Enriching SO42− Immobilization on α-Fe2O3 via Spatial Confinement for Robust NH3-SCR Denitration

The application of iron oxide to NH3-SCR is attractive but largely hindered by its poor acid properties, and surface sulfation is proven to be a prominent way of enhancing the acidity. As such, the method of enriching the sulfate species on iron oxide is crucial for improving the NH3-SCR performance...

Full description

Saved in:
Bibliographic Details
Published in:Catalysts 2022-09, Vol.12 (9), p.991
Main Authors: Gu, Zhiwen, Cheng, Lijun, Tan, Chong, Sin, Songil, Huang, Chunkai, Tang, Changjin
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:The application of iron oxide to NH3-SCR is attractive but largely hindered by its poor acid properties, and surface sulfation is proven to be a prominent way of enhancing the acidity. As such, the method of enriching the sulfate species on iron oxide is crucial for improving the NH3-SCR performance. In the present study, by employing ammonium bisulfate (ABS) as the source of gaseous SO2 for the purpose of trapping, we reported an effective strategy for enhancing the SO42− immobilization on α-Fe2O3 catalyst via spatial confinement in a mesoporous SBA-15 framework. Interestingly, although the presence of the mesopore channel had an adverse effect on the ABS decomposition, which was expected to produce less available SO2, the measured SO42− immobilized on α-Fe2O3 in the mesoporous SBA-15 system was significantly greater than that of the regular SiO2, demonstrating the promoting effect of the spatial confinement on the SO42− enrichment. Further characterizations of the NH3-TPD, NO oxidation, and NH3-SCR performance tests proved that, as a result of the enhanced acidity, the enrichment of SO42− on α-Fe2O3 displayed a clear correlation with the SCR activity. The results of the present study provide an effective strategy for boosting the catalytic performance of iron oxide in NH3-SCR via SO42− enrichment.
ISSN:2073-4344
2073-4344
DOI:10.3390/catal12090991