Effect of wear debris of Al^sub 2^O3, ZrO2 and WC balls on Y-[alpha]/[beta]-SiAlON ceramics consolidated by spark plasma sintering

Three types of Y-[alpha]/[beta]-SiAlON powders were prepared by mixing and milling the raw materials for 20 h using Al^sub 2^O3, ZrO2, and WC balls, thereafter denoted as SNA, SNZ and SNW, respectively. The three types of specimens were sintered using spark plasma sintering (SPS) at 1510 °C for 5 mi...

Full description

Saved in:
Bibliographic Details
Published in:Metals and materials international 2013-03, Vol.19 (2), p.163
Main Authors: Chun, Sungsu, Min, Bong-ki, Han, Young-hwan, Kim, Young-moon, Lee, Kyeongseok, Jung, Young Geun, Kim, Kwang-ho, Kim, Young-ki, Kim, Sukyoung
Format: Article
Language:English
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
cited_by
cites
container_end_page
container_issue 2
container_start_page 163
container_title Metals and materials international
container_volume 19
creator Chun, Sungsu
Min, Bong-ki
Han, Young-hwan
Kim, Young-moon
Lee, Kyeongseok
Jung, Young Geun
Kim, Kwang-ho
Kim, Young-ki
Kim, Sukyoung
description Three types of Y-[alpha]/[beta]-SiAlON powders were prepared by mixing and milling the raw materials for 20 h using Al^sub 2^O3, ZrO2, and WC balls, thereafter denoted as SNA, SNZ and SNW, respectively. The three types of specimens were sintered using spark plasma sintering (SPS) at 1510 °C for 5 min under 30 MPa in a vacuum. [alpha]-phases (SiAlON and Si^sub 3^N^sub 4^) and [beta]-SiAlON phase were observed in the SNA and SNZ specimens, but only the [beta]-SiAlON phase existed in the SNW specimen. The wear debris of the WC balls affected the grain boundary properties and eventually promoted the full phase transformation of [alpha]-Si^sub 3^N^sub 4^ into [alpha]- and [beta]-SiAlON phases. However, SNA and SNZ were partially transformed into [alpha]- and [beta]-SiAlON phases. The Vickers hardness of SNA was the highest (18.7 GPa), due to its having the highest content of [alpha]-phase, but its fracture toughness was the lowest (4.09 MPam^sup 1/2^) due to its having the lowest content of [beta]-SiAlON phase. The wear debris and secondary phases existed at the grain boundary, mostly at the triple junction, and also affected the color. The color of the sintered specimen was quite different depending on the milling media.[PUBLICATION ABSTRACT]
doi_str_mv 10.1007/s12540-013-2005-2
format article
fullrecord <record><control><sourceid>proquest</sourceid><recordid>TN_cdi_proquest_journals_1317165270</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>2918995971</sourcerecordid><originalsourceid>FETCH-proquest_journals_13171652703</originalsourceid><addsrcrecordid>eNqNjr1OwzAUhS0EEqHwAGxXYsXUdv7IWFVFnchQJARVW90kDri4dvBNhFh5cgLiAZjOOfq-4TB2KcWNFCKfklRpIriQMVdCpFwdsei3JDIpjlkk0-KWF5mKT9kZ0V6ITMZSRexr0ba67sG38KExQKOrYOhnzuyWhgrUtoyv4TmUCtA18DiHCq0dDQdPfI22e8XNdF3pHjd8ZWa2vIdaBzyYmqD2jrw1Dfa6geoTqMPwBp1FOiCQcb0Oxr2cs5MWLemLv5ywq7vFw3zJu-DfB039bu-H4Ea0Gz_nMktVLuL_Wd-a-VUq</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>1317165270</pqid></control><display><type>article</type><title>Effect of wear debris of Al^sub 2^O3, ZrO2 and WC balls on Y-[alpha]/[beta]-SiAlON ceramics consolidated by spark plasma sintering</title><source>Springer Nature</source><creator>Chun, Sungsu ; Min, Bong-ki ; Han, Young-hwan ; Kim, Young-moon ; Lee, Kyeongseok ; Jung, Young Geun ; Kim, Kwang-ho ; Kim, Young-ki ; Kim, Sukyoung</creator><creatorcontrib>Chun, Sungsu ; Min, Bong-ki ; Han, Young-hwan ; Kim, Young-moon ; Lee, Kyeongseok ; Jung, Young Geun ; Kim, Kwang-ho ; Kim, Young-ki ; Kim, Sukyoung</creatorcontrib><description>Three types of Y-[alpha]/[beta]-SiAlON powders were prepared by mixing and milling the raw materials for 20 h using Al^sub 2^O3, ZrO2, and WC balls, thereafter denoted as SNA, SNZ and SNW, respectively. The three types of specimens were sintered using spark plasma sintering (SPS) at 1510 °C for 5 min under 30 MPa in a vacuum. [alpha]-phases (SiAlON and Si^sub 3^N^sub 4^) and [beta]-SiAlON phase were observed in the SNA and SNZ specimens, but only the [beta]-SiAlON phase existed in the SNW specimen. The wear debris of the WC balls affected the grain boundary properties and eventually promoted the full phase transformation of [alpha]-Si^sub 3^N^sub 4^ into [alpha]- and [beta]-SiAlON phases. However, SNA and SNZ were partially transformed into [alpha]- and [beta]-SiAlON phases. The Vickers hardness of SNA was the highest (18.7 GPa), due to its having the highest content of [alpha]-phase, but its fracture toughness was the lowest (4.09 MPam^sup 1/2^) due to its having the lowest content of [beta]-SiAlON phase. The wear debris and secondary phases existed at the grain boundary, mostly at the triple junction, and also affected the color. The color of the sintered specimen was quite different depending on the milling media.[PUBLICATION ABSTRACT]</description><identifier>ISSN: 1598-9623</identifier><identifier>EISSN: 2005-4149</identifier><identifier>DOI: 10.1007/s12540-013-2005-2</identifier><language>eng</language><publisher>Seoul: Springer Nature B.V</publisher><ispartof>Metals and materials international, 2013-03, Vol.19 (2), p.163</ispartof><rights>The Korean Institute of Metals and Materials and Springer Science+Business Media Dordrecht 2013</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,780,784,27922,27923</link.rule.ids></links><search><creatorcontrib>Chun, Sungsu</creatorcontrib><creatorcontrib>Min, Bong-ki</creatorcontrib><creatorcontrib>Han, Young-hwan</creatorcontrib><creatorcontrib>Kim, Young-moon</creatorcontrib><creatorcontrib>Lee, Kyeongseok</creatorcontrib><creatorcontrib>Jung, Young Geun</creatorcontrib><creatorcontrib>Kim, Kwang-ho</creatorcontrib><creatorcontrib>Kim, Young-ki</creatorcontrib><creatorcontrib>Kim, Sukyoung</creatorcontrib><title>Effect of wear debris of Al^sub 2^O3, ZrO2 and WC balls on Y-[alpha]/[beta]-SiAlON ceramics consolidated by spark plasma sintering</title><title>Metals and materials international</title><description>Three types of Y-[alpha]/[beta]-SiAlON powders were prepared by mixing and milling the raw materials for 20 h using Al^sub 2^O3, ZrO2, and WC balls, thereafter denoted as SNA, SNZ and SNW, respectively. The three types of specimens were sintered using spark plasma sintering (SPS) at 1510 °C for 5 min under 30 MPa in a vacuum. [alpha]-phases (SiAlON and Si^sub 3^N^sub 4^) and [beta]-SiAlON phase were observed in the SNA and SNZ specimens, but only the [beta]-SiAlON phase existed in the SNW specimen. The wear debris of the WC balls affected the grain boundary properties and eventually promoted the full phase transformation of [alpha]-Si^sub 3^N^sub 4^ into [alpha]- and [beta]-SiAlON phases. However, SNA and SNZ were partially transformed into [alpha]- and [beta]-SiAlON phases. The Vickers hardness of SNA was the highest (18.7 GPa), due to its having the highest content of [alpha]-phase, but its fracture toughness was the lowest (4.09 MPam^sup 1/2^) due to its having the lowest content of [beta]-SiAlON phase. The wear debris and secondary phases existed at the grain boundary, mostly at the triple junction, and also affected the color. The color of the sintered specimen was quite different depending on the milling media.[PUBLICATION ABSTRACT]</description><issn>1598-9623</issn><issn>2005-4149</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2013</creationdate><recordtype>article</recordtype><recordid>eNqNjr1OwzAUhS0EEqHwAGxXYsXUdv7IWFVFnchQJARVW90kDri4dvBNhFh5cgLiAZjOOfq-4TB2KcWNFCKfklRpIriQMVdCpFwdsei3JDIpjlkk0-KWF5mKT9kZ0V6ITMZSRexr0ba67sG38KExQKOrYOhnzuyWhgrUtoyv4TmUCtA18DiHCq0dDQdPfI22e8XNdF3pHjd8ZWa2vIdaBzyYmqD2jrw1Dfa6geoTqMPwBp1FOiCQcb0Oxr2cs5MWLemLv5ywq7vFw3zJu-DfB039bu-H4Ea0Gz_nMktVLuL_Wd-a-VUq</recordid><startdate>20130301</startdate><enddate>20130301</enddate><creator>Chun, Sungsu</creator><creator>Min, Bong-ki</creator><creator>Han, Young-hwan</creator><creator>Kim, Young-moon</creator><creator>Lee, Kyeongseok</creator><creator>Jung, Young Geun</creator><creator>Kim, Kwang-ho</creator><creator>Kim, Young-ki</creator><creator>Kim, Sukyoung</creator><general>Springer Nature B.V</general><scope>7SR</scope><scope>8BQ</scope><scope>8FD</scope><scope>8FE</scope><scope>8FG</scope><scope>ABJCF</scope><scope>AFKRA</scope><scope>BENPR</scope><scope>BGLVJ</scope><scope>CCPQU</scope><scope>D1I</scope><scope>DWQXO</scope><scope>HCIFZ</scope><scope>JG9</scope><scope>KB.</scope><scope>PDBOC</scope><scope>PQEST</scope><scope>PQQKQ</scope><scope>PQUKI</scope><scope>PRINS</scope></search><sort><creationdate>20130301</creationdate><title>Effect of wear debris of Al^sub 2^O3, ZrO2 and WC balls on Y-[alpha]/[beta]-SiAlON ceramics consolidated by spark plasma sintering</title><author>Chun, Sungsu ; Min, Bong-ki ; Han, Young-hwan ; Kim, Young-moon ; Lee, Kyeongseok ; Jung, Young Geun ; Kim, Kwang-ho ; Kim, Young-ki ; Kim, Sukyoung</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-proquest_journals_13171652703</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2013</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Chun, Sungsu</creatorcontrib><creatorcontrib>Min, Bong-ki</creatorcontrib><creatorcontrib>Han, Young-hwan</creatorcontrib><creatorcontrib>Kim, Young-moon</creatorcontrib><creatorcontrib>Lee, Kyeongseok</creatorcontrib><creatorcontrib>Jung, Young Geun</creatorcontrib><creatorcontrib>Kim, Kwang-ho</creatorcontrib><creatorcontrib>Kim, Young-ki</creatorcontrib><creatorcontrib>Kim, Sukyoung</creatorcontrib><collection>Engineered Materials Abstracts</collection><collection>METADEX</collection><collection>Technology Research Database</collection><collection>ProQuest SciTech Collection</collection><collection>ProQuest Technology Collection</collection><collection>Materials Science &amp; Engineering Collection</collection><collection>ProQuest Central</collection><collection>AUTh Library subscriptions: ProQuest Central</collection><collection>Technology Collection</collection><collection>ProQuest One Community College</collection><collection>ProQuest Materials Science Collection</collection><collection>ProQuest Central</collection><collection>SciTech Premium Collection</collection><collection>Materials Research Database</collection><collection>Materials Science Database</collection><collection>Materials Science Collection</collection><collection>ProQuest One Academic Eastern Edition (DO NOT USE)</collection><collection>ProQuest One Academic</collection><collection>ProQuest One Academic UKI Edition</collection><collection>ProQuest Central China</collection><jtitle>Metals and materials international</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Chun, Sungsu</au><au>Min, Bong-ki</au><au>Han, Young-hwan</au><au>Kim, Young-moon</au><au>Lee, Kyeongseok</au><au>Jung, Young Geun</au><au>Kim, Kwang-ho</au><au>Kim, Young-ki</au><au>Kim, Sukyoung</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Effect of wear debris of Al^sub 2^O3, ZrO2 and WC balls on Y-[alpha]/[beta]-SiAlON ceramics consolidated by spark plasma sintering</atitle><jtitle>Metals and materials international</jtitle><date>2013-03-01</date><risdate>2013</risdate><volume>19</volume><issue>2</issue><spage>163</spage><pages>163-</pages><issn>1598-9623</issn><eissn>2005-4149</eissn><abstract>Three types of Y-[alpha]/[beta]-SiAlON powders were prepared by mixing and milling the raw materials for 20 h using Al^sub 2^O3, ZrO2, and WC balls, thereafter denoted as SNA, SNZ and SNW, respectively. The three types of specimens were sintered using spark plasma sintering (SPS) at 1510 °C for 5 min under 30 MPa in a vacuum. [alpha]-phases (SiAlON and Si^sub 3^N^sub 4^) and [beta]-SiAlON phase were observed in the SNA and SNZ specimens, but only the [beta]-SiAlON phase existed in the SNW specimen. The wear debris of the WC balls affected the grain boundary properties and eventually promoted the full phase transformation of [alpha]-Si^sub 3^N^sub 4^ into [alpha]- and [beta]-SiAlON phases. However, SNA and SNZ were partially transformed into [alpha]- and [beta]-SiAlON phases. The Vickers hardness of SNA was the highest (18.7 GPa), due to its having the highest content of [alpha]-phase, but its fracture toughness was the lowest (4.09 MPam^sup 1/2^) due to its having the lowest content of [beta]-SiAlON phase. The wear debris and secondary phases existed at the grain boundary, mostly at the triple junction, and also affected the color. The color of the sintered specimen was quite different depending on the milling media.[PUBLICATION ABSTRACT]</abstract><cop>Seoul</cop><pub>Springer Nature B.V</pub><doi>10.1007/s12540-013-2005-2</doi></addata></record>
fulltext fulltext
identifier ISSN: 1598-9623
ispartof Metals and materials international, 2013-03, Vol.19 (2), p.163
issn 1598-9623
2005-4149
language eng
recordid cdi_proquest_journals_1317165270
source Springer Nature
title Effect of wear debris of Al^sub 2^O3, ZrO2 and WC balls on Y-[alpha]/[beta]-SiAlON ceramics consolidated by spark plasma sintering
url http://sfxeu10.hosted.exlibrisgroup.com/loughborough?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-14T00%3A22%3A35IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Effect%20of%20wear%20debris%20of%20Al%5Esub%202%5EO3,%20ZrO2%20and%20WC%20balls%20on%20Y-%5Balpha%5D/%5Bbeta%5D-SiAlON%20ceramics%20consolidated%20by%20spark%20plasma%20sintering&rft.jtitle=Metals%20and%20materials%20international&rft.au=Chun,%20Sungsu&rft.date=2013-03-01&rft.volume=19&rft.issue=2&rft.spage=163&rft.pages=163-&rft.issn=1598-9623&rft.eissn=2005-4149&rft_id=info:doi/10.1007/s12540-013-2005-2&rft_dat=%3Cproquest%3E2918995971%3C/proquest%3E%3Cgrp_id%3Ecdi_FETCH-proquest_journals_13171652703%3C/grp_id%3E%3Coa%3E%3C/oa%3E%3Curl%3E%3C/url%3E&rft_id=info:oai/&rft_pqid=1317165270&rft_id=info:pmid/&rfr_iscdi=true