Color Stability of Ceramic Veneers Luted With Resin Cements and Pre-Heated Composites: 12 Months Follow-Up

Abstract The objective was to evaluate the color stability of ceramic veneers luted with resin cements and pre-heated composite resins (60oC) for 12 months, and determine the degree of conversion (DC) of the luting agents. Two resin cements (AllCem Veneer, light-cured (LRC) and AllCem, dual-cured (D...

Full description

Saved in:
Bibliographic Details
Published in:Brazilian dental journal 2020-01, Vol.31 (1), p.69-77
Main Authors: Gugelmin, Brenda Procopiak, Miguel, Luiz Carlos Machado, Baratto Filho, Flares, Cunha, Leonardo Fernandes da, Correr, Gisele Maria, Gonzaga, Carla Castiglia
Format: Article
Language:English
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Abstract The objective was to evaluate the color stability of ceramic veneers luted with resin cements and pre-heated composite resins (60oC) for 12 months, and determine the degree of conversion (DC) of the luting agents. Two resin cements (AllCem Veneer, light-cured (LRC) and AllCem, dual-cured (DRC)] and three composite resins [Z100 (MNCR-minifilled), Herculite Classic (MHCR-micro-hybrid) and Durafill (MCCR-microfilled)] were used for cementing 0.8-mm-thick lithium-silicate glass-ceramic laminates (Suprinity, shade B2-HT, Vita) on bovine enamel (n=10). The specimens were stored at 37oC in distilled water. CIELab parameters were determined at 24h after luting (baseline), 7, 30, 90, 180 days and 12 months. Three specimens were prepared for DC evaluation, performed by micro-Raman spectroscopy. Data were analyzed by ANOVA and Tukey’s test (a=5%). For ΔEab and ΔE00, there were significant differences for luting material (p
ISSN:0103-6440
1806-4760
DOI:10.1590/0103-6440202002842