Pre-Corrosion and Surface Treatments Effects on the Fatigue Life of AA6082 T6
Applying of surface treatments as shot peening and ball burnishing had markedly enhanced the fatigue life of AA6082 T6. Both surface treatments resulted in a surface strengthen and induced compressive residual stresses in the near surface regions. Pre‐corrosion in 3.5% NaCl solution resulted in nume...
Saved in:
Published in: | Advanced engineering materials 2013-10, Vol.15 (10), p.1002-1006 |
---|---|
Main Authors: | , , |
Format: | Article |
Language: | English |
Subjects: | |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | Applying of surface treatments as shot peening and ball burnishing had markedly enhanced the fatigue life of AA6082 T6. Both surface treatments resulted in a surface strengthen and induced compressive residual stresses in the near surface regions. Pre‐corrosion in 3.5% NaCl solution resulted in numerous surface pits that led to degradation of fatigue life of the reference electrolytically polished conditions. These detrimental effects on fatigue life could be entirely eliminated by applying surface treatments either before or after pre‐corrosion. |
---|---|
ISSN: | 1438-1656 1527-2648 |
DOI: | 10.1002/adem.201300054 |