POLYURETHANES FROM 4,4′-DIPHENYLMETHANE DIISOCYANATE AND POLY(OXYETHYLENE) GLYCOLS. I. PREPARATION AND GENERAL PROPERTIES
Linear polyurethanes (PU) from 4,4′-diphenylmethane diisocyanate and an equimolar quantity of poly(oxyethylene) glycol (PEG) of various molecular weight (106, 200, 400, 1000, 2000, and 4000) were obtained by polymerization using 4-methylpentanone-2 as solvent at 115 °C. Alternative reaction conditio...
Saved in:
Published in: | Journal of macromolecular science. Part A, Pure and applied chemistry Pure and applied chemistry, 2001-06, Vol.38 (7), p.673-680 |
---|---|
Main Authors: | , |
Format: | Article |
Language: | English |
Subjects: | |
Citations: | Items that cite this one |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | Linear polyurethanes (PU) from 4,4′-diphenylmethane diisocyanate and an equimolar quantity of poly(oxyethylene) glycol (PEG) of various molecular weight (106, 200, 400, 1000, 2000, and 4000) were obtained by polymerization using 4-methylpentanone-2 as solvent at 115 °C. Alternative reaction conditions and melt polymerization were also applied. Samples were characterized by elemental analysis, solubility, I.R. spectroscopy, DSC (T
m
,
T
g
), [n] and [Mbar]
n
(osmotic). The results are correlated with the molecular weight of PEG and discussed. |
---|---|