Shear performance and accelerated reliability of solder interconnects for fan-out wafer-level package

As the packaging density in wafer-level packaging increases, there is an increasing need for packaging processes for fan-out packaged devices; thus, the soldering reliability of board-level devices is particularly important. Fan-out wafer-level packaging (FOWLP) is typically packaged using flip-chip...

Full description

Saved in:
Bibliographic Details
Published in:Journal of advanced joining processes 2022-06, Vol.5, p.100076, Article 100076
Main Authors: Zhang, Shuye, Duan, Ran, Xu, Sunwu, Xue, Panfei, Wang, Chengqian, Chen, Jieshi, Paik, Kyung-Wook, He, Peng
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
cited_by cdi_FETCH-LOGICAL-c410t-850ff2a7f0089bb8a3b004571e8644d86e8b232c3e2e3b89e114f2319ec931a3
cites cdi_FETCH-LOGICAL-c410t-850ff2a7f0089bb8a3b004571e8644d86e8b232c3e2e3b89e114f2319ec931a3
container_end_page
container_issue
container_start_page 100076
container_title Journal of advanced joining processes
container_volume 5
creator Zhang, Shuye
Duan, Ran
Xu, Sunwu
Xue, Panfei
Wang, Chengqian
Chen, Jieshi
Paik, Kyung-Wook
He, Peng
description As the packaging density in wafer-level packaging increases, there is an increasing need for packaging processes for fan-out packaged devices; thus, the soldering reliability of board-level devices is particularly important. Fan-out wafer-level packaging (FOWLP) is typically packaged using flip-chip methods on Cu electrodes and printed circuit board (PCB) substrates. Therefore, in this study, we designed new PCBs based on a 6 × 4 mm2 FOWLP test vehicle with an electroless nickel gold (ENIG) surface finish. After optimizing 21 bonding parameters (temperature, holding time, and shear strength), the ideal bonding parameter was achieved at 260 °C for 10 s. We also found that the ENIG pads were dissolved in solder joints at conditions above 270 °C for 10 s, causing the pads to break away from the PCB and the solder joint failure. As a result, the mechanical properties of the joints declined. Under long high-temperature durations, the molten Sn bypassed the Ni layer, flowed into the bottom of the pad, and reacted with Cu, causing volume shrinkage of the solder joints and the pads to break away from the PCB.
doi_str_mv 10.1016/j.jajp.2021.100076
format article
fullrecord <record><control><sourceid>elsevier_doaj_</sourceid><recordid>TN_cdi_doaj_primary_oai_doaj_org_article_3e661cd4f66e4193a51dc52064637b8a</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S2666330921000364</els_id><doaj_id>oai_doaj_org_article_3e661cd4f66e4193a51dc52064637b8a</doaj_id><sourcerecordid>S2666330921000364</sourcerecordid><originalsourceid>FETCH-LOGICAL-c410t-850ff2a7f0089bb8a3b004571e8644d86e8b232c3e2e3b89e114f2319ec931a3</originalsourceid><addsrcrecordid>eNp9kMtOwzAQRS0EElXpD7DyD6T4kTiOxAZVPCpVYkH31sQZF4c0jpxQxN-TEIRYsZrR1dw7M4eQa87WnHF1U69rqLu1YIKPAmO5OiMLoZRKpGTF-Z_-kqz6vh5HhOZMy2xB8OUVIdIOowvxCK1FCm1FwVpsMMKAFY3YeCh944dPGhztQ1NhpL4dMNrQtmiHno5m6qBNwvtAP8BhTBo8YUM7sG9wwCty4aDpcfVTl2T_cL_fPCW758ft5m6X2JSzIdEZc05A7hjTRVlqkCVjaZZz1CpNK61Ql0IKK1GgLHWBnKdOSF6gLSQHuSTbObYKUJsu-iPETxPAm28hxIOBOHjboJGoFLdV6pTClBcSMl7ZTDCVKplPm5dEzFk2hr6P6H7zODMTdlObCbuZsJsZ-2i6nU04PnnyGE1vPY5QKx9HTuMZ_j_7F4zbi3A</addsrcrecordid><sourcetype>Open Website</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Shear performance and accelerated reliability of solder interconnects for fan-out wafer-level package</title><source>ScienceDirect Journals</source><creator>Zhang, Shuye ; Duan, Ran ; Xu, Sunwu ; Xue, Panfei ; Wang, Chengqian ; Chen, Jieshi ; Paik, Kyung-Wook ; He, Peng</creator><creatorcontrib>Zhang, Shuye ; Duan, Ran ; Xu, Sunwu ; Xue, Panfei ; Wang, Chengqian ; Chen, Jieshi ; Paik, Kyung-Wook ; He, Peng</creatorcontrib><description>As the packaging density in wafer-level packaging increases, there is an increasing need for packaging processes for fan-out packaged devices; thus, the soldering reliability of board-level devices is particularly important. Fan-out wafer-level packaging (FOWLP) is typically packaged using flip-chip methods on Cu electrodes and printed circuit board (PCB) substrates. Therefore, in this study, we designed new PCBs based on a 6 × 4 mm2 FOWLP test vehicle with an electroless nickel gold (ENIG) surface finish. After optimizing 21 bonding parameters (temperature, holding time, and shear strength), the ideal bonding parameter was achieved at 260 °C for 10 s. We also found that the ENIG pads were dissolved in solder joints at conditions above 270 °C for 10 s, causing the pads to break away from the PCB and the solder joint failure. As a result, the mechanical properties of the joints declined. Under long high-temperature durations, the molten Sn bypassed the Ni layer, flowed into the bottom of the pad, and reacted with Cu, causing volume shrinkage of the solder joints and the pads to break away from the PCB.</description><identifier>ISSN: 2666-3309</identifier><identifier>EISSN: 2666-3309</identifier><identifier>DOI: 10.1016/j.jajp.2021.100076</identifier><language>eng</language><publisher>Elsevier B.V</publisher><subject>Accelerated reliability ; Fan-out wafer-level package ; Shear strength ; Soldering process</subject><ispartof>Journal of advanced joining processes, 2022-06, Vol.5, p.100076, Article 100076</ispartof><rights>2021 The Author(s)</rights><lds50>peer_reviewed</lds50><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c410t-850ff2a7f0089bb8a3b004571e8644d86e8b232c3e2e3b89e114f2319ec931a3</citedby><cites>FETCH-LOGICAL-c410t-850ff2a7f0089bb8a3b004571e8644d86e8b232c3e2e3b89e114f2319ec931a3</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://www.sciencedirect.com/science/article/pii/S2666330921000364$$EHTML$$P50$$Gelsevier$$Hfree_for_read</linktohtml><link.rule.ids>314,780,784,3547,27923,27924,45779</link.rule.ids></links><search><creatorcontrib>Zhang, Shuye</creatorcontrib><creatorcontrib>Duan, Ran</creatorcontrib><creatorcontrib>Xu, Sunwu</creatorcontrib><creatorcontrib>Xue, Panfei</creatorcontrib><creatorcontrib>Wang, Chengqian</creatorcontrib><creatorcontrib>Chen, Jieshi</creatorcontrib><creatorcontrib>Paik, Kyung-Wook</creatorcontrib><creatorcontrib>He, Peng</creatorcontrib><title>Shear performance and accelerated reliability of solder interconnects for fan-out wafer-level package</title><title>Journal of advanced joining processes</title><description>As the packaging density in wafer-level packaging increases, there is an increasing need for packaging processes for fan-out packaged devices; thus, the soldering reliability of board-level devices is particularly important. Fan-out wafer-level packaging (FOWLP) is typically packaged using flip-chip methods on Cu electrodes and printed circuit board (PCB) substrates. Therefore, in this study, we designed new PCBs based on a 6 × 4 mm2 FOWLP test vehicle with an electroless nickel gold (ENIG) surface finish. After optimizing 21 bonding parameters (temperature, holding time, and shear strength), the ideal bonding parameter was achieved at 260 °C for 10 s. We also found that the ENIG pads were dissolved in solder joints at conditions above 270 °C for 10 s, causing the pads to break away from the PCB and the solder joint failure. As a result, the mechanical properties of the joints declined. Under long high-temperature durations, the molten Sn bypassed the Ni layer, flowed into the bottom of the pad, and reacted with Cu, causing volume shrinkage of the solder joints and the pads to break away from the PCB.</description><subject>Accelerated reliability</subject><subject>Fan-out wafer-level package</subject><subject>Shear strength</subject><subject>Soldering process</subject><issn>2666-3309</issn><issn>2666-3309</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2022</creationdate><recordtype>article</recordtype><sourceid>DOA</sourceid><recordid>eNp9kMtOwzAQRS0EElXpD7DyD6T4kTiOxAZVPCpVYkH31sQZF4c0jpxQxN-TEIRYsZrR1dw7M4eQa87WnHF1U69rqLu1YIKPAmO5OiMLoZRKpGTF-Z_-kqz6vh5HhOZMy2xB8OUVIdIOowvxCK1FCm1FwVpsMMKAFY3YeCh944dPGhztQ1NhpL4dMNrQtmiHno5m6qBNwvtAP8BhTBo8YUM7sG9wwCty4aDpcfVTl2T_cL_fPCW758ft5m6X2JSzIdEZc05A7hjTRVlqkCVjaZZz1CpNK61Ql0IKK1GgLHWBnKdOSF6gLSQHuSTbObYKUJsu-iPETxPAm28hxIOBOHjboJGoFLdV6pTClBcSMl7ZTDCVKplPm5dEzFk2hr6P6H7zODMTdlObCbuZsJsZ-2i6nU04PnnyGE1vPY5QKx9HTuMZ_j_7F4zbi3A</recordid><startdate>202206</startdate><enddate>202206</enddate><creator>Zhang, Shuye</creator><creator>Duan, Ran</creator><creator>Xu, Sunwu</creator><creator>Xue, Panfei</creator><creator>Wang, Chengqian</creator><creator>Chen, Jieshi</creator><creator>Paik, Kyung-Wook</creator><creator>He, Peng</creator><general>Elsevier B.V</general><general>Elsevier</general><scope>6I.</scope><scope>AAFTH</scope><scope>AAYXX</scope><scope>CITATION</scope><scope>DOA</scope></search><sort><creationdate>202206</creationdate><title>Shear performance and accelerated reliability of solder interconnects for fan-out wafer-level package</title><author>Zhang, Shuye ; Duan, Ran ; Xu, Sunwu ; Xue, Panfei ; Wang, Chengqian ; Chen, Jieshi ; Paik, Kyung-Wook ; He, Peng</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c410t-850ff2a7f0089bb8a3b004571e8644d86e8b232c3e2e3b89e114f2319ec931a3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2022</creationdate><topic>Accelerated reliability</topic><topic>Fan-out wafer-level package</topic><topic>Shear strength</topic><topic>Soldering process</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Zhang, Shuye</creatorcontrib><creatorcontrib>Duan, Ran</creatorcontrib><creatorcontrib>Xu, Sunwu</creatorcontrib><creatorcontrib>Xue, Panfei</creatorcontrib><creatorcontrib>Wang, Chengqian</creatorcontrib><creatorcontrib>Chen, Jieshi</creatorcontrib><creatorcontrib>Paik, Kyung-Wook</creatorcontrib><creatorcontrib>He, Peng</creatorcontrib><collection>ScienceDirect Open Access Titles</collection><collection>Elsevier:ScienceDirect:Open Access</collection><collection>CrossRef</collection><collection>DOAJ Directory of Open Access Journals</collection><jtitle>Journal of advanced joining processes</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Zhang, Shuye</au><au>Duan, Ran</au><au>Xu, Sunwu</au><au>Xue, Panfei</au><au>Wang, Chengqian</au><au>Chen, Jieshi</au><au>Paik, Kyung-Wook</au><au>He, Peng</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Shear performance and accelerated reliability of solder interconnects for fan-out wafer-level package</atitle><jtitle>Journal of advanced joining processes</jtitle><date>2022-06</date><risdate>2022</risdate><volume>5</volume><spage>100076</spage><pages>100076-</pages><artnum>100076</artnum><issn>2666-3309</issn><eissn>2666-3309</eissn><abstract>As the packaging density in wafer-level packaging increases, there is an increasing need for packaging processes for fan-out packaged devices; thus, the soldering reliability of board-level devices is particularly important. Fan-out wafer-level packaging (FOWLP) is typically packaged using flip-chip methods on Cu electrodes and printed circuit board (PCB) substrates. Therefore, in this study, we designed new PCBs based on a 6 × 4 mm2 FOWLP test vehicle with an electroless nickel gold (ENIG) surface finish. After optimizing 21 bonding parameters (temperature, holding time, and shear strength), the ideal bonding parameter was achieved at 260 °C for 10 s. We also found that the ENIG pads were dissolved in solder joints at conditions above 270 °C for 10 s, causing the pads to break away from the PCB and the solder joint failure. As a result, the mechanical properties of the joints declined. Under long high-temperature durations, the molten Sn bypassed the Ni layer, flowed into the bottom of the pad, and reacted with Cu, causing volume shrinkage of the solder joints and the pads to break away from the PCB.</abstract><pub>Elsevier B.V</pub><doi>10.1016/j.jajp.2021.100076</doi><oa>free_for_read</oa></addata></record>
fulltext fulltext
identifier ISSN: 2666-3309
ispartof Journal of advanced joining processes, 2022-06, Vol.5, p.100076, Article 100076
issn 2666-3309
2666-3309
language eng
recordid cdi_doaj_primary_oai_doaj_org_article_3e661cd4f66e4193a51dc52064637b8a
source ScienceDirect Journals
subjects Accelerated reliability
Fan-out wafer-level package
Shear strength
Soldering process
title Shear performance and accelerated reliability of solder interconnects for fan-out wafer-level package
url http://sfxeu10.hosted.exlibrisgroup.com/loughborough?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-11T12%3A34%3A59IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-elsevier_doaj_&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Shear%20performance%20and%20accelerated%20reliability%20of%20solder%20interconnects%20for%20fan-out%20wafer-level%20package&rft.jtitle=Journal%20of%20advanced%20joining%20processes&rft.au=Zhang,%20Shuye&rft.date=2022-06&rft.volume=5&rft.spage=100076&rft.pages=100076-&rft.artnum=100076&rft.issn=2666-3309&rft.eissn=2666-3309&rft_id=info:doi/10.1016/j.jajp.2021.100076&rft_dat=%3Celsevier_doaj_%3ES2666330921000364%3C/elsevier_doaj_%3E%3Cgrp_id%3Ecdi_FETCH-LOGICAL-c410t-850ff2a7f0089bb8a3b004571e8644d86e8b232c3e2e3b89e114f2319ec931a3%3C/grp_id%3E%3Coa%3E%3C/oa%3E%3Curl%3E%3C/url%3E&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true