Influence of preliminary plastic deformation of 12Kh18N12T steel on its mechanical properties
We have established that the preliminary plastic deformation of 12Kh18N12T austenitic steel causes cold-work hardening, which depends on the strain rate. With increase in the strain rate of specimens from 8∙10 −4 to 417∙10 −4 sec −1 , both strength (ultimate strength) and plasticity (percentage elo...
Saved in:
Published in: | Materials science (New York, N.Y.) N.Y.), 2012, Vol.47 (4), p.438-446 |
---|---|
Main Authors: | , , |
Format: | Article |
Language: | English |
Subjects: | |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | We have established that the preliminary plastic deformation of 12Kh18N12T austenitic steel causes cold-work hardening, which depends on the strain rate. With increase in the strain rate of specimens from 8∙10
−4
to 417∙10
−4
sec
−1
, both strength (ultimate strength) and plasticity (percentage elongation) characteristics of 12Kh18N12T steel decrease. After holding of the preliminarily work-hardened steel at a temperature of 650°C, its strength increases, and its plasticity decreases. At the same time, the isothermal influence for 1 and 10 h does not facilitate intercrystalline corrosion of the steel during its holding in a corrosive medium for 24 h. |
---|---|