Oxidation of AISI 304L and 348 Stainless Steels in Water at High Temperatures

Oxidation of AISI 304L and 348 stainless steels was investigated in water at 1000 – 1350 °C by TGA, SEM, EDS, and Raman spectroscopy. Linear-Parabolic kinetics and multilayer oxide scales with voids were found for both alloys. Based on the experimental results, AISI 304L presented higher oxidation r...

Full description

Saved in:
Bibliographic Details
Published in:Materials research (São Carlos, São Paulo, Brazil) São Paulo, Brazil), 2020-01, Vol.23 (6), p.1
Main Authors: Avelar, Alan Matias, Giovedi, Claudia, Abe, Alfredo Yuuitiro, Mourão, Marcelo Breda
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Oxidation of AISI 304L and 348 stainless steels was investigated in water at 1000 – 1350 °C by TGA, SEM, EDS, and Raman spectroscopy. Linear-Parabolic kinetics and multilayer oxide scales with voids were found for both alloys. Based on the experimental results, AISI 304L presented higher oxidation resistance and higher activation energy. Zircaloy-4 kinetic results were used for validation and performance comparison. In severe accidents conditions, stainless steel might lead to a faster hydrogen production comparing to Zircaloy.