Effect of Dentine Pretreatment with 38% Silver Diamine Fluoride and CPP-ACPF on Micro-Shear Bond Strength of Resin Modified Glass Ionomer Cement

The aim of the study is to evaluate the micro-shear bond strength and mode of failure of resin modified glass ionomer cement (RMGIC) placed on demineralized dentin pre-treated with 38% silver diamine fluoride (SDF) and casein phosphopeptide amorphous calcium phosphate (CPP-ACP). In order to mount th...

Full description

Saved in:
Bibliographic Details
Published in:Asian journal of chemistry 2023-06, Vol.35 (6), p.1445-1448
Main Authors: PhaniKumar, Mettapalli Sai, RojaRamya, Kakarla Sri, Vinay, C., Uloopi, K.S., Alla, Rama Krishna, Chaitanya, Penmatsa
Format: Article
Language:English
Citations: Items that this one cites
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
cited_by
cites cdi_FETCH-LOGICAL-c1579-cd26c1f657a447d1fd3e14fbdbb463ef1e72371eed89cde11088ce0946c9d0f23
container_end_page 1448
container_issue 6
container_start_page 1445
container_title Asian journal of chemistry
container_volume 35
creator PhaniKumar, Mettapalli Sai
RojaRamya, Kakarla Sri
Vinay, C.
Uloopi, K.S.
Alla, Rama Krishna
Chaitanya, Penmatsa
description The aim of the study is to evaluate the micro-shear bond strength and mode of failure of resin modified glass ionomer cement (RMGIC) placed on demineralized dentin pre-treated with 38% silver diamine fluoride (SDF) and casein phosphopeptide amorphous calcium phosphate (CPP-ACP). In order to mount the premolars in acrylic blocks, 30 caries-free human premolars were divided mesio-distally into two equal halves.. Then the enamel was removed to expose the dentin and immersed in demineralizing solution for 96 h, which were then randomly allocated into three groups: Group-1: pretreatment with 38% SDF + RMGIC; Group-2: pretreatment with CPP-ACPF + RMGIC; and Group-3: No pretreatment + RMGIC (control). After the pre-treatment, resin modified glass ionomer cement was placed over the dentin surface using cylindrical mold. Then the micro-shear bond strength was evaluated using universal testing machine and mode of fracture was analyzed with stereomicroscopy. The micro-shear bond strength was found to be higher for the control group (35.73 ± 4.15) followed by SDF (28.39 ± 1.64) and CPP-ACPF (23.00 ± 2.17) and this difference was found to be statistically significant (p = 0.001). On analyzing the mode of failure, the adhesive type of failure was most common in all the groups and the difference in the percentages of mode of failure between the groups was not significant (p = 0.337). Application of 38% SDF and CPP-ACPF on demineralized dentin samples has shown to reduce the micro-shear bond strength of resin modified glass ionomer cement. Adhesive failures were the most common type of failures in both pretreated and untreated groups.
doi_str_mv 10.14233/ajchem.2023.27589
format article
fullrecord <record><control><sourceid>crossref</sourceid><recordid>TN_cdi_crossref_primary_10_14233_ajchem_2023_27589</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>10_14233_ajchem_2023_27589</sourcerecordid><originalsourceid>FETCH-LOGICAL-c1579-cd26c1f657a447d1fd3e14fbdbb463ef1e72371eed89cde11088ce0946c9d0f23</originalsourceid><addsrcrecordid>eNotkMtOwzAQRS0EElXpD7DyhmWKH0mcLEv6oFIREQWJXeTaY-oqiZEdQPwFn4xbmM3MaK7OHV2ErimZ0pRxfisPag_dlBHGp0xkRXmGRqQUWZIy8Xp-mkkiiBCXaBLCgcTKacYEG6GfhTGgBuwMnkM_2B5w7WHwIIcu7vjLDnvMixu8te0neDy3sjuKlu2H81YDlr3GVV0ns6peYtfjB6u8S7Z7kB7fuXjcRlj_FinR4gmCjRKnrbGg8aqVIeC1610X0RUcHa_QhZFtgMl_H6OX5eK5uk82j6t1NdskimaiTJRmuaImz4RMU6Gp0RxoanZ6t0tzDoaCYFxQAF2USgOlpCgUkDLNVamJYXyM2B83vhuCB9O8e9tJ_91Q0pxibf5ibY6xNqdY-S8wGG0q</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Effect of Dentine Pretreatment with 38% Silver Diamine Fluoride and CPP-ACPF on Micro-Shear Bond Strength of Resin Modified Glass Ionomer Cement</title><source>Alma/SFX Local Collection</source><creator>PhaniKumar, Mettapalli Sai ; RojaRamya, Kakarla Sri ; Vinay, C. ; Uloopi, K.S. ; Alla, Rama Krishna ; Chaitanya, Penmatsa</creator><creatorcontrib>PhaniKumar, Mettapalli Sai ; RojaRamya, Kakarla Sri ; Vinay, C. ; Uloopi, K.S. ; Alla, Rama Krishna ; Chaitanya, Penmatsa</creatorcontrib><description>The aim of the study is to evaluate the micro-shear bond strength and mode of failure of resin modified glass ionomer cement (RMGIC) placed on demineralized dentin pre-treated with 38% silver diamine fluoride (SDF) and casein phosphopeptide amorphous calcium phosphate (CPP-ACP). In order to mount the premolars in acrylic blocks, 30 caries-free human premolars were divided mesio-distally into two equal halves.. Then the enamel was removed to expose the dentin and immersed in demineralizing solution for 96 h, which were then randomly allocated into three groups: Group-1: pretreatment with 38% SDF + RMGIC; Group-2: pretreatment with CPP-ACPF + RMGIC; and Group-3: No pretreatment + RMGIC (control). After the pre-treatment, resin modified glass ionomer cement was placed over the dentin surface using cylindrical mold. Then the micro-shear bond strength was evaluated using universal testing machine and mode of fracture was analyzed with stereomicroscopy. The micro-shear bond strength was found to be higher for the control group (35.73 ± 4.15) followed by SDF (28.39 ± 1.64) and CPP-ACPF (23.00 ± 2.17) and this difference was found to be statistically significant (p = 0.001). On analyzing the mode of failure, the adhesive type of failure was most common in all the groups and the difference in the percentages of mode of failure between the groups was not significant (p = 0.337). Application of 38% SDF and CPP-ACPF on demineralized dentin samples has shown to reduce the micro-shear bond strength of resin modified glass ionomer cement. Adhesive failures were the most common type of failures in both pretreated and untreated groups.</description><identifier>ISSN: 0970-7077</identifier><identifier>EISSN: 0975-427X</identifier><identifier>DOI: 10.14233/ajchem.2023.27589</identifier><language>eng</language><ispartof>Asian journal of chemistry, 2023-06, Vol.35 (6), p.1445-1448</ispartof><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed><cites>FETCH-LOGICAL-c1579-cd26c1f657a447d1fd3e14fbdbb463ef1e72371eed89cde11088ce0946c9d0f23</cites><orcidid>0009-0008-2251-8704 ; 0000-0003-2379-7238 ; 0000-0002-3477-0340 ; 0000-0003-2607-297X ; 0000-0003-4872-3067 ; 0000-0002-0668-4605</orcidid></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,780,784,27924,27925</link.rule.ids></links><search><creatorcontrib>PhaniKumar, Mettapalli Sai</creatorcontrib><creatorcontrib>RojaRamya, Kakarla Sri</creatorcontrib><creatorcontrib>Vinay, C.</creatorcontrib><creatorcontrib>Uloopi, K.S.</creatorcontrib><creatorcontrib>Alla, Rama Krishna</creatorcontrib><creatorcontrib>Chaitanya, Penmatsa</creatorcontrib><title>Effect of Dentine Pretreatment with 38% Silver Diamine Fluoride and CPP-ACPF on Micro-Shear Bond Strength of Resin Modified Glass Ionomer Cement</title><title>Asian journal of chemistry</title><description>The aim of the study is to evaluate the micro-shear bond strength and mode of failure of resin modified glass ionomer cement (RMGIC) placed on demineralized dentin pre-treated with 38% silver diamine fluoride (SDF) and casein phosphopeptide amorphous calcium phosphate (CPP-ACP). In order to mount the premolars in acrylic blocks, 30 caries-free human premolars were divided mesio-distally into two equal halves.. Then the enamel was removed to expose the dentin and immersed in demineralizing solution for 96 h, which were then randomly allocated into three groups: Group-1: pretreatment with 38% SDF + RMGIC; Group-2: pretreatment with CPP-ACPF + RMGIC; and Group-3: No pretreatment + RMGIC (control). After the pre-treatment, resin modified glass ionomer cement was placed over the dentin surface using cylindrical mold. Then the micro-shear bond strength was evaluated using universal testing machine and mode of fracture was analyzed with stereomicroscopy. The micro-shear bond strength was found to be higher for the control group (35.73 ± 4.15) followed by SDF (28.39 ± 1.64) and CPP-ACPF (23.00 ± 2.17) and this difference was found to be statistically significant (p = 0.001). On analyzing the mode of failure, the adhesive type of failure was most common in all the groups and the difference in the percentages of mode of failure between the groups was not significant (p = 0.337). Application of 38% SDF and CPP-ACPF on demineralized dentin samples has shown to reduce the micro-shear bond strength of resin modified glass ionomer cement. Adhesive failures were the most common type of failures in both pretreated and untreated groups.</description><issn>0970-7077</issn><issn>0975-427X</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2023</creationdate><recordtype>article</recordtype><recordid>eNotkMtOwzAQRS0EElXpD7DyhmWKH0mcLEv6oFIREQWJXeTaY-oqiZEdQPwFn4xbmM3MaK7OHV2ErimZ0pRxfisPag_dlBHGp0xkRXmGRqQUWZIy8Xp-mkkiiBCXaBLCgcTKacYEG6GfhTGgBuwMnkM_2B5w7WHwIIcu7vjLDnvMixu8te0neDy3sjuKlu2H81YDlr3GVV0ns6peYtfjB6u8S7Z7kB7fuXjcRlj_FinR4gmCjRKnrbGg8aqVIeC1610X0RUcHa_QhZFtgMl_H6OX5eK5uk82j6t1NdskimaiTJRmuaImz4RMU6Gp0RxoanZ6t0tzDoaCYFxQAF2USgOlpCgUkDLNVamJYXyM2B83vhuCB9O8e9tJ_91Q0pxibf5ibY6xNqdY-S8wGG0q</recordid><startdate>20230601</startdate><enddate>20230601</enddate><creator>PhaniKumar, Mettapalli Sai</creator><creator>RojaRamya, Kakarla Sri</creator><creator>Vinay, C.</creator><creator>Uloopi, K.S.</creator><creator>Alla, Rama Krishna</creator><creator>Chaitanya, Penmatsa</creator><scope>AAYXX</scope><scope>CITATION</scope><orcidid>https://orcid.org/0009-0008-2251-8704</orcidid><orcidid>https://orcid.org/0000-0003-2379-7238</orcidid><orcidid>https://orcid.org/0000-0002-3477-0340</orcidid><orcidid>https://orcid.org/0000-0003-2607-297X</orcidid><orcidid>https://orcid.org/0000-0003-4872-3067</orcidid><orcidid>https://orcid.org/0000-0002-0668-4605</orcidid></search><sort><creationdate>20230601</creationdate><title>Effect of Dentine Pretreatment with 38% Silver Diamine Fluoride and CPP-ACPF on Micro-Shear Bond Strength of Resin Modified Glass Ionomer Cement</title><author>PhaniKumar, Mettapalli Sai ; RojaRamya, Kakarla Sri ; Vinay, C. ; Uloopi, K.S. ; Alla, Rama Krishna ; Chaitanya, Penmatsa</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c1579-cd26c1f657a447d1fd3e14fbdbb463ef1e72371eed89cde11088ce0946c9d0f23</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2023</creationdate><toplevel>online_resources</toplevel><creatorcontrib>PhaniKumar, Mettapalli Sai</creatorcontrib><creatorcontrib>RojaRamya, Kakarla Sri</creatorcontrib><creatorcontrib>Vinay, C.</creatorcontrib><creatorcontrib>Uloopi, K.S.</creatorcontrib><creatorcontrib>Alla, Rama Krishna</creatorcontrib><creatorcontrib>Chaitanya, Penmatsa</creatorcontrib><collection>CrossRef</collection><jtitle>Asian journal of chemistry</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>PhaniKumar, Mettapalli Sai</au><au>RojaRamya, Kakarla Sri</au><au>Vinay, C.</au><au>Uloopi, K.S.</au><au>Alla, Rama Krishna</au><au>Chaitanya, Penmatsa</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Effect of Dentine Pretreatment with 38% Silver Diamine Fluoride and CPP-ACPF on Micro-Shear Bond Strength of Resin Modified Glass Ionomer Cement</atitle><jtitle>Asian journal of chemistry</jtitle><date>2023-06-01</date><risdate>2023</risdate><volume>35</volume><issue>6</issue><spage>1445</spage><epage>1448</epage><pages>1445-1448</pages><issn>0970-7077</issn><eissn>0975-427X</eissn><abstract>The aim of the study is to evaluate the micro-shear bond strength and mode of failure of resin modified glass ionomer cement (RMGIC) placed on demineralized dentin pre-treated with 38% silver diamine fluoride (SDF) and casein phosphopeptide amorphous calcium phosphate (CPP-ACP). In order to mount the premolars in acrylic blocks, 30 caries-free human premolars were divided mesio-distally into two equal halves.. Then the enamel was removed to expose the dentin and immersed in demineralizing solution for 96 h, which were then randomly allocated into three groups: Group-1: pretreatment with 38% SDF + RMGIC; Group-2: pretreatment with CPP-ACPF + RMGIC; and Group-3: No pretreatment + RMGIC (control). After the pre-treatment, resin modified glass ionomer cement was placed over the dentin surface using cylindrical mold. Then the micro-shear bond strength was evaluated using universal testing machine and mode of fracture was analyzed with stereomicroscopy. The micro-shear bond strength was found to be higher for the control group (35.73 ± 4.15) followed by SDF (28.39 ± 1.64) and CPP-ACPF (23.00 ± 2.17) and this difference was found to be statistically significant (p = 0.001). On analyzing the mode of failure, the adhesive type of failure was most common in all the groups and the difference in the percentages of mode of failure between the groups was not significant (p = 0.337). Application of 38% SDF and CPP-ACPF on demineralized dentin samples has shown to reduce the micro-shear bond strength of resin modified glass ionomer cement. Adhesive failures were the most common type of failures in both pretreated and untreated groups.</abstract><doi>10.14233/ajchem.2023.27589</doi><tpages>4</tpages><orcidid>https://orcid.org/0009-0008-2251-8704</orcidid><orcidid>https://orcid.org/0000-0003-2379-7238</orcidid><orcidid>https://orcid.org/0000-0002-3477-0340</orcidid><orcidid>https://orcid.org/0000-0003-2607-297X</orcidid><orcidid>https://orcid.org/0000-0003-4872-3067</orcidid><orcidid>https://orcid.org/0000-0002-0668-4605</orcidid><oa>free_for_read</oa></addata></record>
fulltext fulltext
identifier ISSN: 0970-7077
ispartof Asian journal of chemistry, 2023-06, Vol.35 (6), p.1445-1448
issn 0970-7077
0975-427X
language eng
recordid cdi_crossref_primary_10_14233_ajchem_2023_27589
source Alma/SFX Local Collection
title Effect of Dentine Pretreatment with 38% Silver Diamine Fluoride and CPP-ACPF on Micro-Shear Bond Strength of Resin Modified Glass Ionomer Cement
url http://sfxeu10.hosted.exlibrisgroup.com/loughborough?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-05T02%3A04%3A45IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-crossref&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Effect%20of%20Dentine%20Pretreatment%20with%2038%25%20Silver%20Diamine%20Fluoride%20and%20CPP-ACPF%20on%20Micro-Shear%20Bond%20Strength%20of%20Resin%20Modified%20Glass%20Ionomer%20Cement&rft.jtitle=Asian%20journal%20of%20chemistry&rft.au=PhaniKumar,%20Mettapalli%20Sai&rft.date=2023-06-01&rft.volume=35&rft.issue=6&rft.spage=1445&rft.epage=1448&rft.pages=1445-1448&rft.issn=0970-7077&rft.eissn=0975-427X&rft_id=info:doi/10.14233/ajchem.2023.27589&rft_dat=%3Ccrossref%3E10_14233_ajchem_2023_27589%3C/crossref%3E%3Cgrp_id%3Ecdi_FETCH-LOGICAL-c1579-cd26c1f657a447d1fd3e14fbdbb463ef1e72371eed89cde11088ce0946c9d0f23%3C/grp_id%3E%3Coa%3E%3C/oa%3E%3Curl%3E%3C/url%3E&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true