Dielectric and Raman investigations on M2(SO4). Te(OH)6 (m =k, Rb and Cs)

Dielectric and Raman investigations in the temperature and frequency ranges 300-550K and 10 2 - 10 4 Hz respectively show that M 2 (SO 4 ). Te(OH) 6 with (M = K, Rb and Cs) materials present three phase transition. The first transition observed at 480, 440 and 460K respectively for M = K, Rb and Cs...

Full description

Saved in:
Bibliographic Details
Published in:Ferroelectrics 1999-01, Vol.234 (1), p.47-59
Main Author: Khemakhem, Hamadi
Format: Article
Language:English
Subjects:
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Dielectric and Raman investigations in the temperature and frequency ranges 300-550K and 10 2 - 10 4 Hz respectively show that M 2 (SO 4 ). Te(OH) 6 with (M = K, Rb and Cs) materials present three phase transition. The first transition observed at 480, 440 and 460K respectively for M = K, Rb and Cs and should be probably of order-disorder type. The second one was observed only for Rb 2 (SO 4 ). Te(OH) 6 and Cs 2 (SO 4 ). Te(OH) 6 respectively at 510 and 495K. The third peak observed at 490, 520 and 510K for M = K, Rb and Cs respectively can be attributed to a ferroelectric-paraelectric phase transition.
ISSN:0015-0193
1563-5112
DOI:10.1080/00150199908225281