Microporous Structure of Alumina Prepared by a Salt Catalytic Sol-Gel Process

A microporous structure of alumina with a narrow distribution of the pore size (∼0.4 nm in diameter) was synthesized by a salt catalytic sol-gel process of dilute Al(OCH(CH3)2)3 and H2O solution without any template molecule. The specific surface area of alumina after the calcination at 300 °C was 9...

Full description

Saved in:
Bibliographic Details
Published in:Chemistry letters 2002, Vol.31 (1), p.110-111
Main Authors: Tanaka, Kazuhiko, Imai, Tomohito, Murakami, Yasushi, Matsumoto, Taki, Sugimoto, Wataru, Takasu, Yoshio
Format: Article
Language:English
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
cited_by cdi_FETCH-LOGICAL-c390t-6fd4332d50732f4594ab1fffd46d5abad67f5e038c5c9d52c868397508e40ca53
cites cdi_FETCH-LOGICAL-c390t-6fd4332d50732f4594ab1fffd46d5abad67f5e038c5c9d52c868397508e40ca53
container_end_page 111
container_issue 1
container_start_page 110
container_title Chemistry letters
container_volume 31
creator Tanaka, Kazuhiko
Imai, Tomohito
Murakami, Yasushi
Matsumoto, Taki
Sugimoto, Wataru
Takasu, Yoshio
description A microporous structure of alumina with a narrow distribution of the pore size (∼0.4 nm in diameter) was synthesized by a salt catalytic sol-gel process of dilute Al(OCH(CH3)2)3 and H2O solution without any template molecule. The specific surface area of alumina after the calcination at 300 °C was 960 m2g-1 while it was 170 m2g-1 even after the calcination at 900 °C.
doi_str_mv 10.1246/cl.2002.110
format article
fullrecord <record><control><sourceid>chemicalsocietyjapan_cross</sourceid><recordid>TN_cdi_crossref_primary_10_1246_cl_2002_110</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>10_1246_cl_2002_110</sourcerecordid><originalsourceid>FETCH-LOGICAL-c390t-6fd4332d50732f4594ab1fffd46d5abad67f5e038c5c9d52c868397508e40ca53</originalsourceid><addsrcrecordid>eNptkMFKAzEURYMoWKsrfyB7mfqSTDKZZSlahRaF6jqkmQSnpM2QZBbz96bYpasHl3Mfl4PQI4EFobV4Nn5BAeiCELhCM8JqWUFD-DWaAROiaoDSW3SX0gEAZMvoDG23vYlhCDGMCe9yHE0eo8XB4aUfj_1J489oBx1th_cT1ninfcYrnbWfcm_wLvhqbX2BgrEp3aMbp32yD5c7R9-vL1-rt2rzsX5fLTeVYS3kSriuZox2HBpGXc3bWu-JcyUVHdd73YnGcQtMGm7ajlMjhWRtw0HaGozmbI6e_v6W7SlF69QQ-6OOkyKgziaU8epsQhUThZYX-scee1OGBdPbPB30oE_qEMZ4Ktm_1V_J1GQo</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Microporous Structure of Alumina Prepared by a Salt Catalytic Sol-Gel Process</title><source>Oxford University Press:Jisc Collections:OUP Read and Publish 2024-2025 (2024 collection) (Reading list)</source><creator>Tanaka, Kazuhiko ; Imai, Tomohito ; Murakami, Yasushi ; Matsumoto, Taki ; Sugimoto, Wataru ; Takasu, Yoshio</creator><creatorcontrib>Tanaka, Kazuhiko ; Imai, Tomohito ; Murakami, Yasushi ; Matsumoto, Taki ; Sugimoto, Wataru ; Takasu, Yoshio</creatorcontrib><description>A microporous structure of alumina with a narrow distribution of the pore size (∼0.4 nm in diameter) was synthesized by a salt catalytic sol-gel process of dilute Al(OCH(CH3)2)3 and H2O solution without any template molecule. The specific surface area of alumina after the calcination at 300 °C was 960 m2g-1 while it was 170 m2g-1 even after the calcination at 900 °C.</description><identifier>ISSN: 0366-7022</identifier><identifier>EISSN: 1348-0715</identifier><identifier>DOI: 10.1246/cl.2002.110</identifier><language>eng</language><publisher>The Chemical Society of Japan</publisher><ispartof>Chemistry letters, 2002, Vol.31 (1), p.110-111</ispartof><rights>The Chemical Society of Japan</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c390t-6fd4332d50732f4594ab1fffd46d5abad67f5e038c5c9d52c868397508e40ca53</citedby><cites>FETCH-LOGICAL-c390t-6fd4332d50732f4594ab1fffd46d5abad67f5e038c5c9d52c868397508e40ca53</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,776,780,4009,27902,27903,27904</link.rule.ids></links><search><creatorcontrib>Tanaka, Kazuhiko</creatorcontrib><creatorcontrib>Imai, Tomohito</creatorcontrib><creatorcontrib>Murakami, Yasushi</creatorcontrib><creatorcontrib>Matsumoto, Taki</creatorcontrib><creatorcontrib>Sugimoto, Wataru</creatorcontrib><creatorcontrib>Takasu, Yoshio</creatorcontrib><title>Microporous Structure of Alumina Prepared by a Salt Catalytic Sol-Gel Process</title><title>Chemistry letters</title><addtitle>Chemistry Letters</addtitle><description>A microporous structure of alumina with a narrow distribution of the pore size (∼0.4 nm in diameter) was synthesized by a salt catalytic sol-gel process of dilute Al(OCH(CH3)2)3 and H2O solution without any template molecule. The specific surface area of alumina after the calcination at 300 °C was 960 m2g-1 while it was 170 m2g-1 even after the calcination at 900 °C.</description><issn>0366-7022</issn><issn>1348-0715</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2002</creationdate><recordtype>article</recordtype><recordid>eNptkMFKAzEURYMoWKsrfyB7mfqSTDKZZSlahRaF6jqkmQSnpM2QZBbz96bYpasHl3Mfl4PQI4EFobV4Nn5BAeiCELhCM8JqWUFD-DWaAROiaoDSW3SX0gEAZMvoDG23vYlhCDGMCe9yHE0eo8XB4aUfj_1J489oBx1th_cT1ninfcYrnbWfcm_wLvhqbX2BgrEp3aMbp32yD5c7R9-vL1-rt2rzsX5fLTeVYS3kSriuZox2HBpGXc3bWu-JcyUVHdd73YnGcQtMGm7ajlMjhWRtw0HaGozmbI6e_v6W7SlF69QQ-6OOkyKgziaU8epsQhUThZYX-scee1OGBdPbPB30oE_qEMZ4Ktm_1V_J1GQo</recordid><startdate>2002</startdate><enddate>2002</enddate><creator>Tanaka, Kazuhiko</creator><creator>Imai, Tomohito</creator><creator>Murakami, Yasushi</creator><creator>Matsumoto, Taki</creator><creator>Sugimoto, Wataru</creator><creator>Takasu, Yoshio</creator><general>The Chemical Society of Japan</general><scope>AAYXX</scope><scope>CITATION</scope></search><sort><creationdate>2002</creationdate><title>Microporous Structure of Alumina Prepared by a Salt Catalytic Sol-Gel Process</title><author>Tanaka, Kazuhiko ; Imai, Tomohito ; Murakami, Yasushi ; Matsumoto, Taki ; Sugimoto, Wataru ; Takasu, Yoshio</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c390t-6fd4332d50732f4594ab1fffd46d5abad67f5e038c5c9d52c868397508e40ca53</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2002</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Tanaka, Kazuhiko</creatorcontrib><creatorcontrib>Imai, Tomohito</creatorcontrib><creatorcontrib>Murakami, Yasushi</creatorcontrib><creatorcontrib>Matsumoto, Taki</creatorcontrib><creatorcontrib>Sugimoto, Wataru</creatorcontrib><creatorcontrib>Takasu, Yoshio</creatorcontrib><collection>CrossRef</collection><jtitle>Chemistry letters</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Tanaka, Kazuhiko</au><au>Imai, Tomohito</au><au>Murakami, Yasushi</au><au>Matsumoto, Taki</au><au>Sugimoto, Wataru</au><au>Takasu, Yoshio</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Microporous Structure of Alumina Prepared by a Salt Catalytic Sol-Gel Process</atitle><jtitle>Chemistry letters</jtitle><addtitle>Chemistry Letters</addtitle><date>2002</date><risdate>2002</risdate><volume>31</volume><issue>1</issue><spage>110</spage><epage>111</epage><pages>110-111</pages><issn>0366-7022</issn><eissn>1348-0715</eissn><abstract>A microporous structure of alumina with a narrow distribution of the pore size (∼0.4 nm in diameter) was synthesized by a salt catalytic sol-gel process of dilute Al(OCH(CH3)2)3 and H2O solution without any template molecule. The specific surface area of alumina after the calcination at 300 °C was 960 m2g-1 while it was 170 m2g-1 even after the calcination at 900 °C.</abstract><pub>The Chemical Society of Japan</pub><doi>10.1246/cl.2002.110</doi><tpages>2</tpages></addata></record>
fulltext fulltext
identifier ISSN: 0366-7022
ispartof Chemistry letters, 2002, Vol.31 (1), p.110-111
issn 0366-7022
1348-0715
language eng
recordid cdi_crossref_primary_10_1246_cl_2002_110
source Oxford University Press:Jisc Collections:OUP Read and Publish 2024-2025 (2024 collection) (Reading list)
title Microporous Structure of Alumina Prepared by a Salt Catalytic Sol-Gel Process
url http://sfxeu10.hosted.exlibrisgroup.com/loughborough?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-22T12%3A33%3A14IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-chemicalsocietyjapan_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Microporous%20Structure%20of%20Alumina%20Prepared%20by%20a%20Salt%20Catalytic%20Sol-Gel%20Process&rft.jtitle=Chemistry%20letters&rft.au=Tanaka,%20Kazuhiko&rft.date=2002&rft.volume=31&rft.issue=1&rft.spage=110&rft.epage=111&rft.pages=110-111&rft.issn=0366-7022&rft.eissn=1348-0715&rft_id=info:doi/10.1246/cl.2002.110&rft_dat=%3Cchemicalsocietyjapan_cross%3E10_1246_cl_2002_110%3C/chemicalsocietyjapan_cross%3E%3Cgrp_id%3Ecdi_FETCH-LOGICAL-c390t-6fd4332d50732f4594ab1fffd46d5abad67f5e038c5c9d52c868397508e40ca53%3C/grp_id%3E%3Coa%3E%3C/oa%3E%3Curl%3E%3C/url%3E&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true