Loading…

Critical parameters governing elastocaloric effect in polyisoprene rubbers for solid-state cooling

The aim of this work is to study the critical parameters governing the eCe (elastocaloric effect) of poly-isoprene rubber (NR and IR) in use conditions of a cooling device, i.e. under partial cyclic loading. The effect of mechanical cyclic loading parameters (pre-extension ratio, waveform and freque...

Full description

Saved in:
Bibliographic Details
Published in:Polymer (Guilford) 2024-07, Vol.307, p.127234, Article 127234
Main Authors: Haissoune, Hiba, Coativy, Gildas, Chazeau, Laurent, Lebrun, Laurent, Sebald, Gael, Chenal, Jean-Marc
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:The aim of this work is to study the critical parameters governing the eCe (elastocaloric effect) of poly-isoprene rubber (NR and IR) in use conditions of a cooling device, i.e. under partial cyclic loading. The effect of mechanical cyclic loading parameters (pre-extension ratio, waveform and frequency) on eCe was first studied. It shows that the eCe increases when the mimimum pre-extension ratio is increased and frequency is lowered from 1Hz to 0.001Hz, as it promotes strain-induced crystallization. However, it also leads to a decrease in potential cooling power, from 7 to 0.01 MW/m3 (i.e. 8 kW/kg to 0.01 kW/kg). At intermediate frequency (f ≈ 0.1 Hz), the comparison of square and triangular waveforms demonstrated that the former enables greater temperature variation. This is due to its holding step (at maximum extension ratio), which maximizes crystallization but also promotes stress relaxation, resulting in increased mechanical losses. Consequently, the square and triangular loadings have a COPmat of 12 and 25, with a temperature variation of 4.2K and 3.6K, respectively. Regarding the formulation, rubbers that do not have a great tendency to crystallize such as synthetic polyisoprene rubber seem to have the best COPmat, while to maximize ΔT, the best of our formulations are NR crosslinked with sulfur and having a crosslink density close to 1.5 × 10−4 mol/cm3, which combine large strain induced crystallization and entropic elasticity. This material has a COPmat of about 27 and allows a ΔT≈4K, i.e.performance comparable to that of the best Shape Memory Alloys (at equivalent COPmat). [Display omitted] •Study of the elastocaloric effect of different formulations of polyisoprene rubbers.•The use of square waveform increases ΔT and the mechanical hysteresis.•The use of triangular waveform improves the COPmat.•Beyond 0.1 Hz, entropic elasticity is the main contribution to elastocaloric effect.•NR crosslinked with sulfur with ν ≈ 1.5 × 10−4 mol/cm3 shows the best eCe.
ISSN:0032-3861
1873-2291
DOI:10.1016/j.polymer.2024.127234