Loading…

Gas absorption between 1.8 and 2.1 μm in low loss (5.2 dB/km) HC-PBGF

19-cell defect HC-PBGF is fabricated with record low loss (5.2 dB/km) at 2 μm. Gas absorption lines present in the fiber post-fabrication are quantified with initial conclusions on the origin and removal of relevant species.

Saved in:
Bibliographic Details
Main Authors: Wheeler, N. V., Petrovich, M. N., Baddela, N. K., Hayes, J. R., Fokoua, E. N., Poletti, F., Richardson, D. J.
Format: Conference Proceeding
Language:English
Subjects:
Online Access:Request full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:19-cell defect HC-PBGF is fabricated with record low loss (5.2 dB/km) at 2 μm. Gas absorption lines present in the fiber post-fabrication are quantified with initial conclusions on the origin and removal of relevant species.