Loading…

Toughening and reinforcing alumina matrix composite with single-wall carbon nanotubes

The authors report an efficient way of incorporating single-wall carbon nanotubes (SWNTs) into alumina matrix with strong interfaces by heterocoagulation. The fracture toughness of SWNTs/ Al 2 O 3 composite reaches 6.40 ± 0.3 MPa m 1 ∕ 2 , which is twice as high as that of unreinforced alumina. The...

Full description

Saved in:
Bibliographic Details
Published in:Applied physics letters 2006-09, Vol.89 (12), p.121910-121910-3
Main Authors: Fan, Jin-Peng, Zhuang, Da-Ming, Zhao, Da-Qing, Zhang, Gong, Wu, Min-Sheng, Wei, Fei, Fan, Zhuang-Jun
Format: Article
Language:English
Subjects:
Citations: Items that this one cites
Items that cite this one
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:The authors report an efficient way of incorporating single-wall carbon nanotubes (SWNTs) into alumina matrix with strong interfaces by heterocoagulation. The fracture toughness of SWNTs/ Al 2 O 3 composite reaches 6.40 ± 0.3 MPa m 1 ∕ 2 , which is twice as high as that of unreinforced alumina. The flexure strength of the composite also increases by 20%. The main toughening mechanism is crack bridging of SWNTs, and SWNT pullout takes effect also.
ISSN:0003-6951
1077-3118
DOI:10.1063/1.2336623