2d3b3aa1ac3d19985b8eb255ef8c7783b79cf3
container_end_page
container_issue 2
container_start_page
container_title Journal of engineered fibers and fabrics
container_volume 12
creator Lima, Paulo R. L.
Santos, Heni Mirna
Camilloto, Geany Peruch
Cruz, Renato Souza
description Sisal fiber, available in various semi-arid regions around the world, is the most studied natural fiber for the reinforcement of polymeric and cement-based composites. However, to improve the fiber–matrix interaction and to reduce the hydrophilicity of the fiber, it is necessary to establish surface treatments that employ sustainable materials, unlike conventional surface treatments. In this work, sisal fibers were coated separately with cellulose acetate, hydrophobic starch, and cassava starch biopolymers in order to verify the possibility of reducing the water absorption capacity of the fiber by the use of a biodegradable resin. A combination of Fourier transform infrared spectroscopy, scanning electron microscopy, and water absorption and tensile tests was used to investigate the effects of the surface treatments on the sisal fiber properties. Pullout tests of sisal fibers with embedded lengths of 20 mm and 40 mm were performed to determine the influence of the treatments on the bond stress with cement mortar. Composites with 4 vol % short fiber were produced and tested for flexion. The study results indicated that all treatments reduced the mechanical properties of the fiber; however, the layer of the cellulose acetate biopolymer film formed on the fiber surface was effective in reducing the fiber hydrophilicity. Experimental tests on the composites revealed that the cellulose acetate treatment reduced the bond stress and, to a lesser degree, the flexural toughness of the composite, despite the increase in flexural strength.
doi_str_mv 10.1177/155892501701200207
format article
fullrecord <record><control><sourceid>sage_AFRWT</sourceid><recordid>TN_cdi_crossref_primary_10_1177_155892501701200207</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sage_id>10.1177_155892501701200207</sage_id><sourcerecordid>10.1177_155892501701200207</sourcerecordid><originalsourceid>FETCH-LOGICAL-c331t-bc2fcbe95ab0cbc95794332c03e2d3b3aa1ac3d19985b8eb255ef8c7783b79cf3</originalsourceid><addsrcrecordid>eNp9kE1Lw0AQhhdRsFb_gKf9A7H74bLZow2tFgoKreAt7E5mJSXJlt300H9vYjwIgqcZHt5nGF5C7jl74FzrBVcqN0IxrhkXjAmmL8hshNlIL3_t1-QmpQNjykjFZuRj5T1CT4Onu1P0FpAu63AMzbnFWAPdR7R9i92Q6OiuTrah69phpG8xHDH2NSZqu2qCWYHf0WXoqlty5W2T8O5nzsn7erUvXrLt6_OmeNpmICXvMwfCg0OjrGPgwChtHqUUwCSKSjppLbcgK25MrlyOTiiFPgetc-m0AS_nREx3IYaUIvryGOvWxnPJWTl2U_7tZpAWk5TsJ5aHcIrd8ON_xhdLwGTN</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Effect of Surface Biopolymeric Treatment on Sisal Fiber Properties and Fiber-Cement Bond</title><source>SAGE Open Access</source><creator>Lima, Paulo R. L. ; Santos, Heni Mirna ; Camilloto, Geany Peruch ; Cruz, Renato Souza</creator><creatorcontrib>Lima, Paulo R. L. ; Santos, Heni Mirna ; Camilloto, Geany Peruch ; Cruz, Renato Souza</creatorcontrib><description>Sisal fiber, available in various semi-arid regions around the world, is the most studied natural fiber for the reinforcement of polymeric and cement-based composites. However, to improve the fiber–matrix interaction and to reduce the hydrophilicity of the fiber, it is necessary to establish surface treatments that employ sustainable materials, unlike conventional surface treatments. In this work, sisal fibers were coated separately with cellulose acetate, hydrophobic starch, and cassava starch biopolymers in order to verify the possibility of reducing the water absorption capacity of the fiber by the use of a biodegradable resin. A combination of Fourier transform infrared spectroscopy, scanning electron microscopy, and water absorption and tensile tests was used to investigate the effects of the surface treatments on the sisal fiber properties. Pullout tests of sisal fibers with embedded lengths of 20 mm and 40 mm were performed to determine the influence of the treatments on the bond stress with cement mortar. Composites with 4 vol % short fiber were produced and tested for flexion. The study results indicated that all treatments reduced the mechanical properties of the fiber; however, the layer of the cellulose acetate biopolymer film formed on the fiber surface was effective in reducing the fiber hydrophilicity. Experimental tests on the composites revealed that the cellulose acetate treatment reduced the bond stress and, to a lesser degree, the flexural toughness of the composite, despite the increase in flexural strength.</description><identifier>ISSN: 1558-9250</identifier><identifier>EISSN: 1558-9250</identifier><identifier>DOI: 10.1177/155892501701200207</identifier><language>eng</language><publisher>London, England: SAGE Publications</publisher><ispartof>Journal of engineered fibers and fabrics, 2017-06, Vol.12 (2)</ispartof><rights>2017 SAGE Publications</rights><lds50>peer_reviewed</lds50><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c331t-bc2fcbe95ab0cbc95794332c03e2d3b3aa1ac3d19985b8eb255ef8c7783b79cf3</citedby><cites>FETCH-LOGICAL-c331t-bc2fcbe95ab0cbc95794332c03e2d3b3aa1ac3d19985b8eb255ef8c7783b79cf3</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktopdf>$$Uhttps://journals.sagepub.com/doi/pdf/10.1177/155892501701200207$$EPDF$$P50$$Gsage$$H</linktopdf><linktohtml>$$Uhttps://journals.sagepub.com/doi/10.1177/155892501701200207$$EHTML$$P50$$Gsage$$H</linktohtml><link.rule.ids>314,780,784,21965,27852,27923,27924,44944,45332</link.rule.ids><linktorsrc>$$Uhttps://journals.sagepub.com/doi/full/10.1177/155892501701200207?utm_source=summon&amp;utm_medium=discovery-provider$$EView_record_in_SAGE_Publications$$FView_record_in_$$GSAGE_Publications</linktorsrc></links><search><creatorcontrib>Lima, Paulo R. L.</creatorcontrib><creatorcontrib>Santos, Heni Mirna</creatorcontrib><creatorcontrib>Camilloto, Geany Peruch</creatorcontrib><creatorcontrib>Cruz, Renato Souza</creatorcontrib><title>Effect of Surface Biopolymeric Treatment on Sisal Fiber Properties and Fiber-Cement Bond</title><title>Journal of engineered fibers and fabrics</title><description>Sisal fiber, available in various semi-arid regions around the world, is the most studied natural fiber for the reinforcement of polymeric and cement-based composites. However, to improve the fiber–matrix interaction and to reduce the hydrophilicity of the fiber, it is necessary to establish surface treatments that employ sustainable materials, unlike conventional surface treatments. In this work, sisal fibers were coated separately with cellulose acetate, hydrophobic starch, and cassava starch biopolymers in order to verify the possibility of reducing the water absorption capacity of the fiber by the use of a biodegradable resin. A combination of Fourier transform infrared spectroscopy, scanning electron microscopy, and water absorption and tensile tests was used to investigate the effects of the surface treatments on the sisal fiber properties. Pullout tests of sisal fibers with embedded lengths of 20 mm and 40 mm were performed to determine the influence of the treatments on the bond stress with cement mortar. Composites with 4 vol % short fiber were produced and tested for flexion. The study results indicated that all treatments reduced the mechanical properties of the fiber; however, the layer of the cellulose acetate biopolymer film formed on the fiber surface was effective in reducing the fiber hydrophilicity. Experimental tests on the composites revealed that the cellulose acetate treatment reduced the bond stress and, to a lesser degree, the flexural toughness of the composite, despite the increase in flexural strength.</description><issn>1558-9250</issn><issn>1558-9250</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2017</creationdate><recordtype>article</recordtype><recordid>eNp9kE1Lw0AQhhdRsFb_gKf9A7H74bLZow2tFgoKreAt7E5mJSXJlt300H9vYjwIgqcZHt5nGF5C7jl74FzrBVcqN0IxrhkXjAmmL8hshNlIL3_t1-QmpQNjykjFZuRj5T1CT4Onu1P0FpAu63AMzbnFWAPdR7R9i92Q6OiuTrah69phpG8xHDH2NSZqu2qCWYHf0WXoqlty5W2T8O5nzsn7erUvXrLt6_OmeNpmICXvMwfCg0OjrGPgwChtHqUUwCSKSjppLbcgK25MrlyOTiiFPgetc-m0AS_nREx3IYaUIvryGOvWxnPJWTl2U_7tZpAWk5TsJ5aHcIrd8ON_xhdLwGTN</recordid><startdate>20170601</startdate><enddate>20170601</enddate><creator>Lima, Paulo R. L.</creator><creator>Santos, Heni Mirna</creator><creator>Camilloto, Geany Peruch</creator><creator>Cruz, Renato Souza</creator><general>SAGE Publications</general><scope>AAYXX</scope><scope>CITATION</scope></search><sort><creationdate>20170601</creationdate><title>Effect of Surface Biopolymeric Treatment on Sisal Fiber Properties and Fiber-Cement Bond</title><author>Lima, Paulo R. L. ; Santos, Heni Mirna ; Camilloto, Geany Peruch ; Cruz, Renato Souza</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c331t-bc2fcbe95ab0cbc95794332c03e2d3b3aa1ac3d19985b8eb255ef8c7783b79cf3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2017</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Lima, Paulo R. L.</creatorcontrib><creatorcontrib>Santos, Heni Mirna</creatorcontrib><creatorcontrib>Camilloto, Geany Peruch</creatorcontrib><creatorcontrib>Cruz, Renato Souza</creatorcontrib><collection>CrossRef</collection><jtitle>Journal of engineered fibers and fabrics</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Lima, Paulo R. L.</au><au>Santos, Heni Mirna</au><au>Camilloto, Geany Peruch</au><au>Cruz, Renato Souza</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Effect of Surface Biopolymeric Treatment on Sisal Fiber Properties and Fiber-Cement Bond</atitle><jtitle>Journal of engineered fibers and fabrics</jtitle><date>2017-06-01</date><risdate>2017</risdate><volume>12</volume><issue>2</issue><issn>1558-9250</issn><eissn>1558-9250</eissn><abstract>Sisal fiber, available in various semi-arid regions around the world, is the most studied natural fiber for the reinforcement of polymeric and cement-based composites. However, to improve the fiber–matrix interaction and to reduce the hydrophilicity of the fiber, it is necessary to establish surface treatments that employ sustainable materials, unlike conventional surface treatments. In this work, sisal fibers were coated separately with cellulose acetate, hydrophobic starch, and cassava starch biopolymers in order to verify the possibility of reducing the water absorption capacity of the fiber by the use of a biodegradable resin. A combination of Fourier transform infrared spectroscopy, scanning electron microscopy, and water absorption and tensile tests was used to investigate the effects of the surface treatments on the sisal fiber properties. Pullout tests of sisal fibers with embedded lengths of 20 mm and 40 mm were performed to determine the influence of the treatments on the bond stress with cement mortar. Composites with 4 vol % short fiber were produced and tested for flexion. The study results indicated that all treatments reduced the mechanical properties of the fiber; however, the layer of the cellulose acetate biopolymer film formed on the fiber surface was effective in reducing the fiber hydrophilicity. Experimental tests on the composites revealed that the cellulose acetate treatment reduced the bond stress and, to a lesser degree, the flexural toughness of the composite, despite the increase in flexural strength.</abstract><cop>London, England</cop><pub>SAGE Publications</pub><doi>10.1177/155892501701200207</doi><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier ISSN: 1558-9250
ispartof Journal of engineered fibers and fabrics, 2017-06, Vol.12 (2)
issn 1558-9250
1558-9250
language eng
recordid cdi_crossref_primary_10_1177_155892501701200207
source SAGE Open Access
title Effect of Surface Biopolymeric Treatment on Sisal Fiber Properties and Fiber-Cement Bond
url http://sfxeu10.hosted.exlibrisgroup.com/loughborough?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-08T15%3A25%3A28IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-sage_AFRWT&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Effect%20of%20Surface%20Biopolymeric%20Treatment%20on%20Sisal%20Fiber%20Properties%20and%20Fiber-Cement%20Bond&rft.jtitle=Journal%20of%20engineered%20fibers%20and%20fabrics&rft.au=Lima,%20Paulo%20R.%20L.&rft.date=2017-06-01&rft.volume=12&rft.issue=2&rft.issn=1558-9250&rft.eissn=1558-9250&rft_id=info:doi/10.1177/155892501701200207&rft_dat=%3Csage_AFRWT%3E10.1177_155892501701200207%3C/sage_AFRWT%3E%3Cgrp_id%3Ecdi_FETCH-LOGICAL-c331t-bc2fcbe95ab0cbc95794332c03e2d3b3aa1ac3d19985b8eb255ef8c7783b79cf3%3C/grp_id%3E%3Coa%3E%3C/oa%3E%3Curl%3E%3C/url%3E&rft_id=info:oai/&rft_id=info:pmid/&rft_sage_id=10.1177_155892501701200207&rfr_iscdi=true