The elastic thermoelectric generator (ETEG) was fabricated by using 27 couples of n-Bi 2 Te 3 and p-Sb 2 Te 3 bulk thermoelectric materials in size of 3 × 3 × 5 mm 3 on silicone substrate and using copper plate for electrodes. It was found that the open circuit voltage shows maximum value of 46.74 m...

Full description

Saved in:
Bibliographic Details
Published in:Journal of physics. Conference series 2021-09, Vol.2013 (1), p.12024
Main Authors: Manawong, Piyada, Singsoog, Kunchit, Seetawan, Tosawat
Format: Article
Language:English
Citations: Items that this one cites
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:The elastic thermoelectric generator (ETEG) was fabricated by using 27 couples of n-Bi 2 Te 3 and p-Sb 2 Te 3 bulk thermoelectric materials in size of 3 × 3 × 5 mm 3 on silicone substrate and using copper plate for electrodes. It was found that the open circuit voltage shows maximum value of 46.74 mV at temperature difference 13.85 K. External load resistances were apply in the measurement and varies for obtaining the maximum output power. The matched load resistance is 0.22 Ω obtaining maximum power about 3.46 mW at temperature difference difference of 13.85 K. The output power, voltage and current were increased with temperature difference increasing and show maximum values about 35.19 mW, 27.82 mV and 126.36 mA at temperature difference 12.75 K.