The Behavior of Pre-Treated Crumb Rubber and Polypropylene-Fiber-Incorporated Mortar Subjected to Elevated Temperatures
Rubber is a waste product produced by the industrial sector in large quantities. Due to its non-degradable nature, it has been a serious threat to the environment. Thus, it is recommended to develop concrete or mortar containing rubber, so that it can save our environment, and it is economical too....
Saved in:
Published in: | Engineering proceedings 2023-08, Vol.44 (1), p.12 |
---|---|
Main Authors: | , , |
Format: | Article |
Language: | English |
Subjects: | |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | Rubber is a waste product produced by the industrial sector in large quantities. Due to its non-degradable nature, it has been a serious threat to the environment. Thus, it is recommended to develop concrete or mortar containing rubber, so that it can save our environment, and it is economical too. Crumb rubber, when incorporated in mortar, reduces its strength, so it can be used along with some fibers to enhance its strength. This study examined the effect of elevated temperatures, i.e., 150, 300, 450, 600, and 750 °C, on mortar samples containing 5% crumb rubber replacement of fine aggregate by volume, and with the incorporation of 1% PPF. The findings indicated a rise in compressive strength up to 300 °C, followed by a subsequent decline. It was also observed that the weight loss of the samples increased with an increase in temperature. |
---|---|