Loading…
Structure and strength of Al-Si alloys obtained by the Stepanov method
Al-Si alloy samples with a silicon content from 8 to 15 wt % were obtained by the Stepanov method at solidification rates of 10 2 and 10 3 µm s −1 . Tensile and bending strain diagrams were studied at a strain rate of about 10 −4 s −1 . The microstructure of the samples was investigated. It was foun...
Saved in:
Published in: | Bulletin of the Russian Academy of Sciences. Physics 2009-10, Vol.73 (10), p.1391-1394 |
---|---|
Main Authors: | , , , , |
Format: | Article |
Language: | English |
Subjects: | |
Citations: | Items that this one cites |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | Al-Si alloy samples with a silicon content from 8 to 15 wt % were obtained by the Stepanov method at solidification rates of 10
2
and 10
3
µm s
−1
. Tensile and bending strain diagrams were studied at a strain rate of about 10
−4
s
−1
. The microstructure of the samples was investigated. It was found that the silicon content in the eutectic structure of the alloy grows as the solidification rate increases. The yield stress and the tensile strength increase as the silicon content grows. |
---|---|
ISSN: | 1062-8738 1934-9432 |
DOI: | 10.3103/S1062873809100207 |