A comprehensive study of an unusual jammed nanocomposite structure using hybrid layered double hydroxide filler

Polystyrene nanocomposites using hybrid organic inorganic (O/I) layered double hydroxide (LDH) and 4[12-(methacryloylamino)dodecanoylamino]benzenesulfonate (MADABS) interleaved molecules were studied as a function of the filler miscibility, dispersion, and the rheological behavior. Incorporation of...

Full description

Saved in:
Bibliographic Details
Published in:Journal of colloid and interface science 2009-04, Vol.332 (2), p.327-335
Main Authors: Leroux, Fabrice, Illaik, Abdallah, Verney, Vincent
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
cited_by cdi_FETCH-LOGICAL-c418t-56e901bb8e10a9b0fa5299af816ded49f3ddfe81d4938b7d35b2d1981dc66d323
cites cdi_FETCH-LOGICAL-c418t-56e901bb8e10a9b0fa5299af816ded49f3ddfe81d4938b7d35b2d1981dc66d323
container_end_page 335
container_issue 2
container_start_page 327
container_title Journal of colloid and interface science
container_volume 332
creator Leroux, Fabrice
Illaik, Abdallah
Verney, Vincent
description Polystyrene nanocomposites using hybrid organic inorganic (O/I) layered double hydroxide (LDH) and 4[12-(methacryloylamino)dodecanoylamino]benzenesulfonate (MADABS) interleaved molecules were studied as a function of the filler miscibility, dispersion, and the rheological behavior. Incorporation of the I/O filler gave rise to an expanded intercalated PS nanocomposite structure, while an immiscible structure was obtained after a thermal pre-treatment. However the utmost non-linear viscoelasticity in the low- ω region was obtained from the immiscible PS nanocomposite structure. Indeed, the presence of a sub-micrometer percolated structure was here depicted resulting in a jammed structure that progressively changed the typical low-frequency Newtonian flow behavior of PS to a shear-thinning behavior against the filler percentage, having as a consequence to restrict the plastic deformation in the low- ω region by obstructing polymer chain motion. From several characterizations XRD, TEM, and rheology, we demonstrated the presence of LDH agglomerates in spite of PS chain crawling in between the layers, whereas the apparent immiscible structure was composed of well dispersed LDH tactoids forming a three-dimensional percolated network. The gel-like behavior illustrated by the frequency power law dependence of the complex viscosity | η ∗ | ∝ ω n , n ≈ − 0.75 at 10 wt% of MADABS/LDH hybrid filler was then explained by the interconnected and concatenated hybrid LDH platelets domains developing an interfacial attrition with PS chains. Interfacial attrition developed between layered double hydroxide platelets organo-modified by monomer surfactant and polystyrene was characterized by rheology under melt polymer condition.
doi_str_mv 10.1016/j.jcis.2008.12.056
format article
fullrecord <record><control><sourceid>proquest_hal_p</sourceid><recordid>TN_cdi_hal_primary_oai_HAL_hal_00399506v1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S0021979708017311</els_id><sourcerecordid>66948642</sourcerecordid><originalsourceid>FETCH-LOGICAL-c418t-56e901bb8e10a9b0fa5299af816ded49f3ddfe81d4938b7d35b2d1981dc66d323</originalsourceid><addsrcrecordid>eNp9kc2O0zAURi0EYjoDL8ACeQPSLBJ8nZ_GEptqBAxSJTawthz7hjpy4mLH1fTtcdQCO1a2Pp37yb6HkDfASmDQfhjLUdtYcsa6EnjJmvYZ2QATTbEFVj0nG8Y4FGIrtjfkNsaRMYCmES_JDQhoGNvWG-J3VPvpGPCAc7QnpHFJ5kz9QNVM05xiUo6OaprQ0FnNfoV9tMsKhqSXFJCmaOef9HDugzXUqTOGDBufeoc5NcE_WYN0sM5heEVeDMpFfH0978iPz5--PzwW-29fvj7s9oWuoVuKpkXBoO87BKZEzwbVcCHU0EFr0NRiqIwZsIN8rbp-a6qm5wZEDnTbmopXd-T-0ntQTh6DnVQ4S6-sfNzt5ZoxVgnRsPYEmX1_YY_B_0oYFznZqNE5NaNPUbatqLu2Xkv5BdTBxxhw-NsMTK5K5ChXJXJVIoHLrCQPvb22pz5v8d_I1UEG3l0BFbVyQ1Dz2vGH48DrOn8zcx8vHOa9nSwGGbXFWaOxAfUijbf_e8dv0K6ryA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>66948642</pqid></control><display><type>article</type><title>A comprehensive study of an unusual jammed nanocomposite structure using hybrid layered double hydroxide filler</title><source>ScienceDirect Journals</source><creator>Leroux, Fabrice ; Illaik, Abdallah ; Verney, Vincent</creator><creatorcontrib>Leroux, Fabrice ; Illaik, Abdallah ; Verney, Vincent</creatorcontrib><description>Polystyrene nanocomposites using hybrid organic inorganic (O/I) layered double hydroxide (LDH) and 4[12-(methacryloylamino)dodecanoylamino]benzenesulfonate (MADABS) interleaved molecules were studied as a function of the filler miscibility, dispersion, and the rheological behavior. Incorporation of the I/O filler gave rise to an expanded intercalated PS nanocomposite structure, while an immiscible structure was obtained after a thermal pre-treatment. However the utmost non-linear viscoelasticity in the low- ω region was obtained from the immiscible PS nanocomposite structure. Indeed, the presence of a sub-micrometer percolated structure was here depicted resulting in a jammed structure that progressively changed the typical low-frequency Newtonian flow behavior of PS to a shear-thinning behavior against the filler percentage, having as a consequence to restrict the plastic deformation in the low- ω region by obstructing polymer chain motion. From several characterizations XRD, TEM, and rheology, we demonstrated the presence of LDH agglomerates in spite of PS chain crawling in between the layers, whereas the apparent immiscible structure was composed of well dispersed LDH tactoids forming a three-dimensional percolated network. The gel-like behavior illustrated by the frequency power law dependence of the complex viscosity | η ∗ | ∝ ω n , n ≈ − 0.75 at 10 wt% of MADABS/LDH hybrid filler was then explained by the interconnected and concatenated hybrid LDH platelets domains developing an interfacial attrition with PS chains. Interfacial attrition developed between layered double hydroxide platelets organo-modified by monomer surfactant and polystyrene was characterized by rheology under melt polymer condition.</description><identifier>ISSN: 0021-9797</identifier><identifier>EISSN: 1095-7103</identifier><identifier>DOI: 10.1016/j.jcis.2008.12.056</identifier><identifier>PMID: 19150074</identifier><identifier>CODEN: JCISA5</identifier><language>eng</language><publisher>Amsterdam: Elsevier Inc</publisher><subject>Chemical Sciences ; Chemistry ; Colloidal state and disperse state ; Exact sciences and technology ; Filler for polymer ; General and physical chemistry ; Interfacial attrition ; Layered double hydroxide ; Polymers ; Rheology ; Surface physical chemistry</subject><ispartof>Journal of colloid and interface science, 2009-04, Vol.332 (2), p.327-335</ispartof><rights>2008 Elsevier Inc.</rights><rights>2009 INIST-CNRS</rights><rights>Distributed under a Creative Commons Attribution 4.0 International License</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c418t-56e901bb8e10a9b0fa5299af816ded49f3ddfe81d4938b7d35b2d1981dc66d323</citedby><cites>FETCH-LOGICAL-c418t-56e901bb8e10a9b0fa5299af816ded49f3ddfe81d4938b7d35b2d1981dc66d323</cites><orcidid>0000-0002-3900-9366 ; 0000-0002-4671-9630</orcidid></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>230,314,776,780,881,27901,27902</link.rule.ids><backlink>$$Uhttp://pascal-francis.inist.fr/vibad/index.php?action=getRecordDetail&amp;idt=21244493$$DView record in Pascal Francis$$Hfree_for_read</backlink><backlink>$$Uhttps://www.ncbi.nlm.nih.gov/pubmed/19150074$$D View this record in MEDLINE/PubMed$$Hfree_for_read</backlink><backlink>$$Uhttps://hal.science/hal-00399506$$DView record in HAL$$Hfree_for_read</backlink></links><search><creatorcontrib>Leroux, Fabrice</creatorcontrib><creatorcontrib>Illaik, Abdallah</creatorcontrib><creatorcontrib>Verney, Vincent</creatorcontrib><title>A comprehensive study of an unusual jammed nanocomposite structure using hybrid layered double hydroxide filler</title><title>Journal of colloid and interface science</title><addtitle>J Colloid Interface Sci</addtitle><description>Polystyrene nanocomposites using hybrid organic inorganic (O/I) layered double hydroxide (LDH) and 4[12-(methacryloylamino)dodecanoylamino]benzenesulfonate (MADABS) interleaved molecules were studied as a function of the filler miscibility, dispersion, and the rheological behavior. Incorporation of the I/O filler gave rise to an expanded intercalated PS nanocomposite structure, while an immiscible structure was obtained after a thermal pre-treatment. However the utmost non-linear viscoelasticity in the low- ω region was obtained from the immiscible PS nanocomposite structure. Indeed, the presence of a sub-micrometer percolated structure was here depicted resulting in a jammed structure that progressively changed the typical low-frequency Newtonian flow behavior of PS to a shear-thinning behavior against the filler percentage, having as a consequence to restrict the plastic deformation in the low- ω region by obstructing polymer chain motion. From several characterizations XRD, TEM, and rheology, we demonstrated the presence of LDH agglomerates in spite of PS chain crawling in between the layers, whereas the apparent immiscible structure was composed of well dispersed LDH tactoids forming a three-dimensional percolated network. The gel-like behavior illustrated by the frequency power law dependence of the complex viscosity | η ∗ | ∝ ω n , n ≈ − 0.75 at 10 wt% of MADABS/LDH hybrid filler was then explained by the interconnected and concatenated hybrid LDH platelets domains developing an interfacial attrition with PS chains. Interfacial attrition developed between layered double hydroxide platelets organo-modified by monomer surfactant and polystyrene was characterized by rheology under melt polymer condition.</description><subject>Chemical Sciences</subject><subject>Chemistry</subject><subject>Colloidal state and disperse state</subject><subject>Exact sciences and technology</subject><subject>Filler for polymer</subject><subject>General and physical chemistry</subject><subject>Interfacial attrition</subject><subject>Layered double hydroxide</subject><subject>Polymers</subject><subject>Rheology</subject><subject>Surface physical chemistry</subject><issn>0021-9797</issn><issn>1095-7103</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2009</creationdate><recordtype>article</recordtype><recordid>eNp9kc2O0zAURi0EYjoDL8ACeQPSLBJ8nZ_GEptqBAxSJTawthz7hjpy4mLH1fTtcdQCO1a2Pp37yb6HkDfASmDQfhjLUdtYcsa6EnjJmvYZ2QATTbEFVj0nG8Y4FGIrtjfkNsaRMYCmES_JDQhoGNvWG-J3VPvpGPCAc7QnpHFJ5kz9QNVM05xiUo6OaprQ0FnNfoV9tMsKhqSXFJCmaOef9HDugzXUqTOGDBufeoc5NcE_WYN0sM5heEVeDMpFfH0978iPz5--PzwW-29fvj7s9oWuoVuKpkXBoO87BKZEzwbVcCHU0EFr0NRiqIwZsIN8rbp-a6qm5wZEDnTbmopXd-T-0ntQTh6DnVQ4S6-sfNzt5ZoxVgnRsPYEmX1_YY_B_0oYFznZqNE5NaNPUbatqLu2Xkv5BdTBxxhw-NsMTK5K5ChXJXJVIoHLrCQPvb22pz5v8d_I1UEG3l0BFbVyQ1Dz2vGH48DrOn8zcx8vHOa9nSwGGbXFWaOxAfUijbf_e8dv0K6ryA</recordid><startdate>20090415</startdate><enddate>20090415</enddate><creator>Leroux, Fabrice</creator><creator>Illaik, Abdallah</creator><creator>Verney, Vincent</creator><general>Elsevier Inc</general><general>Elsevier</general><scope>IQODW</scope><scope>NPM</scope><scope>AAYXX</scope><scope>CITATION</scope><scope>7X8</scope><scope>1XC</scope><orcidid>https://orcid.org/0000-0002-3900-9366</orcidid><orcidid>https://orcid.org/0000-0002-4671-9630</orcidid></search><sort><creationdate>20090415</creationdate><title>A comprehensive study of an unusual jammed nanocomposite structure using hybrid layered double hydroxide filler</title><author>Leroux, Fabrice ; Illaik, Abdallah ; Verney, Vincent</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c418t-56e901bb8e10a9b0fa5299af816ded49f3ddfe81d4938b7d35b2d1981dc66d323</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2009</creationdate><topic>Chemical Sciences</topic><topic>Chemistry</topic><topic>Colloidal state and disperse state</topic><topic>Exact sciences and technology</topic><topic>Filler for polymer</topic><topic>General and physical chemistry</topic><topic>Interfacial attrition</topic><topic>Layered double hydroxide</topic><topic>Polymers</topic><topic>Rheology</topic><topic>Surface physical chemistry</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Leroux, Fabrice</creatorcontrib><creatorcontrib>Illaik, Abdallah</creatorcontrib><creatorcontrib>Verney, Vincent</creatorcontrib><collection>Pascal-Francis</collection><collection>PubMed</collection><collection>CrossRef</collection><collection>MEDLINE - Academic</collection><collection>Hyper Article en Ligne (HAL)</collection><jtitle>Journal of colloid and interface science</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Leroux, Fabrice</au><au>Illaik, Abdallah</au><au>Verney, Vincent</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>A comprehensive study of an unusual jammed nanocomposite structure using hybrid layered double hydroxide filler</atitle><jtitle>Journal of colloid and interface science</jtitle><addtitle>J Colloid Interface Sci</addtitle><date>2009-04-15</date><risdate>2009</risdate><volume>332</volume><issue>2</issue><spage>327</spage><epage>335</epage><pages>327-335</pages><issn>0021-9797</issn><eissn>1095-7103</eissn><coden>JCISA5</coden><abstract>Polystyrene nanocomposites using hybrid organic inorganic (O/I) layered double hydroxide (LDH) and 4[12-(methacryloylamino)dodecanoylamino]benzenesulfonate (MADABS) interleaved molecules were studied as a function of the filler miscibility, dispersion, and the rheological behavior. Incorporation of the I/O filler gave rise to an expanded intercalated PS nanocomposite structure, while an immiscible structure was obtained after a thermal pre-treatment. However the utmost non-linear viscoelasticity in the low- ω region was obtained from the immiscible PS nanocomposite structure. Indeed, the presence of a sub-micrometer percolated structure was here depicted resulting in a jammed structure that progressively changed the typical low-frequency Newtonian flow behavior of PS to a shear-thinning behavior against the filler percentage, having as a consequence to restrict the plastic deformation in the low- ω region by obstructing polymer chain motion. From several characterizations XRD, TEM, and rheology, we demonstrated the presence of LDH agglomerates in spite of PS chain crawling in between the layers, whereas the apparent immiscible structure was composed of well dispersed LDH tactoids forming a three-dimensional percolated network. The gel-like behavior illustrated by the frequency power law dependence of the complex viscosity | η ∗ | ∝ ω n , n ≈ − 0.75 at 10 wt% of MADABS/LDH hybrid filler was then explained by the interconnected and concatenated hybrid LDH platelets domains developing an interfacial attrition with PS chains. Interfacial attrition developed between layered double hydroxide platelets organo-modified by monomer surfactant and polystyrene was characterized by rheology under melt polymer condition.</abstract><cop>Amsterdam</cop><pub>Elsevier Inc</pub><pmid>19150074</pmid><doi>10.1016/j.jcis.2008.12.056</doi><tpages>9</tpages><orcidid>https://orcid.org/0000-0002-3900-9366</orcidid><orcidid>https://orcid.org/0000-0002-4671-9630</orcidid></addata></record>
fulltext fulltext
identifier ISSN: 0021-9797
ispartof Journal of colloid and interface science, 2009-04, Vol.332 (2), p.327-335
issn 0021-9797
1095-7103
language eng
recordid cdi_hal_primary_oai_HAL_hal_00399506v1
source ScienceDirect Journals
subjects Chemical Sciences
Chemistry
Colloidal state and disperse state
Exact sciences and technology
Filler for polymer
General and physical chemistry
Interfacial attrition
Layered double hydroxide
Polymers
Rheology
Surface physical chemistry
title A comprehensive study of an unusual jammed nanocomposite structure using hybrid layered double hydroxide filler
url http://sfxeu10.hosted.exlibrisgroup.com/loughborough?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-08T09%3A16%3A16IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_hal_p&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=A%20comprehensive%20study%20of%20an%20unusual%20jammed%20nanocomposite%20structure%20using%20hybrid%20layered%20double%20hydroxide%20filler&rft.jtitle=Journal%20of%20colloid%20and%20interface%20science&rft.au=Leroux,%20Fabrice&rft.date=2009-04-15&rft.volume=332&rft.issue=2&rft.spage=327&rft.epage=335&rft.pages=327-335&rft.issn=0021-9797&rft.eissn=1095-7103&rft.coden=JCISA5&rft_id=info:doi/10.1016/j.jcis.2008.12.056&rft_dat=%3Cproquest_hal_p%3E66948642%3C/proquest_hal_p%3E%3Cgrp_id%3Ecdi_FETCH-LOGICAL-c418t-56e901bb8e10a9b0fa5299af816ded49f3ddfe81d4938b7d35b2d1981dc66d323%3C/grp_id%3E%3Coa%3E%3C/oa%3E%3Curl%3E%3C/url%3E&rft_id=info:oai/&rft_pqid=66948642&rft_id=info:pmid/19150074&rfr_iscdi=true