Effect of sintering temperature on translucency parameter of zirconia blocks

BackgroundThe main drawbacks of zirconia are its high refractive index and opacity. This study aimed to assess the effect of sintering temperature on the translucency of Ivoclar e. max ZirCAD (IEZ), and White Peaks Symphony (WPS) zirconia blocks. Materials and MethodsIn this in vitro experimental st...

Full description

Saved in:
Bibliographic Details
Published in:Dental research journal 2022-01, Vol.19 (1), p.82-82
Main Authors: Vafaei, Fariborz, Shahbazi, Armaghan, Hooshyarfard, Amirarsalan, Najafi, AmirHosein, Ebrahimi, Maziar, Farhadian, Maryam
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:BackgroundThe main drawbacks of zirconia are its high refractive index and opacity. This study aimed to assess the effect of sintering temperature on the translucency of Ivoclar e. max ZirCAD (IEZ), and White Peaks Symphony (WPS) zirconia blocks. Materials and MethodsIn this in vitro experimental study, 30 IEZ and 30 WPS zirconia blocks measuring 10 mm × 10 mm × 1 mm were prepared and underwent sintering in three subgroups at 1440°C, 1500°C, and 1530°C. The specimens were then photographed against a black and a white background with a standard digital camera. The L*, a*, and b* color parameters were measured using Adobe Photoshop software, and translucency was calculated. Data were analyzed using one-way ANOVA and Tukey's test (P < 0.05). ResultsIn both the IEZ and WPS groups, the maximum and minimum translucency parameters were recorded in 1530°C and 1440°C subgroups, respectively. The difference in the mean translucency was significant among the three subgroups of each zirconia group (P < 0.001). The mean translucency of WPS zirconia was significantly higher than that of IEZ zirconia (P < 0.01), and maximum difference was noted at 1500°C sintering temperature. ConclusionIncreasing the sintering temperature from 1440°C to 1530°C can significantly increase the translucency of IEZ and WPS zirconia blocks, and can be considered to improve the quality of zirconia restorations.