The Influence of GGBFS as an Additive Replacement on the Kinetics of Cement Hydration and the Mechanical Properties of Cement Mortars

Granulated blast furnace slag (GBFS) is a byproduct of the iron production process. The objective of this study is to determine the effects of ground granulated blast furnace slag (GGBFS), used as a replacement admixture (0–40 wt.%) for ordinary Portland cement (OPC), on the setting time, the heat o...

Full description

Saved in:
Bibliographic Details
Published in:Buildings (Basel) 2023-08, Vol.13 (8), p.1960
Main Authors: Jozić, Dražan, Ljubičić, Branimir, Petrović, Andrija, Čović, Anđela, Juradin, Sandra
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Granulated blast furnace slag (GBFS) is a byproduct of the iron production process. The objective of this study is to determine the effects of ground granulated blast furnace slag (GGBFS), used as a replacement admixture (0–40 wt.%) for ordinary Portland cement (OPC), on the setting time, the heat of hydration, and the mechanical properties of cement mortar. The influence of GGBFS as a replacement additive on the setting time shows that it has an accelerating effect on cement hydration. Calorimetric measurements were performed on the cement paste system to determine the effects of GGBFS on the hydration of OPC. Calorimetric measurements carried out show that the replacement of GGBFS in an amount up to 40 wt.% reduces the total heat of hydration by up to 26.36% compared to the reference specimen. The kinetic analysis performed on the calorimetric data confirms the role of GGBFS as an accelerator by shortening the time during which the process of nucleation and growth (NG), as the most active part of hydration, is reduced up to 2.5 h. The value of the Avrami–Erofee constant indicates polydispersity and heterogeneous crystallization. Mechanical tests of cement mortars were performed after 3, 7, 14, 28, 70, and 90 days of hydration and showed that replacement addition of GGBFS slightly reduced the mechanical properties in the early phase of hydration, while in the later phase of hydration it contributed to an increase in the mechanical properties.