Solidification of SSS (sewage sludge slag) has been carried out by the geopolymer binder technique at 80°C steam conditions mixed with CFA (coal fly ash). Geopolymer liquor was prepared by mixing Na-disilicate solution of 1.27 S.G. (specific gravity) and 10 M NaOH solution in 3:1 proportion. Obtaine...
Saved in:
Published in: | Journal of the Ceramic Society of Japan 2010, Vol.118(1374), pp.107-112 |
---|---|
Main Authors: | , |
Format: | Article |
Language: | English |
Subjects: | |
Citations: | Items that this one cites Items that cite this one |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | Solidification of SSS (sewage sludge slag) has been carried out by the geopolymer binder technique at 80°C steam conditions mixed with CFA (coal fly ash). Geopolymer liquor was prepared by mixing Na-disilicate solution of 1.27 S.G. (specific gravity) and 10 M NaOH solution in 3:1 proportion. Obtained monolithic materials were subjected to physical measurements such as 3-point flexural strength, bulk density and expansion-shrinkage. Subsequently, matrix as well as filler chemical compositions were analyzed by SEM-EDX. Results showed SSS is an active filler similar to CFA and maximal strength was reached by blending SSS with CFA in 1:3 proportion. P2O5 and CaO components of SSS strongly contributed to the polycondensation of the geopolymer liquor other than theoretically expected Al2O3 and SiO2 components. |
---|---|
ISSN: | 1882-0743 1348-6535 |
DOI: | 10.2109/jcersj2.118.107 |