Fractal analysis of fracture of powder metallurgical hard alloy
By example of determination of the fractal dimension on a photo of the profile of Palmqvist microcrack obtained as a result of indentation of a Vickers indenter to the surface of a section of metal-ceramic solid alloy (MSA) based on titanium carbonitride, the relationship of microstructure parameter...
Saved in:
Published in: | Inorganic materials : applied research 2017, Vol.8 (1), p.67-74 |
---|---|
Main Authors: | , , |
Format: | Article |
Language: | English |
Subjects: | |
Citations: | Items that this one cites Items that cite this one |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | By example of determination of the fractal dimension on a photo of the profile of Palmqvist microcrack obtained as a result of indentation of a Vickers indenter to the surface of a section of metal-ceramic solid alloy (MSA) based on titanium carbonitride, the relationship of microstructure parameters to the characteristic features of the destruction caused by the development of microcrack is studied. An attempt to find the numerical values of the fractal dimension of microcracks is made. As a solid alloy based on titanium carbonitride, alloys of KNT3, KNT7, and KNT12 grades are selected, where the number indicates volumetric content of the binder phase of Ni–Mo in the alloy, respectively. |
---|---|
ISSN: | 2075-1133 2075-115X |
DOI: | 10.1134/S2075113317010154 |