Dynamic Response of Copper Plates Subjected to Underwater Impulsive Loading

Understanding the mechanical response and failure behaviors of thin plates under impact loading is helpful for the design and improvement of thin plate structures in practical applications. The response of a copper plate subjected to underwater impulsive loading has been studied in fluid-structure i...

Full description

Saved in:
Bibliographic Details
Published in:Applied sciences 2019-05, Vol.9 (9), p.1927
Main Authors: Dai, Kaida, Liu, Han, Chen, Pengwan, Guo, Baoqiao, Xiang, Dalin, Rong, Jili
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Understanding the mechanical response and failure behaviors of thin plates under impact loading is helpful for the design and improvement of thin plate structures in practical applications. The response of a copper plate subjected to underwater impulsive loading has been studied in fluid-structure interaction (FSI) experiments. Three typical copper plates, (a) without a pre-notch, (b) with a cross-shaped pre-notch (+), and (c) with a ring-shaped pre-notch (○) were selected. A high-speed photography system recorded the full-field shape and displacement profiles of the specimens in real time. The 3D transient deformation fields’ measurements were obtained using a 3D digital image correlation (DIC) technique. Strain results from DIC and the strain gauges technique were in good agreement. A dimensionless deflection was used to analyze the effect of plate thickness and loading intensity on the deformation of the copper plates. The typical failure modes of different copper plates were identified. The test plates exhibited large ductile deformation (mode I ) for copper plates without a pre-notch, and large ductile deformation with local necking (mode I c ), splitting (mode II ), splitting and tearing (mode II c ), and fragment (mode III ) for the copper plate with a pre-notch.
ISSN:2076-3417
2076-3417
DOI:10.3390/app9091927