High-Frequency Magnetic Impedance in BSi Amorphous Microwires in a Glass Sheath near the Curie Temperature
The temperature behavior of high-frequency magnetoimpedance (MI) in amorphous microwires in a glass sheath has been studied in the temperature range up to the Curie temperature T.sub.C. Two alloy samples with compositions of Co.sub.27.4Fe.sub.5B.sub.12.26Si.sub.12.26Ni.sub.43.08 (T.sub.C [almost equ...
Saved in:
Published in: | Physics of metals and metallography 2023-01, Vol.124 (1), p.1 |
---|---|
Main Authors: | , , , , , , |
Format: | Article |
Language: | English |
Subjects: | |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | The temperature behavior of high-frequency magnetoimpedance (MI) in amorphous microwires in a glass sheath has been studied in the temperature range up to the Curie temperature T.sub.C. Two alloy samples with compositions of Co.sub.27.4Fe.sub.5B.sub.12.26Si.sub.12.26Ni.sub.43.08 (T.sub.C [almost equal to] 48°C) and Co.sub.64.82Fe.sub.3.9B.sub.10.2Si.sub.12Cr.sub.9Mo.sub.0.08 (T.sub.C [almost equal to] 61°C) with different signs of magnetostriction constant [lambda].sub.s and with different types of magnetic anisotropy were used. For the first alloy sample, [lambda].sub.s 0, and easy axis anisotropy is formed along the wire axis. A substantial decrease in the impedance is observed at elevated frequencies with an increase in the temperature in microwires with easy axis anisotropy, regardless of the application of a magnetic field, while the change in the impedance in wires with circular anisotropy is more substantial in the presence of an external field. Moreover, the change in the impedance with an increase in the temperature from room temperature to T.sub.C can reach 200-300% in the frequency range of 0.5-0.9 GHz in a magnetic field of about 10 Oe. These results may be of interest for the development of miniature temperature sensors. |
---|---|
ISSN: | 0031-918X |
DOI: | 10.1134/S0031918X22601998 |