We applied magnesiothermic reduction for porous silica glass, which was prepared from sodium borosilicate glass. The powdered porous silica glass was reduced to silicon and magnesium silicide at temperatures higher than 600 °C. The silicon was isolated by the hydrochloric acid treatment and the subs...

Full description

Saved in:
Bibliographic Details
Published in:Chemistry letters 2016-10, Vol.45 (10), p.1171-1173
Main Authors: Uehira, Kenta, Okada, Arifumi, Shiomi, Haruhisa, Wakasugi, Takashi, Kadono, Kohei
Format: Article
Language:English
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:We applied magnesiothermic reduction for porous silica glass, which was prepared from sodium borosilicate glass. The powdered porous silica glass was reduced to silicon and magnesium silicide at temperatures higher than 600 °C. The silicon was isolated by the hydrochloric acid treatment and the subsequent hydrofluoric acid treatment for the reduction products. The SEM observation revealed that the prepared silicon had a porous structure. The pore size distribution measured with a porosimeter was similar to that of the stating porous silica glass in the region less than several tens nanometers.