Correction to: The Effect of Aging on the Microstructure of Selective Laser Melted Cu-Ni-Si
In the Experimental Methods section, second paragraph, last sentence of the original article the value for the resistivity of pure copper is incorrect. The correct value is 1.7241 µΩ-cm.
Saved in:
Published in: | Metallurgical and materials transactions. A, Physical metallurgy and materials science Physical metallurgy and materials science, 2018, Vol.49 (1), p.425-425 |
---|---|
Main Authors: | , , , , , , |
Format: | Article |
Language: | English |
Subjects: | |
Online Access: | Get full text |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Summary: | In the Experimental Methods section, second paragraph, last sentence of the original article the value for the resistivity of pure copper is incorrect. The correct value is 1.7241 µΩ-cm. |
---|---|
ISSN: | 1073-5623 1543-1940 |
DOI: | 10.1007/s11661-017-4395-0 |