Induction Hardening Process of G18NiMoCr3-6 Steel

The microstructure and properties of G18NiMoCr3-6 steel after medium frequency. Quenching hardening with different process parameters and its heat treatment process optimizing were studied. The results show that the best combination is voltage 420V, cooling water flow 300L/h, moving speed 200mm/min....

Full description

Saved in:
Bibliographic Details
Published in:IOP conference series. Materials Science and Engineering 2019-12, Vol.677 (2), p.22085
Main Authors: Tang, Cai, Chen, Bo, Fan, Huiji
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:The microstructure and properties of G18NiMoCr3-6 steel after medium frequency. Quenching hardening with different process parameters and its heat treatment process optimizing were studied. The results show that the best combination is voltage 420V, cooling water flow 300L/h, moving speed 200mm/min. After medium frequency induction hardening process, the surface of G18NiMoCr3-6 steel generates uniform and small martensite, the strength and wear resistance significantly increases.